Wood preservation by a mixed anhydride treatment: Using simple models of polymeric wood compounds
2008 - IRG/WP 08-30457
Treatment of wood by a mixed aceto/oleic (or other fatty acid residue) anhydride promoted as a safe and environment friendly wood preservation system has been examined quantitatively by liquid phase 13C NMR and solid phase MAS-DEC (proton decoupling) 13C NMR through all its different stages to determine which reactions occur with simple model compounds of the polymeric constituents of wood. The p...
F Lyon, M-F Thevenon, A Pizzi, G Tondi, A Despres, J Gril, S Rigolet


Depletion and Redistribution of Boron in Bundles of Commercially Treated Lumber Exposed to Artificial and Natural Rainfall
2008 - IRG/WP 08-30474
The depletion and redistribution of boron from stacks of Southern Yellow Pine lumber pressure treated with disodium octaborate tetrahydrate (DOT) and exposed to artificial and natural rainfall was examined. When the lumber was exposed to periodic simulated rainfall, 5.7-8.1% of the measured boron present leached from the lumber after exposure to over 300 mm of rainfall. In tests which exposed bo...
M E Mankowski, M J Manning


The effect of gamma radiation on selected wood properties
2008 - IRG/WP 08-40394
As an easy, fast, and effective sterilisation method, gamma irradiation changes molecular structures not only in pest’s living cells, but also in wooden cell walls. Radiation-induced depolymerisation causes significant changes in some properties of wood crucial for restoration and for laboratory testing of wood-preservative effectiveness. The influence of gamma radiation concerning total amount ...
R Despot, M Hasan, A O Rapp, C Brischke, C R Welzbacher


Preliminary investigation of biological resistance, water absorption and swelling of thermally compressed pine wood panels
2008 - IRG/WP 08-40396
Wood can be modified by compressive, thermal and chemical treatments. Compression of wood under thermal conditions is resulted in densification of wood. This study evaluated decay and termite resistance of thermally compressed pine wood panels at either 5 or 7 MPa and at either 120 or 150?C for one hour. The process caused increases in density and decreases in thickness of the panels; however, lab...
Ö Ünsal, S N Kartal, Z Candan, R Arango, C A Clausen, F Green III


The Effect of Heat Treatment on Water Absorption and Dimensional Stability of Anatolian Chestnut (Castanea sativa Mill.) wood
2008 - IRG/WP 08-40407
The heat treatment of wood is an environment-friendly method for wood preservation. This process improves wood’s resistance to decay and its dimensional stability. However, mechanical properties decrease in different ration because of density loss as a result of heat treatment. In this study, the effect of heat treatment on water absorption and dimensional stability at different relative humidit...
G Gunduz, D Aydemir


Mold fungi - Major impediments to cleaning/repairing flood and rain-damaged homes
2008 - IRG/WP 08-40427
Damage to homes by hurricanes that make landfall in the south and southeastern United States, or sub-tropical and tropical regions, during the hot, humid summer months is compounded by the growth of mold fungi on wetted building materials. Most homeowners are better equipped to deal with construction problems associated with storm damage than to control the growth of mold fungi. Following hurrican...
T L Amburgey


Effectos de la intemperización artificial sobre la madera de mezquite (Prosopis laevigata)
2008 - IRG/WP 08-40430
The effects of artificial weathering on Prosopis laevigata wood were studied on eight replicates (150 x 72 x 15mm (l x t x r)) free of knots, cracks and resin. The samples were exposed tangentially to UV light and to water spray during three cycles (1 cycle corresponded 1 week of artificial weathering). The conditioning time between each cycle was thirty days. The effects were measured according t...
A Carrillo-Parra, F Hapla, C Mai


Moisture adsorption isotherms of wood studies using a dynamic vapour sorption apparatus
2009 - IRG/WP 09-20398
Five types of wood including two Malaysian hardwoods acacia mangium (Acacia mangium) and sesenduk (Endospermum malaccense), two temperate softwoods, Sitka spruce (Picea sitchensis), radiata pine (Pinus radiata) and Accoya (commercially modified wood) were studied to determine their moisture sorption behaviour using a Dynamic Vapour Sorption (DVS) apparatus. The isotherm plot for each species teste...
J Zaihan, C A S Hill, S Curling


Evaluation of Water Repellency of Treated Wood Using Several Alternative Methods
2009 - IRG/WP 09-20419
In this study, the results of water repellency testing using a digital swellometer method for water-borne organic-preservative systems with water repellent additives are reported. The findings suggest that the traditional method of using matched untreated controls as a reference developed from historic solvent-based treatments for determination anti-swelling efficacy (ASE) may underestimate the a...
L Jin, A F Preston


Use of Confocal Profilometry to Quantify the Weathering of Wood
2009 - IRG/WP 09-20421
The methods that have been used to screen chemicals for their ability to prevent the weathering of wood involve assessing the loss in weight and tensile strength of treated wood veneers or measuring the rate of erosion of exposed and unexposed (masked) wood subjected to weathering. The erosion of wood during natural weathering occurs slowly and long exposure times are required to produce differenc...
Chunling Liu, P Evans


Micronized Copper Preservative Systems: Observations on the Release of Cupric ion (Cu2+) from Treated Wood and Performance against Wood Decay Fungi
2009 - IRG/WP 09-30519
In an attempt to address the mechanism of action of micronized copper preservatives, a 20-week continuous water leaching study was conducted. The leaching results indicated that, once impregnated in wood, micronized copper preservatives continuously release cupric ion, and the levels of cupric ion released from micronized copper treated wood are higher than those released from CCA treated wood, a...
J Zhang, R Ziobro


Leaching of the copper component from full scale decking boards during one summer season
2009 - IRG/WP 09-50260
The leaching of copper has been tested in laboratory and in outside exposure for freshly treated pine sapwood samples with three different copper preservatives, Cu HDO, copper quat and copper triazoles. We found in the laboratory leaching test that a fixation with warming to 60 °C (140 °F) for 48 hours without drying and then drying in the laboratory in room temperature gave the lowest leaching of copper. We also found that surface treatments with wood oils reduced the leaching, and that washing of the surface before testing had no effect. Full scale decking board samples (0.25 m2) were then exposed outdoors for rain. The rain water was collected and analysed for copper. After one summer season (about 600 mm rain) we found that the leaching differ for the three preservatives. All samples with a water borne surface treatment had the lowest leaching, about half the amount of untreated.
F G Evans


Modification of Wood by a Water-Repellent Compound Used in the Textile Industry: Boron Release and Termite Resistance
2009 - IRG/WP 09-40447
In the study, wood specimens were treated with disodium octoborate tetrahydrate (DOT) and a commercial water and oil repellent compound, FORGUARD M®, a weak cationic emulsion containing dipropylene glycol monomethylether, water and solids in its formulation and used in the textile industry. There were two different processes for preservative treatments: double and single treatments. The leaching ...
S N Kartal, E Terzi, B Erilkun, Y Imamura


Investigation of chemical changes in acetylated beech wood during weathering
2009 - IRG/WP 09-40460
In this study Beech wood (Fagus orientalis) acetylated and has been subjected to a variety of artificial weathering conditions (water only, light only, water and light together)in difference times (0,50,150 and 300 h), then wood surface analyzed using Fourier Transform Infrared spectroscopy (FTIR).Results shown that weathering process affected the functional groups on the wood surface. Light and w...
M Akhtari, M Arefkhani


Methods for Studying Penetration Depth of Wood Protection Products
2010 - IRG/WP 10-20432
EN 152 is an accepted standard in Europe for measuring how deep a wood protection product penetrates into the surface of treated pine wood. The method has provided consumers with a wide assortment of products that meet the specifications outlined in the standard. Because the test takes 8 or more months to carry out, artificial ageing procedures have evolved in order to standardize and speed up the...
K Hansen, L Sites, D D Nicholas


Treatment of Scots pine wood with oil in water and water in oil emulsion systems: Effects on boron leaching and water absorption
2010 - IRG/WP 10-30535
The aim of this study was to investigate the water absorption and water repellent efficiency of oils and oil water emulsions [oil-in-water (O/W) and water-in-oil (W/O)] and possibilities of reducing the amount of boron leaching from treated wood. Scots pine wood samples treated with waste or sunflower oil and water formulations contained 3%BA. The level of water absorption and water repellent effi...
E D Tomak, Ü C Yildiz, A Can


An investigation on some physical properties of oil heat treated poplar wood
2010 - IRG/WP 10-40509
In this study some physical properties of small samples (20×20×20 cm) of poplar wood (Populus nigra var.pyramidalis) after oil heat treatment with linseed oil was investigated. Two time levels (4.5 & 6 hours) and three temperature stages (180,200 & 220°C) were selected. The results of this study showed significant differences in effects of treatment temperature on physical properties of wood....
B Bazyar, D Parsapajouh, H Khademiesalam


Performance of selected types of coated and uncoated modified wood in artificial and natural weathering
2010 - IRG/WP 10-40510
The objective of the present work was to investigate the influence of commercial wood modification methods on weathering behaviour and coating performance. It was aimed to compare modification methods and to set up maps of weathering behaviour for these methods with and without a semi-transparent wood stain. Artificial and natural weathering trials were carried out with a selection of different ty...
G Grüll, L Podgorski, M Truskaller, I Spitaler, V Georges, S Bollmus, A Steitz


Kinetic Water Vapour Sorption of Sitka Spruce at Variable Temperature Using the Parallel Exponential Kinetics Model
2010 - IRG/WP 10-40512
In this study the water vapour sorption of Sitka spruce (Picea sitchensis (Bongard) Carr.) was measured using a Dynamic Vapour Sorption (DVS) apparatus and then analysed using the parallel exponential kinetics (PEK) model. The water vapour sorption rate of wood quickly increased when the relative humidity was changed. With the elapse of time, the sorption rate gradually decreased within any specif...
Yanjun Xie, C Hill


Study of Microscopy Properties of Modified Wood During Weathering Process
2010 - IRG/WP 10-40517
In this study spruce (Picea excelsa) and Beech (Fagus orientalis) wood acetylated and has been subjected of artificial weathering in difference times (0, 50,150&300 h), then wood surface analyzed using Scanning Electron Microscopy (SEM). The SEM results shown that the surface of wood exposed to weathering undergoes distinct physical changes and the surface degradation appears to be directly propor...
M Akhtari


Biological degradation of acetylated wood after 18 years in ground contact and 10 years in marine water
2010 - IRG/WP 10-40522
This paper addresses the resistance to biological degradation of acetylated wood. Firstly, it presents results from an EN 252 test after 18 years’ exposure. The test is still running in Nordic NWPC test fields, Simlångsdalen in Sweden and Viikki in Finland. Results from this test were presented after 5 years’ exposure ( IRG/WP 97-30139), and showed that the resistance of acetylated wood wit...
P Larsson Brelid, M Westin


Preservative Treatment of simul (Bombax ceiba) Veneers with Hot and Cold Water Solution of borax-boric acid by Soaking Process
2010 - IRG/WP 10-40528
Veneers of simul (Bombax ceiba) were treated with different concentrations of water- borne preservatives borax-boric acid (BB) by soaking process for different time periods. In the case of hot water treatment, it was found that the average retention of preservative chemicals increased gradually with the increasing treatment period from 20 minutes to 60 minutes. Similar trend was observed in the ca...
K Akhter, Md Abul Hashem, S Akhter


Comparative Study of Heat Treatment of Beech Wood in Hot Water and Steam Medium
2010 - IRG/WP 10-40536
Heat treatment of wood is an effective method to improve the dimensional stability and durability against biodegradation. Heat treatments of beech wood in 2 different mediums (hot water and steam) in 180ºC were compared in physical, mechanical and anatomical properties. Mass loss in hydrothermally treated wood was higher than hygrothermally treated samples. Mechanical properties (MOR, MOE and CS)...
A Talaei, K Yaghoobi, A N Karimi


Theoretic discussion on the way and driving forces of moisture migration in wood during vacuum drying
2011 - IRG/WP 10-40538
Most of parameters in conventional drying cannot explain a lot of phenomena appeared in vacuum condition, so it is necessary to further explore the moisture migration way and driving forces in wood under vacuum condition. For the water movement channel in wood is very narrow, the characteristic of heat and mass transfer in wood is similar to that in microscale. This article applies theory of liqui...
Zhengbin He, Xueli Yao, Liqiong Chen, Songlin Yi


Effectiveness of Water Based Bentonite-Borate Slurry for In-situ Remedial Protection of Historic Wooden Piles: The Eurobor Protocol, Part 2
2011 - IRG/WP 11-30574
The study of the biocide product Eurobor®, water mixture of boric acid, borax and sodium bentonite, aimed to verify previous findings regarding borates penetration from a clay-water mixture of foundation timber. The product was applied on samples from 100 year old timber foundation from the city of Göteborg. Although in ground for this long the timber was in acceptable god condition due to groun...