Insight in moisture dynamics of wood treated with organosilicon compounds
2016 - IRG/WP 16-20598
The SILEX project “Improving sustainability of construction materials using innovative Silicon based treatment” is a Life+ project with reference LIFE+11 ENV/BE/1046 and started in April 2013. This project intends to demonstrate that a new class of compounds can be used for wood treatment for an extended service life combined with enhanced new testing methodology. The project aims at demonstra...
J Van Acker, J Van den Bulcke, I De Windt, S Colpaert, S De Rocker, S Salvati, J-P Lecomte


Effect of the Storage Time of Logs in Anti-Stain Treatment Effectiveness
2016 - IRG/WP 16-30683
Storage of green lumber, for 7 months, operationally treated with anti-stain products, depending on the storage time of the logs (10, 20 and 30 days) post harvesting allows to affirm that with increasing storage time of the logs, occurs a progressive increase in intensity, severity and types of fungi present in the logs. It is further noted, a significant increase in the percentage of sawn lumber ...
M A Peredo, C Barria


Anti-Fungal Activity on Some Wood extracts as a Wood Protectant
2016 - IRG/WP 16-30684
In this study, six different wood barks were used, where obtained bark extracts were blended with potato-agar in order to investigate their antifungal properties. To determine the inhibition effectiveness of extractives, two different fungi; Coniophera puteana and Trametes versicolor were selected. Fungal activity was carefully observed for the duration of seven days. Following biological testing,...
Ö Özgenç, S Durmaz


Assessment of the biological durability of wood treated with organosilicon compounds
2016 - IRG/WP 16-30685
The European wood construction market is in need of environmentally friendly wood-based products whose service life meets the expectations of end users. Non-biocidal silicon-based water repellents, which can be applied to different materials, help minimize their vulnerability/susceptibility to liquid water. Consequently, they have the potential of increasing wood’s resistance against decay fungi...
M Kutnik, M Montibus, S Derocker, S Salivati, J-P Lecomte


Superhydrophobic treatment of Norway spruce wood for improvement of its resistance against brown rot and moulds
2016 - IRG/WP 16-40734
Water repellence of wood can be increased and its some other properties influenced by introduction of hydrophobic chemicals into and on cell walls without affecting the wood’s bulk density due to lumen filling. Herein, a simple dipping method to insert octadecyltrichlorosilane (OTS) into cell walls and to deposit the self-assembled hydrophobic monolayers (SAMs) of OTS is reported. It was found o...
A Kumar, P Ryparová, P Hajek, B Kričej, M Pavlič, A S Škapin, M Šernek, J Tywoniak, J Žigon, M Petrič


Development of a new method for wood hydrophobizing and fixation of copper compounds by chemical hardening of vegetable based modified oils
2016 - IRG/WP 16-40754
Wood products with ground and direct water contact, but without sufficient biological durability, have to be protected against biological degradation by fungi and other microorganisms. Due to European legislation (Biocidal Products Regulation 528/2012), the selection of possible chemical agents, which are still allowed to be used, is diminishing rapidly. The use of previously widely applied, very ...
C Swaboda, M Fischer, K Jacobs


Influence of organosilicon compounds and nanocellulose treatment on dimensional stability of waterlogged elm wood
2017 - IRG/WP 17-10891
Commonly used agents for waterlogged wood consolidation (including the most popular polyethylene glycol) have proved ineffective and even dangerous to the preserved objects, jeopardising their integrity. Finding new, effective alternatives for safe preservation of wooden cultural heritage is therefore of key importance. The future conservation agents should, first and foremost, provide the integri...
M Broda, B Mazela, I Dąbek, A Dutkiewicz, H Maciejewski, R Markiewicz, M Grzeszkowiak, S Jurga


Chemical compositions and anti-termite activities of essential oils from Gabonese Canarium schweinfurthii Engl, Dacryodes buettneri Engl and Aucoumea klaineana Pierre wood resins.
2017 - IRG/WP 17-10895
Essential oil extract from resins of Canarium schweinfurthii, Dacryodes buettneri and Aucoumea klaineana woods from Cap Esterias and Oyem areas, Gabon, were prepared by Clevenger - steam distillation. The chemical compositions of these respective essential oils were analyzed by a Gas Chromatography coupled with Mass Spectrometry (GC-MS). Although monoterpenes were the main constituents of the thre...
Chemical compositions and anti-termite activities of essential oils from Gabonese Canarium schweinfurthii Engl, Dacryodes buettneri Engl and Aucoumea klaineana Pierre wood resins.


Anti-fungal activity of rutin and rutin-metal complexes as wood protectants
2017 - IRG/WP 17-30708
The anti-fungal activity of Rutin, a flavonoid, alone or complexed with copper or zinc was investigated in a petri dish test with Gloeophyllum trabeum and Trametes versicolor as the test fungi. Rutin and the Rutin-metal complexes showed significant inhibition against each fungus. Rutin-Cu and Rutin-Zn strongly inhibited the brown rot fungus, G. trabeum, while Rutin and Rutin-Zn inhibited T. versic...
Li Yan, J J Morrell, Jie Zhong, Xiuzhu Mao


Organosilicon-based impregnation hydrophobers for wood
2017 - IRG/WP 17-40808
The SILEX project “Improving sustainability of construction materials using innovative Silicon based treatment” is a Life+ project with reference LIFE+11 ENV/BE/1046 and started in April 2013. This project intends to demonstrate that a new class of compounds can be used for wood treatment for an extended service life combined with enhanced new testing methodology. The project aims at demonstra...
J-P Lecomte, J Van Acker, J Van den Bulcke, M Kutnik, M Montibus, S Salvati, S Derocker


Chemical composition and termiticidal activity of Khaya ivorensis stem bark extracts on woods
2018 - IRG/WP 18-30723
The genus Khaya is extractives rich, but the extractives in the stem bark are among the most abundant, accessible and utilised materials in Nigeria. These extractives are of considerable interest for wood protection because of their pesticidal properties. In this study, the chemical constituents of Khaya ivorensis stem bark (KISB) and their termiticidal activity were investigated on Triplochiton s...
G A Adedeji, O Y Ogunsanwo, F S Eguankun, T O Elufioye


Hydrolytic stabilization of chemically modified Bambusa vulgaris Shrad ex JC Wendl
2018 - IRG/WP 18-40830
The main drawback which greatly limit the utilisation of bamboos is their high moisture intake, biodegradation and physical properties changes with environmental variations. To prevent excessive dimensional changes and improve moisture properties of bamboo, Bambusa vulgaris was chemically treated with acetic-anhydride without co-solvent. To evaluate the influence of acetylation on the moisture pro...
N A Sadiku, S M Akintayo


Enhancing service life performance of oak decking and cladding using organosilicon treatments
2018 - IRG/WP 18-40838
The Life+ project SILEX, in full “Improving sustainability of construction materials using innovative Silicon based treatment” started in April 2013 and was finalized mid 2017. The aim of this project was to demonstrate that a new class of compounds can be used for wood treatment for an extended service life combined with enhanced new testing methodology. Ultimately, it was the intention to de...
J Van Acker, J Van den Bulcke, J-P Lecomte


Non-stochiometric oxidation and ROS generation promoted by guaiacol lignin structures and lignocelluose surfaces may be a component of brown rot fungal degradation mechanisms
2019 - IRG/WP 19-10937
Model guaiacol compounds representing lignin monomers, as well as DHP-lignin and wood flour of controlled particle size were used to assess iron reduction at the pH of the natural wood cell wall. All compounds functioned as electron donors for ferric iron, with the lignin monomers demonstrating capacity for non-stochiometric reduction of iron with multiple moles of ferric ion reduced per mole of l...
Y Tamarua, M Yoshidaa, L D Eltisb, B Goodell


Identification of Antifungal Compounds in Konjac Flying Powder and Assessment against Wood Decay Fungi
2019 - IRG/WP 19-30737
The antifungal activity of konjac (Amorphophallus rivieri) flying powder (a by-product produced during mechanical processing of konjac flour) ethanol extract was evaluated against wood decay fungi in culture. Compounds associated with antifungal activity in the extracts were isolated and purified by silica gel column chromatography. The antifungal active fractions were identified by ultra-high-per...
Z Bi, F Yang, Y Lei, J J Morrell, L Yan


The anti-weathering mechanism of extractives in thermally modified Scots pine
2019 - IRG/WP 19-40880
Results from the electron spin-resonance spectroscopy (ESR) analysis indicated that thermally modification of wood can inhibit the generation of phenoxyl radicals during UV irradiation and consequently lead to the increase of the color stability of wood. In order to clarify the evolution and role of extractives in thermally modified wood during the process of weathering, the compositions of aceton...
H Shen, J Cao


Alternative products enhancing dimensional stability comparing to conventional treated products in Japan
2019 - IRG/WP 19-40885
The Act on the Promotion of the Utilization of Wood in Public Buildings (2010) in Japan has made a new stream of the utilization field of timber from housing constructions to larger scale non-housing constructions. After the act, the performance of dimensional stability in preservative treated products becomes more important factor than before. Therefore, various technologies have been developed, ...
K Yamamoto, D Tezuka, Y Sugai, S Maeda, I Momohara


Chemical composition and performances of slow pyrolysis by-product from sugarcane bagasse for wood protection
2020 - IRG/WP 20-30752
Pyrolysis distillate or bio-oil, a by-product of biomasses’ slow pyrolysis in the char-making process, has been traditionally used as bio-pesticides by Asian farmers. Due to its large composition of bio-active chemicals, bio-oil obtained from various biomass has become of interest in many applications, including wood protectants. This study aims to characterize the chemical composition of bio-oi...
F D Boer, M-F Thévenon, J-M Commandre, M Fournier


Water interactions in wood polyesterified with sorbitol and citric acid
2020 - IRG/WP 20-40888
Polyesterifcation of wood with sorbitol and citric acid seems to be a promising chemical wood modification technique that is both low-cost and produced from bio-based chemicals. An interesting aspect of the modification is the interaction of water with the polyesterified wood since the relationship with moisture appears to be unique compared to other wood modification systems. This communication p...
G Beck, A Treu, E Larnøy


Extraction, identification and antifungal activity of polar extractives originated from various wood species
2020 - IRG/WP 20-20673
Extractives are non-cell wall small molecules present in wood and other lignocellulosic materials that can be removed by solvents. Although they represent a minor fraction in comparison with the structural cell wall components, they are an important source of functional groups or molecules with bioactivity or antioxidant properties, that could be used in medicine, cosmetic or wood preservation. T...
R Herrera, F Poohphajai, J Labidi, S Willför, A Sandak


The influence of chemical compounds on wood cell wall to surface cracks
2020 - IRG/WP 20-40908
Degradation due to cracking and dimensional changes caused by drying, have a significantly negative impact on the preservation and durability of wood. Therefore, the prevention of surface cracking, which tends to occur during the drying process, is vital. High temperature set drying is one of the most effective methods for preventing wood surface cracking. It begins with softening the wood at a hi...
R Suzuki, Y Mori, K Yoshihiro, K Yamashita, M Kiguchi


Effect of MVOC exposure on mycelial growth of wood rotting fungi
2021 - IRG/WP 21-10977
It is well known that wood rotting fungi produce microbial volatile organic compounds (MVOCs) as metabolites. In our previous studies, we have found that some MVOCs produced by wood rotting fungi are common to fungal species tested in the studies, while others are specific to each species. Furthermore, it has been also shown that each wood rotting fungi do not always produce the same type of MVOCs...
S Horikawa, R Konuma, M Yoshida


Antifungal and antitermite activities of acetonic extractives from Cedrus Atlantica heartwood
2022 - IRG/WP 22-10990
Cedrus atlantica is a woody species present in France, which in a context of climate change can be privileged in the next years. In addition, this woody species presents great ecological and socio-economic interest as it is mainly recognized for its durable timbers and its essential oil presenting some interesting chemical properties. Therefore, the studies of its heartwood formation and propertie...
R Dijoux, R Ducruet, E Kieny, D Aznar, C Cayzac, L Bidel, C J Allemand, K Candelier


Comparative study on the efficacy of biobased wood preservative over conventional wood preservatives against fungi and termites
2022 - IRG/WP 22-30761
The current focus of wood preservation research is on developing wood preservatives from natural and environmentally compatible compounds for industrial application. Liquefaction of wood is one of the promising approaches to utilize woody waste where the wood powder is converted into a chemically active liquid with the help of a liquefying agent like phenol, cresol, plant-based solvent as CNSL and...
A Kumar, A John, B N Hazarika


Impregnation of wood with antifungal compounds from low-quality tree biomass
2022 - IRG/WP 22-30763
In this paper we have reviewed recent research on the development of bio-based preservative formulations for wood done at the Department of wood science and technology, Ljubljana. Preservative formulations used in this investigation were prepared using plant polyphenols as biocidal agents. These nonstructural components of wood were stilbenes and flavonoids, and were extracted from wood of broken ...
V Vek, I Poljanšek, A Balzano, M Humar, P Oven