The relationship between blue-stain and bark beetles
1971 - IRG/WP 19
The attack of bark beetles on standing or in newly-felled stems provides special growth conditions to wood-inhabiting fungi. In the wood attacked by bark beetles, a specific and rich fungus flora is found, and from these fungi the economically important group of blueing fungi has been more thoroughly investigated. These fungi live on nutritive substances present in the cells, especially in the med...
A Käärik


Fungicidal effectiveness of amended alkylammonium compound
1987 - IRG/WP 3421
Amendment of didecyldimethylammonium chloride was attempted to improve its fungicidal effectiveness and properties of treating solutions. Addition of copper definitely increased effectiveness in controlling wood decay fungi, although metal corrosiveness and stability of treating solutions was unsatisfactory. Further amendment with stabilizer(s), anticorrosive agent(s) and sequestering agent(s) res...
K Tsunoda, K Nishimoto


Domestic wood preservation - Remedial treatments in Australia
1978 - IRG/WP 3128
Domestic construction in Australia relies heavily upon timber. Because of availability, local conditions and building practices, the timbers and other materials employed vary considerably between the States. In recent years, the timber floor has given way to 'raft construction' (concrete slab-on-ground). Not surprisingly, there is a tendency in each State to use local timbers for...
J Beesley, H Greaves


Gaseous boron treatments of wood and wood products
1992 - IRG/WP 92-3691
Treatment of wood and wood products by gaseous organoborates has now been under study for about 5 years. This technique has potential for boron treatment of a wide range of substrates from solid wood through to wood composite materials such as particleboard or wet and dry formed fibreboards. The vapour treatment technique is proving to be very flexible in that it can be adapted to integrate into a...
A J Bergervoet, R Burton, K Nasheri, D R Page, P Vinden


Antisapstain field trials of NeXgen in New Zealand
1997 - IRG/WP 97-30145
This document covers the results of summer and winter log trials of NeXgen, an antisapstain formulation containing methylene bis thiocyanate plus chlorothalonil. Log billets (20 - 25cm diameter) were stripped of bark using a commercial maul debarker and antisapstain treated within 8 hours of felling by dip application. Billets were stored in a pole barn and assessed for internal sapstain and decay...
R N Wakeling, T L Woods, D R Eden, C M Chittenden, B Carpenter


Anti-bluestain treatment developed for log cargoes stacked in subtropical conditions for export on logging ships
1995 - IRG/WP 95-30081
Subtropical environments impose conditions of temperature, humidity and rainfall which are optimal for growth of bluestain fungi. Unprotected softwoods under such conditions become bluestained three days after felling. Furthermore, intervals between harvesting and delivery to export marketplaces exceed the 30-day protection periods attributed to anti-bluestain formulations in such conditions. Thes...
A A W Baecker, M Behr, G D Shelver


Facts or feelings to decide on wood preservation
1988 - IRG/WP 3480
Feelings against the use of chemicals in general and of wood preservatives in special get increasing importance within the population. They are based mainly on an uncertain fear for unknown health risks and vary between different countries and regions. No straight line can be traced. Nevertheless feelings often will influence a decision against chemical wood preservation. Therefore they have to be...
H Willeitner


Defacement of freshly sawn Corsican pine lumber by sapstain and mould fungi and the influence of arthropods
1997 - IRG/WP 97-10227
In a trial to study the arthropods associated with sapstain and mould fungi, freshly sawn Corsican pine (Pinus nigra var. maritima (Aiton) Melville) boards were block stacked at a local sawmill. Each stack was constructed in a nest arrangement with smaller boards in experimental tanks, positioned in the centre of the stacks. Boards were converted from a stock of sawlogs at monthly intervals, to pr...
N J Strong, J F Webber, R A Eaton


Log fumigation prevents enzyme-mediated sapwood discolorations in hardwoods
1993 - IRG/WP 93-10003
Non-microbial sapwood discolorations in hardwood lumber can cause economic loss by degrade of quality. Based on the hypothesis that the enzyme-mediated sapstain may develop in part from byproducts of parenchyma cells in wood, reshly felled logs of red oak (Quercus spp.) and sugar hackberry (Celtis laevigata) were fumigated under a plastic tarp with methyl bromide. Log sections were checked after f...
E L Schmidt, T L Amburgey


Database of sapstain fungi affecting lumber, logs and trees
2004 - IRG/WP 04-10534
Sapstain fungi discolour lumber, logs and tree sapwood and are often mistaken for moulds, which cause a superficial discoloration. Stained wood has a lower market value. Further, because stained wood products can potentially carry pathogenic fungi, such products may be refused by importing countries. Addressing these issues involves developing ways for accurately identifying staining fungi, docume...
S Lee, F de Giuli Vallverdu, S Alamouti, Jae-Jin Kim, A Uzunovic, C Breuil


Performance of groundline bandage remedial treatments in western US species transmission poles
1993 - IRG/WP 93-30019
Groundline bandages are an important element in remedial treatment strategies for utility poles in the United States. Several bandages containing new or reformulated components have recently been developed but have not been adequately tested. This paper reports on the degree of diffusion of copper naphthenate, boron, and sodium fluoride from groundline bandages into pressuretreated Douglas-fir, po...
P G Forsyth, J J Morrell


Prevention of non-microbial sapwood discolorations in hardwood lumber: chemical and mechanical treatments
1997 - IRG/WP 97-30137
Sapwood discolorations in hardwood lumber that are non-microbial in origin result from the formation of pigmented starch-like granules in ray parenchyma cells. These discolorations can be prevented by treating unseasoned lumber with an antioxidant (sodium bisulfite). Exposing unseasoned lumber to microwaves or treating logs with fumigants also will prevent these discolorations. Subjecting unseason...
T L Amburgey, S Kitchens


Effect of treatment process on performance of copper-chrome-arsenate. Part 1: Fungus cellar tests
1995 - IRG/WP 95-40045
Pinus radiata sapwood stakes 20 x 20 x 400 mm³ were treated with CCA Type C using a range of concentrations and three treatment processes; Bethell, Lowry and Rueping. Preservative retention was determined by chemical analysis of treated material. Following fixation, fungus cellar stakelets, 5 x 10 x 180 mm³ were cut from treated material and after leaching were exposed in unsterile soil beds in ...
M E Hedley, J Anderson, J B Foster, B E Patterson


The preventive effectiveness of preservative treatments against wood-rotting fungi. Preliminary results
1992 - IRG/WP 92-2407
The efficacy of a range of preservative treatments in preventing colonisation by decay fungi has been assessed using a method developed at BRE and similar to that adopted by Working Group 9 of European Standards Committee CEN/TC 38. Assessment was made using baits inserted into the test blocks, in holes which had been drilled after treatment to within defined distances of the treated face exposed ...
J K Carey


Effect of aqueous polymer treatments on wood properties. Part 2: Mechanical properties
1990 - IRG/WP 3611
Partially air-dried sapwood of sweetgum (Liquidambar styraciflua) and southern pine (Pinus spp.) was treated with either aqueous polyacrylate or aqueous dimethyloldihydroxyethyleneurea (DMDHEU) solutions. Tests for static bending, toughness, and hardness were conducted on matched treated and untreated pieces according to ASTM Standards. Properties of pine were not affected by treatment with the po...
Z Ashaari, H M Barnes, D E Lyon, R C Vasishth, D D Nicholas


Comparison of the anti-fungal efficacy of Cobra with drill perforation on oscillating pressure treated spruce transmission poles -Laboratory test
1988 - IRG/WP 3469
A laboratory method for measuring the depth of penetration of the fungicidal concentrations effective against basidiomycetes (brown rot) was developed. The tests on CCB oscillating pressure treated spruce transmission poles have shown that the depth of salt penetration can be increased by about 10 mm by a drill perforation before the impregnation. An even better penetration is reached, however, if...
E Graf, B Zgraggen


Comparison of thermally modified wood originating from four industrial scale processes – durability
2002 - IRG/WP 02-40229
This study examined the differences in biological wood properties of heat treated wood originating from four different European industrial heat treatment plants. The manufacturers of heat treated material were: PLATO Hout B.V./Netherlands, Thermo Wood/Finland, New Option Wood/France and Menz Holz/Germany where Oil-Heat treated Wood (OHT) is produced. The results of miniblock tests with basidiomyc...
C R Welzbacher, A O Rapp


Effects of chemicals used for ground-line protection of hardwood poles on termite attack
1988 - IRG/WP 1356
The majority of chemicals formulatet to protect the groundline of hardwood poles in Australia have been fungicides. Nine products were tested against Coptotermes lacteus attack to determine their value in preventing attack by subterranean termites. Results indicated that Busan, high temperature creosote, pigment emulsified creosote, copper naphthenate gel and "Blue 7" had a repellent effect on Cop...
R S Johnstone, R H Eldridge


Preservative treatment specifications in Fiji
1982 - IRG/WP 3190
The preservative treatment specification used in Fiji is outlined. Reference is made to a basic end use classification and to locally approved treatment processes, preservatives and retention levels. Amenability ratings are defined and penetration requirements for broad commodities indicated. Currently commercial operations rely entirely on pressure treatment with copper-chrome-arsenic multisalts ...
A S Alston


A new type of biocide suitable for use in different fields of wood preservation
1993 - IRG/WP 93-30014
A new type of polymeric biocides was developed containing quaternary ammonium and boron ester groups as active structure elements, to overcome the disadvantages of AAC's in wood preservation use and to utilise their good performance due to a broad efficacy against fungi on the other hand. The new biocides called polymeric betains have been tested in laboratory and field tests and especial...
V Barth, H Härtner


Protection of pile tops using combinations of internal treatments and water shedding caps
1993 - IRG/WP 93-30020
Preservative treatment produces an excellent barrier against fungal, insect, and marine borer attack; however, fabricators often disrupt this barrier during construction, creating avenues for entry of decay agents. This problem is particularly acute in marinas along the coastal United States. Standards recommend the application of a water-shedding cap at the time of installation to prevent pile to...
P Schnieder, M A Newbill, J J Morrell


Metal plate fasteners in trussed rafters treated with preservatives or flame retardants - corrosion risks
1977 - IRG/WP 3104
In designing roof trusses employing metal plate fasteners it is generally assumed that the roof will remain dry in service. Whilst this is generally true, damp conditions do arise under some circumstances, although it is not possible to quantify the extent of the risk. It is only possible, therefore, to give general recommendations which must be interpreted in the light of local experience of serv...
R A Laidlaw, L C Pinion


Information from the COIPM Wood Group
1988 - IRG/WP 4146
Abstract from the COIPM minutes: Wood in marine environment: Mrs Gambetta stated that the main item discussed by the Group was the collaborative work to test the durability of heat shrinkable polyolephin sheating materials for the protection of wood against marine organisms. The work began last year when wood samples were sent out to the participants. Three samples of Pinus sylvestris wrapped in ...
A Gambetta


Validation of the sapstain danger index
2000 - IRG/WP 00-10333
The Sapstain Danger Index (SDI) is a model that is used to indicate sites in the New Zealand forest where felled logs are more prone to sapstain, specifically it should indicate how soon after felling of a log should it be treated for sapstain. The validation of SDI has the goal to identify whether the SDI can be used to predict sapstain development and to eventually minimise loss of value of logs...
P A Cooper, S Downs, R l Farrell


Studies and experiences of occurrence and development of soft rot in salt-treated poles of pine (Pinus sylvestris) installed in Swedish transmission lines in the years 1940-1945
1977 - IRG/WP 277
The present work describes the result of microscopic examinations of some 2,000 borings extracted from 20 to 23-year-old salt-treated poles (Scots pine) from the southern and central parts of Sweden. The purpose was to map out the occurrence of soft rot in Sweden and its influence on the mechanical strength of the poles as well as to contribute to the development of new and more satisfactory metho...
H Friis-Hansen