IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 358 documents. Displaying 25 entries per page.


Preliminary field and laboratory findings regarding the efficacy of a novel anti-marine wood borer agent
2000 - IRG/WP 00-10380
Blocks of sapwood of Pinus nigra were treated by vacuum impregnation with Biocide A to retentions of 0.5, 1 and 2 kg m-3. Similar blocks were vacuum-pressure impregnated with CCA to retentions of 2, 24 and 38kg m-3. The blocks were exposed subtidally in Mourilyan Harbour (Queensland, Australia). After 5 and 10 months exposure, blocks were removed, examined for superficial signs of attack by wood b...
A Praël, S M Cragg, R A Eaton


Long-term protection of stored lumber against mould, stain, and specifically decay: A comparative field test of fungicidal formulations
1984 - IRG/WP 3281
The problem of decay in packaged, unseasoned lumber stored for many months has become of major importance in recent years. Large financial claims have resulted from decay in Canadian lumber stored at length in seaports and storage yards of distributors. For decades acceptable protection from moulds and sapstain was readily achieved with chlorinated phenols applied at appropriate treating levels. H...
A J Cserjesi, A Byrne, E L Johnson


Biological control of sapstain fungi in wood
1996 - IRG/WP 96-10158
Sapstain fungi can cause serious damage to wood and wood products, resulting in a significant economic loss for the wood products industry. The purpose of the present investigation was to determine whether the sapstain in wood caused by sapstain fungi could be biologically controlled. Biological control of sapstain fungi in wood was demonstrated in field trials with nonpigmented isolates of Cerato...
S C Croan


Effects of heat treatment on water repellence and anti-swelling efficiency of beech wood
2002 - IRG/WP 02-40223
The heating of solid wood to higher temperatures is the simplest and the cheapest means for stabilizing its dimensions. For the investigation of the effect of thermal treatment on water repellency effectiveness and anti-swelling efficiency of beech wood (Fagus orientalis Lipsky), air-seasoned samples of beech wood were heated in presence of air at temperatures of 130 C, 150 C, 180 C and 200 C for ...
S Yildiz


Biocontrol and bioprotection of wood decay and sapstain fungi
2003 - IRG/WP 03-10474
The most serious damages caused in the wood industries by decay and sapstain fungi, and the growing international pressures on the use of biocides products with toxic active ingredients harmful to human health and the environment, have made it necessary to search for alternative chemical products to protect the wood, and for the possibility to use micro-organisms as biological controllers. This la...
M T De Troya, F Rubio, M Villarreal, F Arenal, F Llinares, V Rubio, D Muñoz-Mingarro, N Acero


Health and safety aspects of the use of wood preservatives in Sweden
1977 - IRG/WP 396
The Act on products Hazardous to Health and to the Environment (Swedish Code of Statutes SFS 1973:329) came into force on 1st July 1973. The Act cancelled and superseded the Poison Act, the Pesticides Act and the PCB Act from 1962, 1962 and 1971 respectively. Regulations for the implementation of the Act are contained in the Ordinance on Products Hazardous to Health and to the Environment (SFS 197...
B Henningsson


Treatment of wood-based panel products with volatile borate
1990 - IRG/WP 3616
The paper presents recent developments in the use of volatile borate esters for the preservative treatment of wood based board materials. Several advances on previous reports are discussed. In laboratory studies, treatment times of approximately ten minutes at 20°C on boards at equilibrium moisture content provided full penetration and retentions of 1% wt/wt boric acid. Biological tests have been...
P Turner, R J Murphy, D J Dickinson


Risk reduction from curative treatments, restoration and maintenance of building and individual housing - simple precautions that make the difference
2005 - IRG/WP 05-50224-15
This document explores the potentialities of risk reduction, from activities of remediation in construction, developped at small scale by professionals or individuals on targets like moulds, rots, termites and other wood destroying insects, with products distributed for professional or do-it-yourself purposes. At the first stage, an inventory of the type / interest of products / processes is carri...
G Ozanne


SEM investigation of the production of extracellular mucilaginous material (ECM) by some wood inhabiting and wood decay fungi when grown in wood
1997 - IRG/WP 97-10193
Previous reports have illustrated the involvement of extracellular mucilage (ECM) in wood decay by Basidiomycetes. Its production is investigated in a range of stain, mould and soft rot fungi in Corsican pine, Scots pine and European beech. Fungi examined were: Chaetomium globosum, Ceratocystis coerulescens, Trichoderma harzianum, Ophiostoma piceae, Mucor sp. and Penicillium. sp. The samples were ...
A R Abu, D J Dickinson, R J Murphy


Environmental risk assessment of treated timber in service: The Environment Focus Group approach
2000 - IRG/WP 00-50162
In the context of the Biocidal Products Directive (98/8/EC), and of the OECD work on wood preservatives, the Environment Focus Group (EFG), comprising 8 institutes and the European Wood Preservative Manufacturers Group, has been working on the environmental risk assessment of treated timber in service. A literature review of emissions from treated timber has revealed that very little existing data...
G Deroubaix, G Labat, I Le Bayon, S Legay, P Marchal, C Yrieix, E Melcher, R-D Peek, S De Geyter, J Van Acker, W J Homan, D J Dickinson, R J Murphy, E D Suttie, A J Nurmi, A-C Ritschkoff, D Rudolph, I Stephan, D Aston, E F Baines, J B Simonin


The efficacy of Sentry® as a treatment for the control of sapstain in pre-infected radiata pine
2001 - IRG/WP 01-30260
Experiments were conducted to determine the efficacy of Sentry® when used to control sapstain fungi on radiata pine branch billets stored under high fungal hazard conditions. Prior to antisapstain treatment, the billets were pre-infected with a mixed inoculum of staining fungi and held from zero to 10 days at 25°C and 75% relative humidity. This was done to produce billets with different degrees...
C Chittenden, J G van der Waals, B Kreber, R N Wakeling


Copper leaching from Kemwood ACQ and Embalit CBC treated wood products
2000 - IRG/WP 00-50150
TNO has performed a study on the leaching of copper from Kemwood ACQ and Embalit CBC treated wood products, further referred to as ACQ and CBC. The sawn dry wood has been impregnated using an industrial vacuum-pressure process with ACQ (with or without Ultrawood 4) or with CBC, under supervision of Flexchemie B.V. After treatment samples have been transported and subjected to leaching tests at TNO...
P Esser, W L D Suitela, H Trompetter


Effect of mobile fungicides on fungal pre-infection in radiata pine billets.
1999 - IRG/WP 99-30191
In New Zealand, fungal infection of logs begins directly after felling and whilst severe degrade can be prevented if antisapstain-treated within 24 hours, such short turn-around times of logs are not always practicable. However, conventional antisapstain formulations in use only provide an envelope of protection on the log surface but are unable to control pre-infections below the surface. The obj...
D R Eden, T Singh, B Kreber


Controlling the sapstain fungus Ceratocystis coerulescens by metabolites obtained from Bjerkandera adusta and Talaromyces flavus
1993 - IRG/WP 93-10024
Sapstain causes severe damage to wood and wood products, posing a major economic problem for the wood industry. The purpose of this study was to determine if metabolites from Bjerkandera adusta and Talaromyces flavus would (1) decolorize stain in wood caused by Ceratocystis coerulescens and (2) prevent sapstain by Ceratocystis coerulescens. We studied the interaction of the sapstain fungus Ceratoc...
S C Croan, T L Highley


Properties of hot oil treated wood and the possible chemical reactions between wood and soybean oil during heat treatment
2005 - IRG/WP 05-40304
Thermal treatment with hot oil as the heating media based on the original idea from oil-heat treatment in Germany was investigated. The treatment was mainly carried out at 200ºC and 220ºC for 2 hours and 4 hours, and the wood species were mainly spruce and fir. This paper focuses on the difference between soybean oil and palm oil and the possible chemical reactions between wood and soybean oil. ...
Jieying Wang, P A Cooper


Contradiction between uptake of preservative in practical situation and laboratory testing
1992 - IRG/WP 92-2392
By brush treatment water- and solvent-based products were applied on boards of Scots pine and Norway spruce to achieve an uptake of 100 and 200 g/ml. In addition the scope of work to achieve the required uptake of preservative was determined under practical conditions for both product groups. EN 113 (RAL-GZ 830) tests were carried out to test the biological efficacy of products. After 18 months ex...
R Gründlinger, O Janotta, M Melzer


Sentry®, a new antisapstain formulation for protecting logs and lumber. - Part 2: protection of lumber
1999 - IRG/WP 99-30189
Recent research conducted by Forest Research, Chemcolour Industries (NZ) Ltd. and Fletcher Challenge Forest Ltd. has resulted in the development of antisapstain formulations that meet the efficacy requirements of the New Zealand Forest industry for export logs. One treatment, called Sentry®, is now poised for commercial use in New Zealand for treating export logs, having undergone an extensive su...
R N Wakeling, D R Eden, C M Chittenden, J G Van der Waals, B Carpenter, I Dorset, R Kuluz, J Wakeman


Distinguishing isolates of Aureobasidium on the basis of their ability to utilise lignin breakdown products as a sole carbon source
1996 - IRG/WP 96-10151
Wild isolates of Aureobasidium were obtained by dilution plating from a ca 20 year old painted pine window frame. Four isolates were obtained from the paint/wood interface region and four isolated from regions deep in the wood. The isolates were then used to inoculate liquid cultures containing ferulic acid, a lignin breakdown product, present as the sole carbon source. Ability of the isolates to ...
M W Schoeman, D J Dickinson


Which fungi should be included in the laboratory evaluation of anti-stain chemicals?
2001 - IRG/WP 01-20236
Test fungi for efficacy tests of anti-stain formulations were selected based on the assumptions that test fungi should be fungicide-tolerant antagonists and fungi resistant to both fungicides and fungicide- tolerant antagonists, and such fungi should be re-isolated from treated samples with the highest fungicidal concentration used for laboratory evaluation of fungicides. This paper discusses the ...
Hyung-Jun Kim, Jae-Jin Kim, Gyu-Hyeok Kim


Monitoring the potential biological control agent Cartapip
2000 - IRG/WP 00-10365
Attempts to biocontrol woodstain caused by Ophiostoma species led to the development of an O. piliferum colorless mutant - Cartapip (AgraSoL). The mutant's ability to prevent sapstain of stored logs and lumber is tested in a variety of field trials in Germany, England, Canada and New Zealand. To carry out biocontrol field trials, users have to obtain a permit from a regulatory agency and ...
S Schröder, K Sterfinger, Seong Hwan Kim, C Breuil


L-joint trials: Part 3: Relative performance of a range of preservative products
2002 - IRG/WP 02-30292
Long-term trials using the L-joints described in BS EN 330 and AWPA Standard E9-97 have been in progress at BRE since 1982. This paper records the current assessments of decay of L-joints in trials started between 1982 and 1994 with treatments applied to both Scots pine sapwood (Pinus sylvestris) and spruce (Picea sp.). Data are provided on a range of active ingredients including TnBTO, PCP, a...
J K Carey


Soil bed studies of the dimensional stability of composite products
1999 - IRG/WP 99-40134
The influence of boron and isocyanate resin on the dimensional stability of high moisture resistant particleboard was assessed after burial in a soil bed for one month. The samples were treated with two levels of a boron compound and coated in isocyanate resin. The samples were randomly placed in a fungal cellar in soils of two different water holding capacities. Weight differences and dimensional...
K M Filcock, P Vinden


Pest control products act. An overview of regulation of heavy duty wood preservatives
1995 - IRG/WP 95-50040-30
The regulation of pesticides in Canada is carried out under the authority of the Pest Control Products Act and Regulations. Products which control, prevent, destroy, mitigate, attract or repel a pest are required to undergo a presale assessment for safety, merit and value. This review will determine whether a product, when used according to label directions, can be used both safely and will be eff...
K McCullogh


Association of contents of nitrogen and sugars in rubberwood (Hevea brasiliensis) clones with susceptibility to sapstain by Botryodiplodia theobromae, Aureobasidium pullulans and Aspergillus niger
1999 - IRG/WP 99-10307
The purpose of this study was to determine if nitrogen and sugar contents in rubberwood from three selected varieties (clones) rubber trees would affect the rate of colonisation by Botryodiplodia theobromae (a tropical sapstain fungus), Aureobasidium pullulans (a temperate sapstain fungus) and Aspergillus niger (a common mould fungus). Sapstain growth was rated daily until at least 50% mycelial co...
A J Ashari, J W Palfreyman, A H H Wong


Destaining wood sapstains caused by Ceratocystis coerulescens
1996 - IRG/WP 96-10159
Fungal sapstain does not reduce the strength of wood, but it does discolor the wood, detracting from its appearance and decreasing the value of wood and wood products. The purpose of this investigation was to assess whether wood sapstain caused by Ceratocystis coerulescens could be destained and existing growth eradicated. The hydroxyl radicals generation under optimized conditions destained the s...
S C Croan


Previous Page | Next Page