Feeding response of field populations of Coptotermes species to softwood blocks treated with non-toxic water-proofing and anti-microbial products.
2003 - IRG/WP 03-10487
The feeding response of field populations of the subterranean termite, Coptotermes lacteus, to Pinus radiata wood blocks (50 x 40 x40 mm) treated with various combinations of non-toxic and odourless water-proofing materials based on natural high molecular weight esters (TimberTreatÒ) and a new water insoluble quaternary ammonium compound (‘anti-microbial’) is described. Treated wood blocks we...
J R J French, T Pynsent, M Susic


The study of blue stain found in coniferous timber in SR Slovenia (Yugoslavia)
1983 - IRG/WP 1177
The report concerns the problems connected with blue stain in coniferous timbers stored in warehouses at wood-processing plants in SR Slovenia (Yugoslavia). The amounts of spruce-wood (Picea abies Karst.) found to have been infected with blue stain have been measured and some of the fungi causing the stain have been identified and their biology studied. It was found that the percentage of spruce-w...
R Benko


Anti-sapstain chemicals for diffusion treatment of rubber wood
1986 - IRG/WP 3367
Performance of Sinesto B and Akzo EN 494, two formulated products of alkyl ammonium compounds, was tested as fungicidal additive in the boron solution to control mould and stain during diffusion storage of rubber wood. Sinesto B at 2.0% (a.i.) concentration has given good control over mould and its protection against sapstain was only satisfactory. Akzo EN 494 at 0.7% (a.i.) concentration has give...
R Gnanaharan


The risk assessment process. Point of view of a biocide manufacturer [Évaluation du risque. Point de vue d'un fabricant de biocide]
1990 - IRG/WP 3568
Risk assessment is an inherent part of our everyday lives. The risk assessment equation combines Hazards and Exposure. For the Wood Preservation Industry, the hazards may be characterised by the toxicity a the ecotoxicity of chemicals and the exposure by the identification of exposed people, of the exposure routes and exposure frequency. To quantify the exposure, good co-operation is required betw...
D Baur


A field trial to assess the potential of antisapstain chemicals for long-term protection of sawn radiata pine
1986 - IRG/WP 3375
Seven chemical formulations were tested as antisapstain treatments for freshly sawn radiata pine sapwood (90x50 mm²). Each formulation was used with and without a water-repellent additive and was sprayed on to 1 m long boards. The boards were then stacked into "mini" packets and stored unprotected from the weather for 6 months. Haipen 50w (at 0.2 or 0.4% active) and NaPCP (1% active) plus 1.5% bo...
J A Drysdale


Mycoparasitism by some white rot fungi on blue stain fungi in culture
1986 - IRG/WP 1304
When studying biological control of blue stain an interesting phenomenon of parasitism by some white rot fungi on blue stain fungi has been encountered. The majority of the 22 tested white rot fungi act parasitically upon blue stain fungi. The most interesting species among them is Bjerkandera adusta (Willd. ex Fr.) Karst., causing almost complete or complete decoloration of the hyphae of the blue...
R Benko, B Henningsson


"XYLOPHENE ANTI-TERMITES" :A complete range of treatment products against termites
2000 - IRG/WP 00-30230
Dyrup-Xylochimie purpose for several years efficient treatment products for timber and wood materials, with its trade mark : "Xylophèn". As everybody know, termites become an important problem for construction in France. So important that, a national law was voted in May 1999, to define areas where termites are present, in order to protect future landowner. To prevent efficiently termites damages...
L Cubizolles, E Wozniak


Pretreatment decay in poles of Pinus sylvestris
1987 - IRG/WP 1329
Storage damage by blue stain and decay in poles before impregnation has been increasingly observed during recent years and there have been reports that salt-impregnated poles today are of lower quality because of incipient decay being increasingly common. The attacks may have started at the time of cutting and then continued during the period of seasoning at the plant, which could be as long as tw...
H Lundström, M-L Edlund


Analysis of the degradation of carbohydrates by blue-stain fungi
1990 - IRG/WP 1457
The topic of the degradative ability of blue-stain fungi literature is not clear. Many authors support the idea that those fungi don't have enzymatic capability to decay the wall of the ligneous cells. However, others have found some decay activity. In this study, we have attempted to analyze which wall cells soluble carbohydrates are metabolized by some blue-stain fungi, found in Spain. ...
M T De Troya, A M Navarrete, E Relano


Laboratory evaluation of anti-sapstain formulations
1989 - IRG/WP 3510
Four formulations were tested for their efficacy in controlling molds and sapstaining fungi on wood according to the Standard-II of Japan Wood Preserving Association (JWPA). Relative efficacy was compared on the basis of visual rating of the fungal growth on the treated and untreated wood surfaces when the wood specimens were exposed to each monoculture of 5 test fungi at 26±2°C and 70-80% for 4...
K Tsunoda


What is OECD doing to promote harmonization of biocide regulations
1999 - IRG/WP 99-20182
OECD began work on biocides in 1997 to help Member countries co-operate in the assessment and registration of these products. The work is a part of OECD's Pesticide Programme, and is co-ordinated by the Biocides Steering Group. The goal is to harmonize regulatory approaches to allow countries to conduct evaluations of biocides more efficiently. More efficient evaluations can advance the p...
M Paneli, N Grandy


The effect of stack height on the performance of preservatives used for the prevention of sapstain on seasoning wood
1997 - IRG/WP 97-10192
The performance of three anti-sapstain preservatives was investigated under field conditions in south east England. The preservatives under test were: copper-8-quinolinolate (Mitrol PQ8) trimethylalkylammoniumchloride and sodium hexanoate (Sinesto B) and chlorothalonil (Tuff Brite). The preservatives were tested on Corsican Pine grown in south east England. The field trial was set up to investigat...
J R Williams, D J Dickinson, J F Webber


Comparison of bluestain fungi growing in vitro and in vivo
1996 - IRG/WP 96-10149
Both moulds and bluestain fungi cause serious economic losses for forestry and timber processing industries and much research is aimed at finding environmentally and economically acceptable methods of control. It is especially important to study the growth of these fungi in freshly cut wood, which has been unaltered by drying or sterilisation, and which therefore resembles the substratum they woul...
A Uzunovic, J F Webber, D J Dickinson


Blue stain in timber in service. Progress review of Sub-group collaborative tests - 1981/82
1982 - IRG/WP 2178
Following from the discussions after reporting Document IRG/WP/2146 at the Meeting in Sarajevo, 1981, it was decided that 1.) more precise definition was needed of the artificial weathering schedules used in the work - participants to re-check Table 8 and send further details or amendments to Dr Bravery; 2.) a further test employing a wider range of chemicals was necessary using a smaller range of...
A F Bravery, D J Dickinson


Blue Staining of Coated Modified and Unmodified Wood
2006 - IRG/WP 06-10589
We investigated resistance of unmodified, DMDHEU modified and oil heat treated uncoated and coated Scots pine wood against blue stain fungi. Both EN 152-1 and the reverse exposure tests showed excellent resistance of DMDHEU and especially of oil heat treated wood against blue staining. It is not needed to add any additional protective coating layers to prevent modified wood from staining. However,...
M Petric, M Pavlic, M Humar, M Tomažic


Direct analysis from wood of the blue stain fungi Aureobasidium pullulans and Hormonema dematioides by denaturing gradient gel electrophoresis
2006 - IRG/WP 06-10595
Aureobasidium pullulans and Hormonema dematioides are the two organisms used in the EN 152 laboratory method for determining the effectiveness of preservatives against blue stain in service. The literature concerning the disfigurement of surface coatings and exposed timber in-service states that A. pullulans is the dominant blue stain fungus, due to its frequent isolation from stained material. In...
M J Ray, D J Dickinson


Study of new wood preservatives from biological origin and low toxicity against wood decay organisms (fungi and termites)
2006 - IRG/WP 06-10600
Wood as an organic material is likely to be attacked by living organisms if no protecting treatment is applied to improve its durability. The biological agents, which in Spain, due to its specific climatologic, cause major damage to wood, are the stain fungi, the rot fungi and the subterranean termites. The commercialisation of the products actually used to treat wood against fungi and to treat t...
M T Troya, M J Prieto, F Rubio, D Lorenzo, J J Teixidó


Efficacies of an insecticide and a fungicide for preventing blue-stain of Japanese red pine logs
2006 - IRG/WP 06-20329
We examined blue-stain fungi on Japanese red pine at 3 forests and 2 saw mills in Iwate Prefecture, Japan. The isolated ophiostomatoid fungi were Leptographium sp and Ophiostoma sp. There were 3 routes of the blue-stain; fungal growth from the spore or hypha stuck on the cross cut surfaces, fungal spread through the inner bark by bark beetles and fungal invasion around whorled knot. The larger ext...
H Taniuchi, T Koiwa, H Masuya, S Doi


EN 152: Is this Standard Relevant for today’s Wood Preservatives? A Critical Review.
2006 - IRG/WP 06-20331
The paper critically reviews the Blue stain test method described in EN 152 including possible test variables. Whereas EN 152 has been successfully used for solvent borne wood preservatives, it appears that the methodology is not suited for modern water borne products, where the majority fail. The paper will show that there exist different quality claims not concordant with EN 599-1 within diff...
B Jensen, F Imsgard, J Larsen


Efficacies of physical barriers for preventing blue-stain of Japanese red pine logs
2007 - IRG/WP 07-20359
This paper deals with field trials on physical barriers to prevent blue stain on Japanese red pine logs using a fly screen, bark and leaves of Japanese cedar as covering materials. These barriers arrested blue stain and bark beetle attacks to low levels than control for 1 month except covering with a small amount of bark. Covering with the fly screen and a large amount of bark permissibly suppress...
H Taniuchi, T Koiwa, H Masuya, S Doi


Some textile auxiliaries as wood protective agents
2007 - IRG/WP 07-30417
This study evaluated some textile auxiliaries applicable for wood protection. Commercial alkoxysilane quarternary ammonium formulation and fluorocarbon based water-oil repellent were tested for their ability to provide hydrophobicity and antifungal effect to solid wood samples. Scots pine (Pinus sylvestris L.) sapwood samples were impregnated with 25, 50 and 100 % concentrations of the above menti...
E Dizman, A Temiz, N Terziev, Ü C Yildiz


Protection of wood for above ground application through modification with a fatty acid modified N-methylol/paraffin formulation
2007 - IRG/WP 07-40378
Hydrophobic chemical modification can be regarded as an alternative approach to conventional wood preservation using biocides in order to protect wood in hazard class 3 according the European Standard EN 335-1. A formulation containing fatty acid modified N-methylol/paraffin and an aluminium salt catalyst was used to change the material properties of wood in order to protect wood from fungal dec...
Nguyen Hong Minh, H Militz, C Mai


End Coating Masson Pine Grown in South China to Prevent the Development of Blue Stain
2007 - IRG/WP 07-30428
One end (randomly selected) of logs of mason pine (Pinus massoniana) were coated with a wax-type end coating called ANCHORSEAL® immediately after tree cutting. The logs were then stored in summer weather in Guangxi, China. During the storage, at week 1, 2, 3, 4, 6, 8 and 12, five logs of mason pine were sawn into lumber or veneer for the visual observation and measurement of blue stain at the coa...
Zhao Youke, Qin Li, Huang Rongfeng, Lu Jianxiong


Laboratory test of blue stain control by chemicals
2007 - IRG/WP 07-30430
8 chemicals and some mixtures against Botryodiplodia theobromae Pat., Fusarium verticillioides(Sacc.)Nirenberg, Trichoderma harzianum Rifai, Trichoderma viride Pers., and Penicillium purpurogenum Stoll were conducted in laboratory by inhibition zone in the paper. The results were shown that: CBZ and benomyl as well as copper oxine alone are much high efficacy for inhibiting most of the 5 fungi tha...
Zhijuan Wang, Zehui Jiang, Mingliang Jiang, Chungen Piao


Laser stain removal of fungus-induced stains on paper-based cultural relics
2007 - IRG/WP 07-40389
Laser techniques has been developed and applied in commercial use for 40 years, but it has not been used successfully to remove stains from paper-based cultural relics . The purpose of this study was to investigate the paper cleaning by using a technique of Nd-YAG laser. Artificial stained papers were inoculated with fungi and then were treated at different laser cleaning parameters, in order to f...
Tsang-Chyi Shiah, Han Chien Lin