Natural progression of decay in unrestrained, Southern pine sapwood exposed above ground
1995 - IRG/WP 95-20060
In this study, the natural progression of decay is being monitored in 2.4-m (8-ft) lengths of dimension lumber. The 2.4-m lengths are supported without restraint in a horizontal plane approximately 0.75 m above ground in a partially shaded field plot in southern Mississippi. The lumber is 100% sapwood. Prior to installation in the field, each piece was planed to exactly 38 by 89 mm² (1.5 by 3.5 i...
R C De Groot, R J Ross, W Nelson


Application of a novel strength evaluation technique during screening of wood preservatives
1986 - IRG/WP 2262
The effectiveness of CCA and ACA in treated aspen mini stakes tested using a novel bag procedure, with unsterile soil fortified with Chaetomium globosum and Ceratocystis albida, is reported. Good agreement between toxic limits determined using the standard weight loss procedure, and those determined by the strength technique were found, with some indication that the strength loss method is more se...
J N R Ruddick


Evaluation of wood durability by laboratory test - A new equation to predict wood durability
2001 - IRG/WP 01-20230
To estimate the wood durability in a short term, periodical weight determination was carried out in a laboratory test. This test provided the results comparable to those of the field test and the fungus cellar test, but it required much more jobs in comparison to the usual accelerated laboratory test. To save the time and jobbing for this method, a new equation was devised from simple two assumpti...
I Momohara, K Yamamoto


A technique for the rapid assessment of wood surface degradation during weathering
1987 - IRG/WP 2281
Radiate pine (Pinus radiata D. Don) sapwood samples taken from four trees were converted into thin strips 100 x 10 x 0.085 (85 µm) mm³, (longitudinal x radial x tangential) in size and exposed in preweighed hatches to the weather inclined at 45° facing equatorially for 10, 20, 40, 60, 80 and 100 days. Significant (P < 0.001) weight losses occurred with time over the exposure period. Differen...
P D Evans, D Abbott, S Thein


IUFRO rating system compares favourably to weight loss for soil-bed testing
1990 - IRG/WP 2343
The soil-bed/small stake test is commonly used for rapidly evaluating the performance of new, more environmentally acceptable, preservatives. In a 1.5 year experiment with three copper-based waterborne preservatives, visual evaluation and probing using the IUFRO performance rating scale (0-4) gave very similar toxic thresholds to those derived from measurement of weight loss at the end of the expe...
P I Morris


Soluble nutrient influences on toxicity and permanence of CCA preservatives in wood
1980 - IRG/WP 3144
The influence of soluble carbohydrate and nitrogenous components concentrated at evaporative surfaces of wood on the toxicity and permanence of CCA preservatives has been examined using soil-burial techniques. Nutrient concentrations in lime (Tilia vulgaris Hayne) have been shown to be associated with reduction of toxic limits of preservatives to an extent in which a 100% increase in preservative ...
B King, G M Smith, A Bruce


Treatment of poplar plywood with solvent and water-borne preservatives
1989 - IRG/WP 3538
Poplar as a light hardwood is appropriate for plywood production. Owing to its low natural durability it is generally recommended to preserve it in all conditions where risks of fungal attack may be present. A research project has been carried out on preservative treatments of plywood commodities. Parameters studied were various treatment cycles, three types of plywood, and a number of solvent and...
J Van Acker, M Stevens


Laboratory testing of wood natural durability - In soil-bed assays
1998 - IRG/WP 98-20141
Laboratory methods for assessing wood decay resistance are being investigated in the framework of an ongoing European research project. This paper summarizes the main results obtained for soil-bed tests based on the European prestandard ENV 807-Test 2. The data suggest that this testing methodology is suitable for evaluating the natural durability of timber species in soil-contact under conditions...
R Sierra-Alvarez, I Le Bayon, J K Carey, I Stephan, J Van Acker, M Grinda, G Kleist, H Militz, R-D Peek


Rapid loss of lignin at wood surfaces during natural weathering
1992 - IRG/WP 92-2390
Thin veneers of radiata pine (Pinus radiata D. Don) were exposed to natural weathering over a period of 30 days. Incident UV radiation was monitored at the test site. FTIR internal reflectance spectroscopy was used to study the chemical changes taking place at the veneer surface during weathering. Spectra obtained show that after only 3 days exposure there was substantial delignification at veneer...
P D Evans, K J Schmalzl, A J Michell


Screening techniques for potential wood preservative chemicals. Proceedings of a special seminar held in association with the 10th Annual Meeting of the IRG, Peebles 1978. Report No 136, 1979
1980 - IRG/WP 2138
This paper continues following issues: I. SCREENING INSECTICIDES 1) R W Berry (BRE/PRL, UK): Screen testing of insecticides for use in remedial wood preservatives. 2) D J Cross (FRI, New Zealand): Rapid screening of contact insecticides for use on forest products. 3) C R Coggins; A Forsyth; A E Glaser (Rentokil, UK): Experience in the use of indicative screening techniques for termiticides. ...
Anonymous


Laboratory tests on the natural durability of timber methods and problems
1984 - IRG/WP 2217
In literature a large variety of test methods is mentioned to examine the natural resistance of timber against fungal attack. This concerns the kind of sampling as well as the test procedure, the test fungi, the duration of test, and the classification of the resistance according to the test results. These variations, however, are of great influence on the test result. Long term exposure will lead...
H Willeitner


A dynamic approach to assess the modulus of elasticity in wood decay testing
1998 - IRG/WP 98-20139
In this study, the changes in elastic behaviour and mass losses of different hardwood and softwood species exposed to decay in a laboratory soil tests were assessed. Wood decay was monitored using different assessment methods, namely: mass loss and changes in elastic behaviours (MOE) determination. Elastic changes were determined by static and dynamic methods, for the latter, acoustic technique wa...
L Machek, H Militz, R Sierra-Alvarez


The comparative resistance to fungi of the wood munika (Pinus heldreichii Christ.), fir (Abies alba Mill.) and spruce (Picea excelsa Poir.) compared with Pinus sylvestris L. and some physical and mechanical characteristics of munika
1981 - IRG/WP 1129
The munika (Pinus heldreichii Christ.) is situated primarily in the Balkans, and partially in the south of the Apenine peninsula. As an endemic species, with a very little annual increment, it has not been used enough as a timber for mechanical conversion up till now, although the oldest trees can grow to 27 m in height, with a diameter at breast height of about 60 cm. According to data of many Ba...
M Petrovic, M Miric


Assessing the importance of degradation mechanisms on the loss of effectiveness of wood preservatives
2000 - IRG/WP 00-20193
Accelerated ageing systems developed for application to samples in the laboratory prior to biological tests, should reflect those natural deterioration processes that are likely to occur in the hazard classes defined in EN 335-1. Losses through evaporation or the effects of leaching have been recognised, however their importance, relative to other mechanisms has not been quantified. Degradation me...
E D Suttie, R J Orsler, T Dearling


Nasutitermes exitiosus and wood-rotting fungi in Eucalyptus regnans, E. acmenioides, E. wandoo, and E. marginata: force-feeding, laboratory study
1985 - IRG/WP 1231
Under a force-feeding regime, the termitid Nasutitermes exitiosus was fed on four eucalypt timbers infested with several fungal species to investigate the influence of such fungus-infested timbers on mass of wood lost, termite biomass, fat content and water content. The results showed that wood mass losses were markedly affected by species of fungi and timber. The interaction of fungi and timbers ...
D B A Ruyooka


Wood decay of Pinus sylvestris L. and Fagus sylvatica L. by marine fungi. Part 2
1991 - IRG/WP 1471
The water-logged wood conservation requires a good knowledge of the wood decay organims which produce the degradation. Previous conducted studies (ESCORIAL, TROYA, GARCIA DE LOS RIOS, 1990) have shown that the incubation times normally used for in vitro laboratory tests are not sufficients for a significant wood degradation. This has been the reason why the aim of this work was the study of such d...
M T De Troya, A M Navarrete, M C Escorial


Developments in unsterile soil soft rot testing
1984 - IRG/WP 2210
Two unsterile soil test methods, the soil burial technique and a method using vermiculite burial with soil inoculation, were compared using different soils to determine their effectiveness in evaluation of wood preservatives against soft rot. Isolation of fungi and microscopy of decayed wood indicated that both methods produced accelerated soft rot attack in treated and untreated birch. Vermiculit...
P A McKaig


Silicon tetrachloride: A potential wood preservative
1980 - IRG/WP 3133
In its present form, this paper is a preliminary draft of a paper that will eventually be submitted for publication in the Forest Products Journal. We are continuing the work on the effects of silicon tetrachloride on wood and expect to have additional data for the meeting in May 1980. Specifically we are measuring the penetration rate and depth of SiCl4, and we are chemically analyzing the treate...
C W Owens, W T Shortle, A L Shigo


Estimation of mycelial biomass by determination of the ergosterol content of wood decayed by Coniophora puteana and Fomes fomentarius
1989 - IRG/WP 1415
The mycelial biomass of fungi decomposing wood materials may be estimated by the use of an ergosterol assay technique.ln decay tests, essentially according to EN 113, estimates made by HPLC analyses on wood decayed by Coniophora puteana and Fomes fomentarius show the increase in biomass in the wood blocks. The ergosterol contents were correlated with dry weight loss determinations. Degradation of ...
K Nilsson, J Bjurman


Influence of variable lignin content amongst hardwoods on soft-rot susceptibility and performance of CCA preservative
1982 - IRG/WP 1151
This paper presents the outline of an argument, based on both new and established data, which relates varying lignin content to variation of soft-rot susceptibility between hardwood species and of performance of CCA preservatives in controlling soft-rot. Although more data need to be generated to prove this relationship, sufficient evidence exists for the hypothesis to be given close attention, pa...
J A Butcher, T Nilsson


Effect of moisture and cellulosic substrate on decay of hardwoods by soft-rot fungi
1982 - IRG/WP 2173
The development by Forintek Canada Corp. of standard test procedures for laboratory preservative evaluations using soft-rot fungi was requested by the American Wood Preservers&apos; Association. In Europe, through cooperative studies in the International Research Group on Wood Preservation, several attempts have been made to produce a standard procedure, but variability in results obtained bet...
A Byrne, R S Smith


Collaborative soft rot tests: Statistical treatment of results of soil analyses
1971 - IRG/WP 29
Institutes taking part in the collaborative experiments already reported forwarded samples of the soils employed in the tests to the Forest Products Research Laboratory, England. The soils were then autoclaved sterilised under uniform conditions and sent to the Department of Forest Soils, the Royal College of Forestry, Stockholm, Sweden. The results of the soil analyses are given in Table 1, toget...
A F Bravery


Use of compression strength loss for measuring decay in the soil block test
1996 - IRG/WP 96-20083
The possibility of using radial direction compression strength of wood, rather than mass loss, was evaluated for both a brown-rot fungus (Gloeophyllum trabeum) and white-rot fungus (Trametes versicolor). With untreated pine wafers (5 x 19 x 19 mm³ - l x r x t) exposed to Gloeophyllum trabeum in a soil block test for five days, the compression strength loss was nearly 50% compared to a 5% mass los...
D D Nicholas, Zhongwei Jin


On the nature of the tertiary wall in wood cells. Summary of lecture given at 9th Annual Meeting, Noordwijk-aan-Zee, Holland
1977 - IRG/WP 169
During recent discussions on the possible causes of failure of treated hardwood species by soft rot fungi, the uneven micro distribution of toxic components was found to be of importance; this might be attributed to a restricted diffusion of the preservative from the cell lumina into the cell wall.·In this context, the nature of the tertiary wall as the inner lining of wood cells merits special a...
W Liese


The loss of insecticidal action from synthetic pyrethroid-treated wood samples: The effect of high temperatures and relative humidities
1992 - IRG/WP 92-1569
This paper describes the results from bioassays using Hylotrupes bajulus, and chemical analyses, of pyrethroid-treated wood samples following storage for up to 3 years. A range of four storage environments was used consisting of combinations of two temperatures (20°C and 40°C) and two relative humidities (60% and 90%). It is concluded from the chemical analyses that, although losses at room temp...
R W Berry, S J Read