Initial investigations into the spalting potential of Peruvian hardwoods
2014 - IRG/WP 14-10813
This study was performed to determine if several moderately-utilized Peruvian hardwoods had potential for spalting applications. We applied a modified decay jar methodology with six native Peruvian woods and three moulds, with a period of incubation of six weeks. Results showed that Nigrospora sphaerica and Marupa (Simarouba amara) resulted on the highest significant internal pigmentation (black),...
S M Vega Gutiérrez, S C Robinson


The activity of a wood-decaying fungus during drying and rewetting cycles measured by isothermal calorimetry
2013 - IRG/WP 13-20526
Wood decaying fungi are an essential part of any ecosystems as they are the main decomposers of cellulose and lignin-containing materials. But as wood is a common building material the risk for decay fungi growth and subsequent degradation of our construction material is a concern. There are important physiological aspects of the growth and activity of decay fungi that are unknown today, and witho...
S Johansson, L Wadsö, A Pilgård, G Alfredsen


Comparison of moisture loss and its increment during the rehearsal process based on natural drying and water soaking application with or without sealing the trial discs of Common black poplar (Populus nigra L.)
2013 - IRG/WP 13-40639
This study was subjected to be set up to prove the pattern of moisture loss and moisture increment within the same wood samples prepared as the discs (30x23±3 cm diameter) with or without the bark intact during drying and in the duration of the water soaking application. In this concept, wood was exemplified by Common black poplar (Populus nigra L.) of the five 12 year old trees that are grown in...
I Usta


A screening of factors that might influence the result of laboratory decay tests
2014 - IRG/WP 14-20548
Laboratory fungal decay tests provide important tools for performance testing of wood materials. But they are also hampered with some uncertainties regarding reproducibility. In addition to variation between fungal species and strains the test conditions are also believed to have some influence. The aim of this study was to screen the effect of a selection of test parameters that might influence t...
E Larnøy, G Alfredsen, A Treu, S Kolstad


Encapsulation Systems Combined with DOT Borate Treatments – The Future of Treated Crossties
2014 - IRG/WP 14-40670
Borates have been utilized in wood protection systems for many decades but only recently have been used in North America to treat crossties. This colorless, ordorless and very effective wood protection chemical has the ability to arrest and prevent the colonization of wood by both basidiomycete decay fungi and insects such as beetles and termites while ties are air seasoning or in service. Since ...
S C Kitchens, T L Amburgey


Best handling practices for wood crossties (sleepers)
2015 - IRG/WP 15-40714
Wooden crossties (sleepers) dominate the rail industry in the USA. Most ties are hardwood treated with oil-borne preservatives using pressure treatment. Incipient decay (called ‘stack burn’) commonly develops during the pre-treatment drying process and reduces tie performance and longevity. Practices to minimize stack burn and enhance wooden tie performance are discussed as an aid to non-wood ...
N Irby, J Lloyd, A Taylor, J Watt


Effects of fungal exposure on air and liquid permeability of nanosilver- and nanozincoxide-impregnated Paulownia wood
2016 - IRG/WP 16-30680
Effects of aqueous dispersion of silver and zinc-oxide nano-particles on air and liquid permeability of Paulownia wood exposed to T. versicolor were studied in the present research project. Specimens were also heat-treated at 100 and 150°C and compared with the control specimens. Permeability values were measured when the moisture content of the specimens was 12%. Results showed significant incre...
H R Taghiyari, A Kalantari, M Ghorbani Kookandeh, F Bavaneghi, M Akhtari


Three-Dimensional Digital Image Correlation of Strains in Profiled Wood Decking Exposed to Wetting & Drying
2017 - IRG/WP 17-20611
We use three dimensional digital image correlation to measure the strains that develop at the surface of profiled radiata pine (Pinus radiata D. Don) deck boards subjected to a wetting and drying cycle. We hypothesise that surface profiling will change the pattern of strain distribution at the surface of deck boards by concentrating stresses at the base of profile grooves. Five groups of three deck board samples were produced from five different pieces of machine stress-graded radiata pine wood. Two wavy profiles, ribble or ripple, were tested. Flat unprofiled boards acted a control. Each board was fixed to a rigid frame and subjected to a wetting and drying cycle. Full field surface strain data was collected using 3D digital image correlation. Strains varied across the surface of both flat and profiled boards. Profiling changed surface strain patterns; strain maxima and minima developed in the profile ridges and grooves during wetting, respectively, but this pattern of strains reversed during drying. Such a pronounced reversal of strains was not observed when flat boards were exposed to wetting and drying, although there was a shift towards negative strains when flat boards were dried. We conclude that profiling changes surface strain distribution in deck boards exposed to wetting and drying, and causes high strains to develop in the grooves of profiled boards. These findings help explain why checks in profiled deck boards are mainly confined to profile grooves where they are difficult to see, and the success of profiling at reducing the negative effects of checking on the appearance of wood decking.
J Mallet, S Kalyanasundaram, P D Evansa


Durability of energy efficient wooden buildings: a building physical point of view
2017 - IRG/WP 17-40812
The drive for more energy efficient and sustainable buildings resulted in an increased popularity of wooden buildings, even in countries with a masonry tradition. Often guidelines and prescriptions then are copied from other countries. Different climatic boundary conditions and tradition of finishing, though, do require different moisture tolerance criteria. This is clearly the case for water vapo...
S Roels, J Langmans


Influence of Drying Condition of Wood on Rusting of Nail
2019 - IRG/WP 19-40887
Recently in Japan, the durability of metal joint in wooden structures become important. Revised Building Standard Law was enacted in 2000 and Act on the Promotion of Popularization of Long-life Quality Housing was enacted in 2008 in Japan. Since then, the durability of the metal joints in the wooden houses becomes important. But there are not any detailed regulation for the durability of the metal...
H Ishiyama, N Wada, T Nishimura, T Mori


Sterilization of Large Timbers during Preservative Treatment: How Quickly We Forget
2020 - IRG/WP 20-40902
Air seasoning is a common method of moisture management in utility poles and is done de facto during pole storage prior to treatment. However, extended air drying prior to treatment encourages fungal attack and can facilitate establishment of decay fungi in poles before a protective preservative barrier is applied. This problem can be mitigated by proper air-seasoning methods coupled with heat ste...
G Presley, J Cappellazzi, M Konkler, K Maguire, R Nelson, J J Morrell


Hydrophilization of wood using a FE-DBD air plasma
2020 - IRG/WP 20-40907
One of the goals of surface protection of wood with coatings is to prevent the evolution of moisture in wood, which accelerates its degradation by abiotic and biotic factors. Good wettability of wood is a necessary pre-condition for sufficient protection with water-based coatings. Treatment of wood surface with atmospheric dielectric barrier discharge in configuration with a floating electrode was...
J Žigon, M Petrič, S Dahle


Impacts of elevated moisture levels and subsequent drying on screwed
2023 - IRG/WP 23-40970
Mass timber (glue-laminated timber, cross laminated timber (CLT) and laminated veneer lumber) are increasingly used in mid-to high rise structures in Australia where the climate is mainly sub-tropical with elevated moisture levels and high termite risk. Moisture intrusion poses a major challenge anywhere but becomes more critical under these conditions. Untreated/non-durable materials are consider...
C M T Roder, C D Gerber, J J Morrell


The impact of pre-drying on treatment level variations of esterified solid wood analysed by X-ray densitometry
2023 - IRG/WP 23-40977
Wood modification requires homogenous treatment levels within the wood matrix to prevent insufficiently treated areas being subject to biodeterioration. Esterification of wood by citric acid and sorbitol can show differences in density caused by uneven chemical distribution during the curing phase and can be detected by x-ray densitometry. This study used density profiling to investigate the influ...
A Treu, S O Amiandamhem, E Larnoy


Eradication of beetles attacking wooden historical buildings by humidity-controlled warm-air treatment
2023 - IRG/WP 23-11028
Humidity-controlled warm-air treatment is a method that kills mainly beetles that are damaging the wood. In this process, a heat-insulating and airtight covering is placed around the object building, and the temperature inside the covering is gradually raised to about 60°C, held for a certain period of time, and then gradually lowered. While maintained at 60°C, all forms of damaging insects - ad...
Y Fujii, Y Fujiwara, M Harada, H Kitahara, M Shimada, S Kondo, Y Sato, M Shimada, R Kigawa, H Watanabe, Y Komine, S Hidaka, D Ogura


Phytosanitary heat treatment of wood in a laboratory drying oven and, in a pilot-scale kiln using the house longhorn beetle (Hylotrupes bajulus) larvae as a model
2024 - IRG/WP 24-20722
International trade in wood products brings the risk of the movement of tree pests which can cause devasting ecosystem and economic damage. International phytosanitary guidelines were created to help countries that import wood products. Import requirements intend to minimize pest spreading. Thus, the ISPM 15 (International Standards for Phytosanitary Measures No. 15) which specifies the “Regulat...
B Rubio, C L’Hostis, M Montibus, I Paulmier, C Brunet, L Charron, J-P Gaussorgues, C Guiberteau, V Vlahakis, F-R de Cibon, I Le Bayon


Previous Page