IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 631 documents. Displaying 25 entries per page.


Performance of Two Imidacloprid-Treated Malaysian Hardwoods in an Accelerated Aboveground Termite Test
2005 - IRG/WP 05-30389
The performance of the chloronicotinyl insecticide imidacloprid as a wood protecting termiticide, under a simulated Malaysian biological hazard class H2 (exposure aboveground indoors against termites and wood borers), was evaluated by a novel termite field test protocol. Replicate end-grain sealed air dried test blocks (20 x 20 x 20 mm) of two Malaysian hardwoods, Kembang Semangkok (Scaphium spp.)...
A H H Wong


An investigation of the factors influencing the rate of deterioration of timber samples due to microfungi in laboratory tests
1997 - IRG/WP 97-20116
An investigation was performed into the comparative performances of test 1 (vermiculite burial) and test 2 (soil burial) as described in ENV 807. Two test preservatives were used - copper naphthenate and propiconazole. Copper chromate was included as a reference preservative. The wood species used was beech (Fagus sylvatica). Test 1 was performed using both a mixed inoculation of the five stipulat...
I J Herring, D J Dickinson, S M Gray, J K Carey


Soil treatment tests with the three products of boric acid for the prevention of the hyphal growth of Serpula lacrymans
1992 - IRG/WP 92-3693
Laboratory soil treatment tests were conducted for the evaluation of fungicidal or fungistatic effect of boric acid products against Serpula lacrymans. Boric acid products tested were the following three: a thickened boric acid solution in triethanolamine, boric acid-silica gel complex granules, and a nonwoven fabric laminated with a polypropylene film and coated with boric acid granules on one si...
S Doi, A Yamada, Y Mineki, M Mori


Relative merits of laboratory and field tests for assessing wood decay resistance
1993 - IRG/WP 93-20009
Laboratory and field trials have long been employed for assessing natural durability of a variety of wood species, but there is a continuing debate concerning the relative merits of approach. While laboratory tests provide carefully controlled conditions for decay, they are often criticized for being too artificial to produce meaningful results. Conversely, field trials often vary widely between t...
T C Scheffer, J J Morrell


Termite physical barriers: Update on retrofitting Granitgard around 'mock up' buildings after four years
1996 - IRG/WP 96-10140
This field experiment was installed four years ago (March 1992) to evaluate the effectiveness of graded crushed granite stone, commercially marketed under the name, Granitgard, as a physical termite barrier when retrofitted around 'mock-up' buildings. The field site is located at Walpeup in the semi-arid mallee region of north-west Victoria (360 km from Melbourne), and there are ...
B M Ahmed, J R J French


Leaching of preservative components from pine decking treated with CCA and copper azole, and interactions of leachates with soils
2001 - IRG/WP 01-50171
Radiata pine decking was treated with CCA and copper azole preservatives to Australian H3 retention using conventional and modified Bethel schedules, and air-dried. Treated decking boards and durable hardwood controls were subjected to leaching in weather-exposed decks, and matching 19mm cubes were leached in extended AWPA E11-97 lab tests. Deck runoff and E11 leachate water was analysed after rai...
M J Kennedy, P A Collins


Field tests with Antiblue and Biocide TT for the prevention of sapstain and mould fungi on Pinus elliottii timber
1992 - IRG/WP 92-3682
Freshly cut and sawn Pinus elliottii timber was dipped in four concentrations of Antiblue (active ingredient sodium pentachlorophenate) and Biucide TT (local substitute), at four immersion times and stacked in the open at Chisengu sawmill. Five weeks later, the timber was assessed for the incidence and intensity of stain and mould. The results showed that Antiblue was the better chemical providing...
A J Masuka


Some studies on fungal deterioration of rubber wood (Hevea brasiliensis)
1980 - IRG/WP 2140
For the sreening of anti-stain chemicals trials with selected agricultural fungicides and new chemicals were carried out. Botryodiplodia theobromae, Aspergillus sp. and Penicillium sp. were used at test organisms. For testing the durability of rubber wood (Hevea brasiliensis) suitable local rotting fungi (Basidiomycetes), based on high degrading power, which may later be employed in standard tests...
A Sujan, A G Tan, M Stevens


Occurrence of wood-boring pholads in Kochi harbour waters (south-west coast of India)
1992 - IRG/WP 92-4175
The paper reports the occurrence of four species of wood-boring pholads (Pholadidae: Martesiinae), namely Martesia (Martesia) striata (Linnaeus), Martesia (Martesia) fragilis Verrill and Bush. Martesia (Particoma) nairi Turner and Santhakumaran and Lignopholas fluminalis (Blanford), in the Kochi back-waters, south-west coast of India. Of these Martesia nairi and Lignopholas fluminalis are now reco...
L N Santhakumaran, M V Rao


Toxic values derived from EN 113 tests - are they determined by the virulence of a test fungus? - Results from a round robin test -
1999 - IRG/WP 99-20176
The virulence of Coniophora puteana BAM Ebw. 15, the obligatory test fungus on softwood in tests according to EN 113, is known to be rather inconstant at least in some laboratories. The mass losses of untreated Scots pine sapwood blocks in an EN 113 test may range from below 20% to up to more than 50%. Possible reasons for these differences as well as the impact of a low virulence on the toxic val...
H Leithoff, R-D Peek, H V Borck, R Goettsche, H Kirk, M Grinda


Preliminary evaluations of a small wafer assay for screening potential biological control agents
1989 - IRG/WP 2332
Screening potential biological agents for controlling wood decay fungi poses a dilemma. The ideal test would eliminate as many variables as possible. Most tests utilize pure cultures of the test organism on an artificial media which in no way resembles wood. The use of sawdust improves this approach, but the sawdust increases fungal access to the lignocellulose matrix, potentially inflating the im...
C M Freitag, J J Morrell


The evaluation of the effectiveness of wood preservatives by means of IUFRO's method for field tests with wooden stakes
1985 - IRG/WP 3348
Pinus elliottii and Eucalyptus saligna stakes treated with CCA-A, CCA-C, CCB, Cashew Nut Shell Oil and Benzotar solutions were exposed in seven test sites in Sao Paulo State, Brazil. After five years of exposure, between oil-borne preservatives Benzotar show better performance than CNSL (cashew nut shell liquid), and within waterborne preservatives the performance of CCB is not so good as that of ...
G A C Lopez, A M F Oliveira, E S Lepage


Leaching of active components from preservative-treated timber. Stages 2 & 3: Laboratory testing and comparison with semi-field testing
2004 - IRG/WP 04-20303
This part of the project is focussed on leaching from preservative-treated wood obtained by the laboratory test method CEN/OECD draft guideline, February 2003 ”OECD guideline for the testing of chemicals proposal for new guideline XXX. Estimation of Emissions from Preservative-treated Wood to the Environment: Laboratory Method for wood held in the storage yard after treatment and for wooden comm...
N Morsing, B Lindegaard


Current status of AAC preservatives in New Zealand
1980 - IRG/WP 3141
Two types of alkylammonium compounds (AAC) have been approved as commercially acceptable wood preservatives by the NZ Timber Preservation Authority (TPA). They are alkyldimethylbenzyl ammonium chloride and alkyldimethylamine acetate, both of which must contain either (a) 70% alkyl chains of C12 + C14 and less than 10% of any other individual chain length, or (b) 85% alkyl chains of C12 + C14 with ...
J A Butcher


Accelerated diffusion treatment of sawn Sitka spruce grown in the UK
1986 - IRG/WP 3395
The treatment of 'green' sapwood and heartwood of Sitka spruce by diffusion methods was investigated. Steam/dip treatment processes gave increased solution uptakes and depths of penetration of copper in comparison with a simple dip treatment. Further investigation is required to reduce diffusion gradients with copper based formulations and to improve the penetration of '...
R J Murphy, D J Dickinson


Co-operative research project on L-joint testing. Progress report to March 1986
1986 - IRG/WP 2272
Further sets of data received from CTFT (France) after 18 months exposure, BAM (Germany) after 18 months exposure, STU (Sweden) after 9.5 months exposure and TI (Denmark) after 12 and 17.5 months exposure are presented and discussed in conjunction with data previously reported. The new data are generally in agreement with those presented previously and indicate the major difference between the co-...
J K Carey, A F Bravery


Results on field stake tests against termite – Maximum for 8 years examination at Kumamoto in Japan
2003 - IRG/WP 03-10463
Various preservative treated or modified wood and charcoal painting stakes were tested in field, maximum for eight years in Kumamoto, distributed two main termite species, Coptotermes formosanus and Reticulitermes speratus. After two years in field, untreated sapwood of sugi (Cryptomeria japonica) were observed severe attacks by termites, but the preservative treated stakes were observed no signif...
K Suzuki


Nasutitermes exitiosus and wood-rotting fungi in Eucalyptus regnans, E. acmenioides, E. wandoo, and E. marginata: force-feeding, laboratory study
1985 - IRG/WP 1231
Under a force-feeding regime, the termitid Nasutitermes exitiosus was fed on four eucalypt timbers infested with several fungal species to investigate the influence of such fungus-infested timbers on mass of wood lost, termite biomass, fat content and water content. The results showed that wood mass losses were markedly affected by species of fungi and timber. The interaction of fungi and timbers ...
D B A Ruyooka


A field test with anti-stain chemicals on sawn pine timber in Brazil
1989 - IRG/WP 3513
Field tests were carried out in São Paulo State - Brazil, to evaluate pre-treatment formulations of O-Phenyl-Phenol (OPP) based products. The Sodium Pentachlorophenate solution was used as a reference formulation. The treated test blocks were stacked in a covered shed, and in an uncovered place for air drying. The evaluation was done by measuring the percentage of stained surface on each test blo...
M B B Monteiro, S Brazolin


Wood decay of Pinus sylvestris L. and Fagus sylvatica L. by marine fungi. Part 2
1991 - IRG/WP 1471
The water-logged wood conservation requires a good knowledge of the wood decay organims which produce the degradation. Previous conducted studies (ESCORIAL, TROYA, GARCIA DE LOS RIOS, 1990) have shown that the incubation times normally used for in vitro laboratory tests are not sufficients for a significant wood degradation. This has been the reason why the aim of this work was the study of such d...
M T De Troya, A M Navarrete, M C Escorial


Artificial weathering as an aid to assessing the effectiveness of chemicals for preventing blue stain in service - a co-operative study
1984 - IRG/WP 2215
The paper reports co-operative studies carried out within Working Group II of the International Research Group on Wood Preservation to assess the effects of different artificial weathering systems on the performance of fungicides to control blue-stain in service. It has been shown that Atlas, Xenotest and Marr equipments operated according to particular standard schedules can give essentially the ...
A F Bravery, D J Dickinson


Cyclic delamination analysis of preservative-treated wood/FRP interfaces
2002 - IRG/WP 02-40244
Wood preservative chemicals can interfere with adhesive properties when bonding wood laminates or wood/FRP (Fiber Reinforced Polymer) laminate composites. In this work we studied the effects of various wood preservative treatments, and pre- and post-treatment on wood/wood and wood/FRP bond durability using a severe cyclic delamination test (ASTM D-2559). Pre-treatment of individual laminates with ...
C Tascioglu, B Goodell, R Lopez-Anido


Collaborative soft rot tests: Tests conducted at Princes Risborough and Delft on soil samples from collaborating laboratories
1972 - IRG/WP 210
The laboratories which took part in the original collaborative soft rot test (Savory and Bravery, Holz u Org 5 (1) 58-90, 1970) sent samples of the soil used in the original test to Princes Risborough. Portions of this material were sent to Dr Hof for soil analyses at TNO and the remainder was employed at Princes Risborough for the conduct of comparative tests of soil virulence when used as a comb...
J G Savory


Leaching from CCA-treated wood submerged in seawater: Effect of high loadings, and a comparison between laboratory and marine conditions
1996 - IRG/WP 96-50080
This study of leaching examined the following variables: CCA loading; marine versus laboratory exposure and length of submergence. Blocks of Pinus sylvestris were treated to a range of nominal retentions from 15 to 50 kg/m³. Each block was then divided into three cubes and all transverse faces were sealed. All cubes were allowed to fix at ambient temperature for a minimum of one week. One set of ...
R M Albuquerque, S M Cragg, J D Icely


Which substrate to use in a laboratory test with soft rot micro-fungi: vermiculite or unsterile soil?
1991 - IRG/WP 2372
A draft European Standard is being proposed by CEN TC 38 in which a vermiculite-burial and a soil-burial test to be carried out in succession are required. Various experiments with both procedures were set up with CCA, CC and propiconazole-formulations. The results show that vermiculite and unsterile soil yield comparable threshold values against soft rot. This poses the question of whether a two-...
A R Valcke


Previous Page | Next Page