Fungal decay of acrylate treated wood
2004 - IRG/WP 04-30357
Natural durability of wood species is variable. Chemical wood preservatives, such as biocides are necessary for extension of their service life. Many methods have been developed to increase the resistance of wood and wood products against wood-destroying organisms during the last years. The most frequently used methods are chemical and thermal modification of wood. In wood modification the basic c...
Z Tiralova, L Reinprecht


In situ testing the influence of melamine resins on the enzymatic activity of basidiomycetes
1999 - IRG/WP 99-30194
Waterbased methanol etherificated melamine formaldehyde resins have the potential to increase the resistance of impregnated wood against wood destroying fungi. The mechanism of the increased wood durability is not clear yet. In the present paper the possible interference of melamine resins with wood degrading enzymes of Coniophora puteana and Trametes versicolor was investigated as a possible cont...
D Lukowsky, F Büschelberger, O Schmidt


Enzyme immunoassay to detect Postia placenta in field tests: Comparison of plate ELISA with hydrophobic cloth and cotton dipstick
1991 - IRG/WP 2378
Standard indirect enzyme-linked immunosorbent assay in polystyrene 96-well plates was compared to hydrophobic polyester cloth and cotton dipstick for detection of wood-derived antigens from the brown-rot fungus Postia placenta. The ease of handling, larger surface area, and economics of the latter two adsorbents were surveyed for application as field tests for detection of early decay. At high ant...
C A Clausen


Soft rot tests with soils of different origins
1984 - IRG/WP 2226
In the BAM a comparative soft rot test with 9 different types of soil (one soil each from Canada, New Zealand and Switzerland and 6 soils from laboratories in Germany) were carried out. The pH values of the different soils ranged from 3.2 to 7.1, and the amounts of organic matter were between 4 and 44% (w/w). The test specimens - Pine sapwood blocks treated with different concentrations of a CCA p...
M Gersonde, W Kerner


Physiological properties of fungal test strains according to the European Standard EN 113
1986 - IRG/WP 2258
For the discussion of the European standard EN 113 the EMPA's procedure of culturing the test fungi and the corresponding virulence of the test fungi as well as the wood moisture content at the end of the test are shown. It is mainly shown that within the standard the choice of the solvent may not be left at the test lab if reproducible results shall be obtained. The different solvents in...
E Graf, B Zgraggen, P Manser


Methodologies for termiticide testing and standardization
1993 - IRG/WP 93-10043
Standardization of testing methodologies for termiticides has been one of the main topics of discussion for Working Group 1b in recent IRG meetings. While it is agreed that there is a need to provide a standardized testing procedure for industry and regulatory agencies, concerns remain that such a standardized procedure may become an obstacle for developing better testing methods or innovations in...
N-Y Su


Ecotox Testing of Leachates as an Alternative Approach for Environmental Impact Assessment of Wood Preservatives
2002 - IRG/WP 02-50185
Driven by the implementation of the EU Biocidal Product Directive (BPD) in the environmental assessment of treated wood different methodologies and test strategies are at present under discussion within industry, regulatory authorities and standardizing comittees. Test procedures for the analytical determination of emissions to different environmental compartments according to exposure scenario...
H-W Wegen


Accidental mold/termite testing of high density fiberboard (HDF) treated with borates and N’N-naphthaloylhydroxylamine (NHA)
2003 - IRG/WP 03-10462
High density fibreboard (HDF) was made from beech and pine furnish (50:50) and treated with boric acid (0.1-3%), borax (0.1-3%) or N'-N-(1,8-naphthalyl) hydroxylamine (NHA) (0.1-1%) prior to gluing with urea formaldehyde (UF) resin in order to determine resistance to Eastern subterranean termites (Reticulitermes flavipes Kollar), the most economically important termite species in North Am...
S N Kartal, H H Burdsall Jr, F Green III


Accelerated anti-termite laboratory tests, simulation of field conditions and assessment of results for service life
1994 - IRG/WP 94-20034
Termites are one of the most serious biodegrading agents in the tropics. Though some species of termites occur in the warmer temperate regions, only a few species can withstand the rigours of colder regions. Testing of termite resistance of material is done either by field tests or by accelerated laboratory tests. Field tests, though realistic to assess service life, are elaborate, take a long tim...
P K Sen-Sarma


Method to determine the depth of penetration of the biologically active components of wood preservatives
1978 - IRG/WP 2108
A time-saving method for determining the depth of penetration of the biologically active components of wood preservatives is described. The test specimens were obtained by cutting thin slices from the wood either parallel or perpendicular to the treated surface. The slices were then exposed to fungal attack. A good correlation was found between the test results obtained by the modified German Stan...
H-P Sutter


Limitations of the Pilodyn when assessing decay in graveyard test stakes
1982 - IRG/WP 2168
The following examination was designed to evaluate more precisely the usefulness of the Pilodyn for routine, objective assessments of the condition of field test stakes and to examine its limitations, particularly in respect to: 1.) The importance of variables other than extent of decay which may affect Pilodyn readings; 2.) Practicality of obtaining multiple readings in decayed and non-decayed re...
M E Hedley


Screening test methods with termites as first laboratory evaluation of new active substances for wood preservation
1995 - IRG/WP 95-10135
European test methods (EN) with termites have been compared with long-standing experience from screening test methods in the laboratory of Eberswalde. The results are discussed in terms on the possibility of using screening test methods as the first laboratory evaluation of new active substances in wood preservatives. The advantages and disadvantages of these methods are considered. Only a small a...
W Unger


A comparison of fungal strains used in the bioassay of wood preservatives
1984 - IRG/WP 2220
Previously published data are presented relating to a number of strains of wood-destroying basidiomycetes (Coniophora puteana, Coriolus versicolor, Gloeophyllum abietinum, Gloeophyllum sepiarium, Gloeophyllum trabeum, Lentinus lepideus, Poria placenta, Fibroporia vaillantii and Serpula lacrymans) commonly used as test fungi in the bioassay of wood preservatives. The data, which has not been statis...
J Wazny, H Greaves


Soft rot test of copper/chrome/arsenic treated heartwood of three Malaysian timbers by the vermiculite-burial method. (+ correction document of 25 July 1990)
1990 - IRG/WP 2354
Heartwood of copper-chrome-arsenic (CCA) treated kempas (Koompassia malaccensis), tualang (Koompassia excelsa) and keruing (Dipterocarpus spec.) was found to be susceptible to soft rot in recent pole surveys. Standardized heartwood blocks were impregnated with 0 to 6.3% (w/v) CCA and challenged to decay for twelve weeks by a mixed inocula of Chaetomium globosum, Glenospora graphii, Humicula grisea...
R-D Peek, A H H Wong


Oral toxicity of a slow-acting insecticide Amdro® to the Formosan subterranean termite
1982 - IRG/WP 1162
The use of toxic baits to control the Formosan subterranean termite Coptotermes formosanus Shiraki requires an insecticide that is non-repellent and sufficiently slow acting that poisoned termites leave treated areas before dying. Of the many insecticides screened, only Amdro® exhibited these characteristics. The oral toxicity (LD 50) of Amdro® to Coptotermes formosanus was estimated at 12.33 µ...
N-Y Su, M Tamashiro, J R Yates III


Performance of proprietary formulations of anti-sapstain preservatives on Hevea brasiliensis timbers in laboratory tests
1989 - IRG/WP 3532
A total of 10 proprietary and two experimental formulations were assessed for their effectiveness against sap-stain caused by Botryodiplodia theobromae on Rubberwood (Hevea brasiliensis). Sterilized wood samples 5x20x40 mm³ were dipped in the test chemicals for 60 seconds and then inoculated with 0.5 ml of culture filtrate of Botryodiplodia theobromae for incubation in sterile, damp petri dishes....
L T Hong


Objectives of future collaborative soft rot tests
1972 - IRG/WP 209
Progress has been made towards acceptance of a defined laboratory test method for determining the toxicity of preservatives against soft rot fungi (Documents IRG/WP/201 and IRG/WP/208) and, at the 1971 meeting in Brussels, the framework of collaboration for the next phase of testing was discussed. Time available at Brussels did not permit restatement of objectives, consideration of the stages by w...
J G Savory


Multiple-Phase Pressure (MPP) Process: One-stage CCA treatment and accelerated fixation process. 4. MPP compared with other processes for achieving acceptable treatment of radiata pine heartwood
1998 - IRG/WP 98-40115
Although radiata pine sapwood is very amenable to preservative treatment, it is often difficult to achieve the required standard for heartwood treatment. A preliminary investigation showed that to achieve the NZ Timber Preservation Council minimum penetration requirements for radiata pine heartwood using the Multiple-Phase Pressure (MPP) Process, a hydraulic pressure of at least 1250 kPa for 20 m...
K Nasheri, J A Drysdale, G Durbin, M E Hedley


Exposure of preservative treated wood to terrestrial microcosms, pure cultures of fungi and in the field
1997 - IRG/WP 97-20114
Small stakes (5x10x100 mm3) of treated and untreated Pinus sylvestris sapwood were exposed in terrestrial microcosms with different soils, two taken from test fields in Sweden, one soil from a conifer forest and one garden compost soil. Stakes of the same size were also exposed to pure cultures of the brown and white rot fungi, Postia placenta and Phanerochaete chrysosporium. After exposure, weigh...
M-L Edlund


On the possibilities of the use of juvenile hormone in wood protection
1976 - IRG/WP 363
The annual world-wide extent of losses caused by wood-destroying insects in timber in buildings and timberyards is very difficult to estimate. In general exact values are only known in cases of claims for damages from insurance companies or in litigation. At present the best known wood destroying insects in Switzerland are the house longhorn beetle (Hylotrupes bajulus) and the common furniture bee...
P Tscholl


Co-operative research project on L-joint testing. Sampling after 4 years exposure
1987 - IRG/WP 2274
In September 1983, Document No: IRG/WP/2208 was distributed giving guidance on sampling after 8 months exposure and including tables on which to record the test results. Similarly in September 1984, Document No: IRG/WP/2233 was distributed concerning sampling after 18 months exposure. No major problems have been notified to Princes Risborough Laboratory concerning the sampling method. It is theref...
J K Carey, A F Bravery


Field test of wood preservatives with Nasutitermes rippertii RAMBUR in Cuba
1996 - IRG/WP 96-10181
A field test of wood preservatives was carried out with Nasutitermes rippertii RAMBUR in the vicinity of the Material Testing Centre „Alexander von Humboldt" in Santiago de las Vegas/ Havana (Cuba) for 12 and 24 months. Test specimens of Pinus sylvestris L., Picea abies (L.) Karst. and Fagus sylvatica L. with dimensions of 25 x 25 x 490 mm³ were arranged vertically or horizontally in a circle o...
W Unger


Screening of the technical performance and aquatic toxicity of N-methylolacrylamide treated wood
2000 - IRG/WP 00-40166
In the course of the last decades chemical modification of wood species, with a limited natural durability, has been subjected to intensive research. As a possible alternative and supplementary treatment of non-durable wood in a range of applications it remains one of the major topics in the wood preservation world. Different modification systems have been scaled-up and are now in an industrialisi...
V Rijckaert, S De Geyter, J Van Acker, M Stevens


A technique for measuring preservative loss or redistribution during leaching
1983 - IRG/WP 2199
Radiata pine sapwood stakes were treated with benzalkonium chloride (AAC) or copper-chrome-arsenate (CCA). After fixation and drying the outer 2 mm and 2-4 mm layers were removed from one radial longitudinal face. The planed face was coated with a waterproof coating and AAC-treated stakes were leached for 6, 12 or 18 weeks; 12 weeks for the CCA-treated stakes. After airdrying three 2 mm layers (0-...
J A Drysdale


The movement of iron into field test stakes
1987 - IRG/WP 2284
Failed and sacrificial stakes recovered from the Westham Island field test site were examined for their iron content. Varying amounts were recorded, which were greatest in the failed stakes. The possible role of the iron taken up by the below ground portion of the stakes, in accelerating the decay process and/or the preservative leaching is under investigation. The reaction of the iron with the ch...
J N R Ruddick, P I Morris