Effects of microclimate, wood temperature and surface colour on fungal disfigurement on wooden claddings
2012 - IRG/WP 12-20490
Wooden claddings are common in façades in Norway, and Norway spruce (Picea abies) is the most frequently used species. The cladding is a major part of the facade, and it has visual requirements that may define the aesthetic service life. The visual changes that occur during weathering can be colour changes, abrasion or wear, blistering, flaking, and even cracks in the wood or coating, but more of...
L Ross Gobakken, G I Vestøl


Durability of timber products – Part 2: Proposal for an IRGWP - Durability Database
2012 - IRG/WP 12-20497
A proposal for a web-based platform for scientific exchange of test data in the field of wood durability and wood protection has been made. The overall aim of the durability data base is to improve the usability of existing test data and to create an added value for durability research and service life prediction. The database allows for test results from standardized and non-standardized laborat...
C Brischke, L Meyer, G Alfredsen, M Humar, L Francis


Durability of timber products –Part 1: Inventory and evaluation of above ground data
2012 - IRG/WP12-20498
The material-inherent resistance of wood is one of the most important qualities influencing the durability of timber. Hence, it has also a major effect on the service life to be expected from a timber construction. In addition, design details and the respective climatic conditions determine durability and make it impossible to treat wood durability as an absolute value. Moreover, the reference mag...
C Brischke, L Meyer, G Alfredsen, M Humar, L Francis, P O Flæte, P Larsson Brelid


Testing service life for use class 3: accelerated L-joint performance of commodities
2012 - IRG/WP 12-20500
Above ground testing is considered important for the assessment of treated wood intended for use class 3. Laboratory testing of efficacy of biocides as well as of natural durability focussing on such applications has to be linked to performance and service life. An accelerated L-joint test was some 15 years ago developed at the Ghent University to allow worst case assessment under semi-controlled ...
J Van Acker, J Van den Bulcke, I De Windt, L De Vetter


Effect of an antioxidant on the efficacy of organic wood preservatives in an accelerated soil contact decay test
2012 - IRG/WP 12-30583
In comparison to inorganic wood preservatives, organic biocides in transient carriers are considerably less effective when the treated wood is exposed to soil contact. Various oils are used in some formulations with pentachlorophenol to improve the efficacy. However, use of these oils imparts unacceptable properties to products used in residential applications. Consequently, there is a need to de...
D D Nicholas, J Shi, T P Schultz, L Sites


Biological performance of wood- and bamboo-polypropylene composites: Effects of particle content, particle size and Zn borate
2012 - IRG/WP 12-40577
Particle content and size of wood material in wood plastic composites (WPCs) can affect efficacy of WPCs against fungi and termites. This study evaluated fungal and termite resistance of WPCs manufactured by using two different levels of particle content (50 and 70%) and three different particle sizes (30, 60, and 100 mesh). In fungal resistance tests, Tyromyces palustris, a standardized test fung...
S N Kartal, S Aysal, E Terzi, T Yoshimura, K Tsunoda


Durability of Furfurylated Wood – Results from Laboratory and Field Tests in the Ecobinders project
2012 - IRG/WP 12-40602
Within the EU project Ecobinders, laboratory tests were performed with furfurylated wood produced in semi-industrial scale in the factory of Kebony ASA. Field trials in Horizontal double layer decks and in-ground of transmission poles were also started. Four wood species, Southern yellow pine (SYP), maple, beech and aspen were treated to two treatment levels by using two impregnating liquids with ...
M Westin


Biodegration of treated wood waste by native fungal communities of tropical soil in French Guiana
2012 - IRG/WP 12-50285
Woods have been protected with fungicides for a long time, and the effects of these fungicides on soil after being leached into the ground have turned out to be a true environmental issue. It is in this perspective that we are proposing to study fungal communities of these contaminated woods in a purpose of bioremediation. Most of precedent studies have focused on ability of some Basidiomycetes an...
A Zaremski, L Gastonguay, C Zaremski, F Chaffannel, J Beauchêne, G LeFloch


Succession after Fire of Fungal Fruiting Bodies in Mediterranean Pinus pinaster Stands in Spain
2012 - IRG/WP 12-10789
In this study we present the results of a 4-year survey aimed at describing the succession of fungal communities following fire in a Mediterranean ecosystem in Northwest Spain, dominated by Pinus pinaster Ait. After a large wildfire in 2002, six 2 x 50 m study plots were established in burned and unburned areas corresponding to early and late succession stages. During the autumn seasons from 2003 ...
P Vásquez Gassibe, M Hernández-Rodriguez, R Fraile Fabero, J A Oria-De-Rueda, P Martín-Pinto


Triazole – based ionic liquids to protect of lignocellulosic materials against fungi
2012 - IRG/WP 12-30601
In presented paper we examined on biotic properties of novel structure of tebuconazole derivatieves: tebuconazole hydrochloride, allyltebuconazole chloride, methyltebuconazole iodide, tebuconazole dihydrocitrate. Our investigation against wood-degrading fungi were contained also the didecyldimethylammonium 3-aminotriazolate as well as didecyldime-thylammonium nitrate(V) with tebuconazole or wit...
J Zabielska-Matejuk, J Pernak, I Frąckowiak, A Stangierska, W Przybylska, M Kot


Activities of moulds on wood as a function of relative humidity during desorption and absorption processes
2013 - IRG/WP 13-10794
Three different types of indoor moulds: Penicillium brevicompactum, primary colonizer; Alternaria tenuissima, secondary colonizer and Trichoderma harzianum, tertiary colonizer, grown on wood were measured for their activities under different relative humidity levels. The activities were measured by isothermal calorimetry. The activities of the moulds changed with the change of the relative humidit...
Yujing Li, L Wadsö


High-throughput sequencing highlighted contrasted pioneer fungal communities associated to coniferous and deciduous wood preservation assays
2013 - IRG/WP 13-10800
Studying the fungal communities in the wood, in particular during the first events of the colonization, and the factors that underlie the dynamics of fungal species assemblages remain a challenge in ecology, because of the absence of fructification during the pioneer steps of wood degradation. The use of Next-generation DNA sequencing methods, which produce massive volumes of data, provided new pe...
Y Mathieu, A Dassé, I Le Bayon, M Kutnik, L Harvengt, E Gelhaye, M Buée


The chemistry of wood degradation by Basidiomycetes studied in a van Krevelen diagram
2013 - IRG/WP 13-10805
The atomic composition ratios of decayed wood by Basidiomycetes are mapped in a van Krevelen diagram. It is shown that the wood residue after decay is chemically reduced, rather than oxidized. A previously developed and verified theoretical model for thermal wood modification, relating atomic composition ratios to moisture sorption and fungal resistance properties has tentatively been applied to w...
W Willems, H Militz


Statistical analysis of durability tests - Part 1: Principles of distribution fitting and application on laboratory tests
2013 - IRG/WP 13-20504
Service life prediction is an important topic in wood research, especially with regard to the Construction Products Regulation (CPR). Both laboratory tests as well as in-service performance testing are therefore essential in combination with proper monitoring and analysis tools. A crucial concept is variability in testing and analysis, especially for a biological material such as wood. The larger ...
I De Windt, J Van den Bulcke, C Brischke, C R Welzbacher, A Gellerich, S Bollmus, M Humar,


Characterization of test fields
2013 - IRG/WP 13-20508
Test field characteristics and impact of test fields on wood degradation is important when testing wood protection. The current EN 252 standard has no requirement for knowledge of decay hazards, but most commonly a test field is known as a “brown”,- “white”,- or “soft rot” field. To understand which decay hazard wood preservatives are tested against, each test field should be character...
U Råberg, N Terziev, G Daniel


Statistical analysis of durability tests - Part 2: Principles of time-to-failure and application on field test data
2013 - IRG/WP 13-20512
Service life prediction is an important topic in wood research, especially with regard to the Construction Products Regulation (CPR). Both laboratory tests as well as in-service performance testing is therefore essential, in combination with proper monitoring and analysis tools. A crucial concept is variability and the incorporation of variability in tests and analysis. In this paper we focus on t...
J Van den Bulcke, I De Windt, C Brischke, C R Welzbacher, A O Rapp, J Van Acker


Changes of fungicidal, mechanical and sorption properties of wood during above ground outdoor exposure
2013 - IRG/WP 13-20513
The aim of this preliminary study was to investigate differences in mechanical, fungicidal, and sorption properties of four different wood species (sweet chestnut (Castanea sativa), common beach (Fagus sylvatica), Norway spruce (Picea abies), and copper-ethanolamine (CuE) impregnated Norway spruce (Picea abies)) that were exposed in the 3rd use class (CEN, 1992) for periods between 4 and 30 months...
N Thaler, M Humar


Testing the performance of timber using 27 different field test methods
2013 - IRG/WP 13-20517
Numerous test methods to determine the durability of timber and timber products have been described in relevant literature. However, only some of these methods have been standardized and thus only very few are regularly used for resistance tests in the field. Since results from extensive comparative field studies have shown differences in moisture performance between different test methods, the ai...
L Meyer, C Brischke, J Rieken


Image analysis for mould and sapstain detection on wood
2013 - IRG/WP 13-20519
Laboratory tests for mould growth on wood products are time consuming and rely on visual assessments of specimens utilizing subjective rating systems. Accelerated laboratory methods are needed that can provide rapid, quantitative assessment of mould and sapstain growth on solid and composite wood products. Image analysis of scanned spore imprints from southern pine or oriented strandboard (OSB) sp...
C A Clausen, V W Yang


Accelerated H3 above-ground decay testing
2013 - IRG/WP 13-20520
An above-ground H3 fungal field trial was installed at two sites in Australia and one in New Zealand, as well as in two Accelerated Field Simulators. The aim was to find a method that would shorten the time required for evaluating new preservatives and protection systems. One-quarter H3 retentions were installed, as first results suitable for registration occur when these reach 70% soundness. Twel...
L J Cookson, D Page, T Singh


Predicting the Rate of Decay, and the Potential for Misinterpretation of Proper Scientific Method
2013 - IRG/WP 13-20525
Predicting the rate of fungal attack in wood-based materials and its effect on properties remains the holy grail of wood products pathologists; however, achieving this goal is difficult because of the many variables associated with the process. This paper reviews some of the more important aspects of the decay process in relation to test methodology and then discusses how data are sometimes used b...
B S Goodell, J J Morrell


Cell wall properties of softwood deteriorated by fungi: combined chemical analyses, FT-IR spectroscopy, nanoindentation and micromechanical modelling
2013 - IRG/WP 13-20527
Mechanical properties of wood are determined by its inherent hierarchical microstructure, starting at the nanometer scale, where the elementary components cellulose, hemicelluloses, and lignin build up the wood cell wall material. Fungi cause degradation and decomposition of these components and, thus, alter the mechanical properties of wood. The aim of this study is to gain new insight into these...
L Wagner, T K Bader, K de Borst, T Ters, K Fackler


Development of a rapid method to assess the rate of fungal colonization of wood
2013 - IRG/WP 13-20531
Testing of wood durability is today done mainly with accelerated exposure tests under rather realistic conditions (in ground, outdoors with moisture traps etc). Although such tests are accelerated with respect to the conditions that outdoor exposed wood structures are exposed to, they tend to take rather long time. The present paper presents the development of a rapid method intended to assess at ...
L Wadsö


Fungal laccases as a tool for wood functionalization
2013 - IRG/WP 13-20533
Wood degrading fungi are the most important production organisms for laccase, a promising oxidative biocatalyst with numerous biotechnological applications in the forest products industry. Laccases are multi-copper containing oxidases (EC 1.10.3.2), which catalyse mono-electronic oxidation of phenols, polyphenols and anilines at the expense of molecular oxygen. Interest in these essentially ‘eco...
M Schubert


Report on COST E37 Round Robin Tests – Comparison of results from laboratory and field tests
2013 - IRG/WP 13-20535
A round robin involving 15 European participants was set up in 2006. The round robin consists of both a field test according to the double layer test method and a laboratory test with two different preconditioning methods. When comparing EN 84 preconditioning (two weeks water leaching) with natural preconditioning (1 year in field, above ground) according to CEN/TS 15397, no significant difference...
M Westin, E Conti, J Creemers, P-O Flæte, A Gellerich, I Irbe, M Klamer, B Mazela, E Melcher, R Möller, L Nunes, S Palanti, L Reinprecht, E Suttie, H Viitanen