Comments on leaching in view of accelerated testing
1977 - IRG/WP 294
We developed an accelerated test for leaching at elevated temperatures (75-85°C). This test was used for the examination of 11 preservative formulations containing Cu, Zn and As. The data obtained from these experiments were compared with data on some formulations tested by ASTM standard leaching test. The method consists in making a large surface to volume ratio of wood from a treated block by c...
J Rak


Mechanical properties of CCA-treated southern pine after post-treatment kiln drying
1989 - IRG/WP 3543
This report reviews current research dealing with the effects of waterborne preservative treatment and redrying on the mechanical properties of wood. In general, waterborne preservative treatments reduce average mechanical properties. This effect is exaggerated when treated wood is kiln-dried after treatment, especially at elevated temperatures. For lumber, recently completed research at the Missi...
H M Barnes, J E Winandy


Thermotolerant moulds on timber during kiln drying
1980 - IRG/WP 1109
In recent years a special disease named the wood trimmer's disease has been observed with increasing frequency among saw mill workers. Particularly workers in the trimming department have been affected. The medical symptoms are usually high fever, ague headache, pain in muscles and joints. It was shown that the disease was of immunologic nature and caused by over-exposure to spores from m...
B Henningsson


Effect of post-treatment drying schedule on the modulus of elasticity of CCA-treated southern pine dimension stock using nondestructive methods
1987 - IRG/WP 3413
This paper describes the results from the nondestructive testing for modulus of elasticity (MOE) of southern pine (Pinus sp.) 2 x 6's treated with chromated copper arsenate and redried using three commercial kiln schedules. The data indicate that redrying CCA-treated southern pine dimension stock treated to above-ground retentions (4 kg/m³) has no deleterious effect on the MOE, regardles...
H M Barnes, S Moore


Possible durability transfer from durable to non durable wood species. The study case of teak wood
2001 - IRG/WP 01-10392
Teakwood is well known for its excellent natural durability, mostly due to its high proportion of extracts. Amongst these extracts, quinones, and more precisely some naphtoquinones (such as lapachol) and anthraquinones (such as tectoquinone) appear to play a crucial role in the resistance to wood decay organisms. At a laboratory scale, sawdust from malaysian teak heartwood has been extracted under...
M-F Thévenon, C Roussel, J-P Haluk


Kiln drying of LSOP treated timber: rate of solvent evaporation, overpaintability and recovery of the solvent
1992 - IRG/WP 92-3711
The rate of solvent evaporation from LOSP treated timber dried in a kiln at 35°C has been investigated. Around 50% solvent removal has been found to be consistent with good overpaintability using a water based acrylic primer. It has been demonstrated that an activated carbon solvent recovery system is capable of removing all the solvent vapour from the outlet of a commercial joinery drying kiIn, ...
P Warburton, L B Sheard


Standard and accelerated testing of boron-additive wood protection systems
2005 - IRG/WP 05-30381
The main objective of this research was to determine the effectiveness of boron-additive protection systems for above ground applications by means of field testing. The two field test procedures used are based on the L-joint test described in the European standard EN 330. For the first set up the boron treated timber was coated in accordance with the standard EN 330 system. The second set up is ba...
A Mohareb, J Van Acker, M Stevens


Co-operative studies on determining toxic values against wood-destroying basidiomycetes: Progress report to April 1990
1990 - IRG/WP 2357
This document reports progress on the co-operative study between nine laboratories, set up following the proposals contained in Document IPG/WP/2316 (1988). Results have been received from eight laboratories. Toxic values data have been established successfully for the test fungus Coniophora puteana with soil, malt agar and vermiculite methods and with the test fungi Gloeophyllum trabeum and Poria...
J K Carey, A F Bravery


Evaluation of the protective means of some wood preservatives by means of accelerated tests
1973 - IRG/WP 232
In site conditions of the eastern site in the forest-steppe part of the Krasnovarsk region, the relative effectiveness of a series of wood preservatives was obtained by means of field tests. To obtain a more accurate evaluation of the protective qualities of these accelerated tests were carried out in laboratory conditions. In 9 boxes filled with non-sterile soil taken from the site, 72 samples of...
I A Petrenko


Survey of conditioning treatment practices in the Philippines
1975 - IRG/WP 349
The wood preservation industry in the Philippines is at present beset by many problems. An association of the industry similar to those existing in other countries has only been initiated last year by FORPRIDECOM. It is hoped that the formal organisation of this association will bring into focus the importance of this particular industry in the economic and industrial development of the country. L...
R F Casin


A new concept for the evaluation of wood durability for out of ground contact using accelerated L-joint testing
1997 - IRG/WP 97-20123
Since the wood preservation sector is developing in favour of defining exactly the utilization of wood products and preservation techniques as a function of the envisaged hazard class, more in particular the hazard classes 3 and 4 (EN 350) there is obviously a need for a test method evaluating natural durability for out of ground contact applications. Based on the L-joint test as described in the ...
J Van Acker, M Stevens


Accelerated testing for out of ground contact using natural biological preconditioning
1996 - IRG/WP 96-20088
Small blocks made of Scots pine sapwood were treated, buried in vermiculite and exposed to natural microbial colonisation during outdoor exposure prior to laboratory decay testing. Periodic microbial isolations, moisture content, permeability and weight loss tests were also conducted. Bacteria and moulds colonised the vermiculite and miniblocks well. Aureobasidium pullulans was common on TnBTO tre...
S Molnar, D J Dickinson, R J Murphy


A trial of "sour" felling to prevent bluestain by depletion of sapwood nutrients
2001 - IRG/WP 01-10404
Discoloration of conifer wood caused by bluestain causes large economic losses in Canada. Most deep stain develops in the log stage during storage or transport. In a search for control strategies that will not disrupt woodlands productivity we tested "sour" felling, termed "hagarashi" in Japan. The practice involves delaying the delimbing of freshly harvested trees. The tree continues to transpire...
A Byrne, A Uzunovic, D Minchin, C Breuil


Accelerated anti-termite laboratory tests, simulation of field conditions and assessment of results for service life
1994 - IRG/WP 94-20034
Termites are one of the most serious biodegrading agents in the tropics. Though some species of termites occur in the warmer temperate regions, only a few species can withstand the rigours of colder regions. Testing of termite resistance of material is done either by field tests or by accelerated laboratory tests. Field tests, though realistic to assess service life, are elaborate, take a long tim...
P K Sen-Sarma


Termite durability of sugi (Cryptomeria japonica) heartwood kiln-dried under high-temperature process in relation to wood extractives
2005 - IRG/WP 05-10547
Termite durability of sugi heartwood samples kiln-dried under a high-temperature process were evaluated by using Reticulitermes speratus (Kolbe) as a test termite sp. The n-hexane extractives of these samples were analysed by a GC technique. The less termite durability was shown on the wood samples dried under the high-temperature process, in comparison with that of the air-dried samples. No GC-p...
S Shibutani, E Obataya, K Hanata, S Doi


Soft rot test of copper/chrome/arsenic treated heartwood of three Malaysian timbers by the vermiculite-burial method. (+ correction document of 25 July 1990)
1990 - IRG/WP 2354
Heartwood of copper-chrome-arsenic (CCA) treated kempas (Koompassia malaccensis), tualang (Koompassia excelsa) and keruing (Dipterocarpus spec.) was found to be susceptible to soft rot in recent pole surveys. Standardized heartwood blocks were impregnated with 0 to 6.3% (w/v) CCA and challenged to decay for twelve weeks by a mixed inocula of Chaetomium globosum, Glenospora graphii, Humicula grisea...
R-D Peek, A H H Wong


Multiple-Phase Pressure (MPP) Process: One-stage CCA treatment and accelerated fixation process. 4. MPP compared with other processes for achieving acceptable treatment of radiata pine heartwood
1998 - IRG/WP 98-40115
Although radiata pine sapwood is very amenable to preservative treatment, it is often difficult to achieve the required standard for heartwood treatment. A preliminary investigation showed that to achieve the NZ Timber Preservation Council minimum penetration requirements for radiata pine heartwood using the Multiple-Phase Pressure (MPP) Process, a hydraulic pressure of at least 1250 kPa for 20 m...
K Nasheri, J A Drysdale, G Durbin, M E Hedley


Treatment groups and remedies for CCA treated hardwood and softwood poles
1999 - IRG/WP 99-40142
Different hardwood and softwood species from Bangladesh and Bhutan was investigated regarding density, green fiber stress, natural durability of heartwood and CCA treated sapwood, CCA treatability grades, sapwood thickness, and kiln-drying properties for long term use as electric poles. These properties along with the past service records for nineteen years, separated ten heardwood and five softwo...
A K Lahiry


Gaseous preservative treatment of wood
1990 - IRG/WP 3631
A recent development in processing wood with a gaseous preservative means that dry, treated wood can be produced in under 30 hours with the benefits of product diversification, faster stock turnover and the ability to respond to short term demand. About 400,000 m³ of wood are treated each year in New Zealand with boron salts to protect from borer infestation. Traditionally this treatment is effec...
R Burton, A J Bergervoet, K Nasheri, P Vinden, D R Page


The movement of iron into field test stakes
1987 - IRG/WP 2284
Failed and sacrificial stakes recovered from the Westham Island field test site were examined for their iron content. Varying amounts were recorded, which were greatest in the failed stakes. The possible role of the iron taken up by the below ground portion of the stakes, in accelerating the decay process and/or the preservative leaching is under investigation. The reaction of the iron with the ch...
J N R Ruddick, P I Morris


Studies in an accelerated soil bed facility on the decay susceptibility of U.K. grown spruce and pine poles treated with copper/chrome/arsenic (CCA) by pressurised sap-displacement. Part 1: Setting up of soil beds and initial soft rot results
1990 - IRG/WP 2344
The paper describes the methodology used in the construction and early operation of an accelerated soil bed facility used to examine the decay susceptibility of U.K. grown Scots and Corsican pine and Sitka and Norway spruce treated with C.C.A. by high pressure sap-displacememt. The design and control of the facility as well as the preparation, soil exposure and soft rot decay analysis of quarter p...
A Bruce, S D Hainey, G M Smith, B King, P D Evans


Preliminary pole treatment trials with chlorothalonil in hydrocarbon solvent
1994 - IRG/WP 94-40027
A series of 460-mm long, end-sealed southern pine pole stubs were treated with chlorothalonil in hydrocarbon solvent. Over sixty sections were treated using various combinations of initial seasoning (kiln-drying, steam-conditioning), treating temperature (ambient, 200°F), initial air pressure, and final conditioning (steam flash + vacuum, expansion bath + vacuum, steam distillation + vacuum). Dis...
H M Barnes


Application of oscillating pressure to improve treatability of refractory species
1987 - IRG/WP 3449
Under practical conditions a minimum moisture content of 80% demande by the German quality standard RAL-RG 411 can not be guaranteed throughout the year. Storage of logs with bark prolonges the drying process; a storage without bark must be avoided. A sufficient penetration according the standard can be achieved at least with a moisture content of 60%, optimal conditions may prevail between 100% a...
R-D Peek


Less pollution due to technical approaches on accelerated steam fixation of chromated wood preservatives
1988 - IRG/WP 3487
Steaming of freshly treated wood at 100°C to 120°C initiates a spontaneous fixation of copper-chromate-containing wood preservatives. For the performance, a suitable anticorrosive equipment is necessary. Good results can be achieved using a separate steaming equipment which allows a rapid heating of the wood. While warming-up, in the wood some preservative solution extends and can be partly extr...
H Willeitner, R-D Peek


Accelerated testing for out of ground contact using natural biological preconditioning: Part 2
1997 - IRG/WP 97-20108
Small blocks of scots pine sapwood were treated, buried in vermiculite and exposed to natural microbial colonisation during outdoor exposure prior to laboratory decay testing. An EN 84-type leach trial was carried out on unexposed samples. Periodic microbial isolations, moisture content, permeability and weight loss tests were also conducted. The experiment ran for 12 months. The colonisation of t...
S Molnar, D J Dickinson, R J Murphy