IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 231 documents. Displaying 25 entries per page.


Some Experiences with Stake Tests at BAM Test Fields and in the BAM Fungus Cellar Part 1: Comparison of Results of Visual Assessments and Determinations of Static Moduli of Elasticity (MOE)
2005 - IRG/WP 05-20319
With examples of routine in-ground stake tests differences are shown in the performance of wood preservatives at the BAM test fields Lehre and Horstwalde and in the BAM fungus cellar. Signs of attack of micro-organisms were assessed visually according to EN 252. Periodical determinations of static moduli of elasticity (MOE) revealed the influence of the attack on the elastic properties of the wood...
M Grinda, S Göller


Effects of chlorothalonil (CTN) and butylated hydroxytoluene (BHT) on microbial communities involved in the deterioration of wood using T-RFLP I: Accelerated laboratory decay study
2006 - IRG/WP 06-20332
The effects of Chlorothalonil (CTN) and Butylated Hydroxy Toluene (BHT) on microbial species diversity in wood and the surrounding soil are being assessed by Terminal Restriction Fragment Length Polymorphism (T-RFLP). CTN was selected as a trial organic wood preservative, and BHT is being evaluated for its synergistic effects with CTN. Results from an accelerated decay test will be presented. The...
G T Kirker, M L Prewitt, S V Diehl


Effect of wood decay on the proportional limit of thin wood samples stressed in the bending mode
2006 - IRG/WP 06-20334
When using bending stiffness as a measure of wood decay it is advantageous to repeatedly test individual samples after they are exposed to decay fungi for varying periods of time. In order to obtain reliable results, variation in modulus of elasticity (MOE) values of the test samples that are repeatable bent to a given deflection must be considered. In this study it was shown that sound 3mm thick ...
G Li, D Nicholas, T Schultz


L-joint based testing for service life prediction of exterior plywood in out of ground contact conditions
2006 - IRG/WP 06-20342
Good biological performance of several plywood types in exterior conditions is most probably related to altered wood moisture behaviour compared to solid wood. Therefore a test set up was developed, using EN 330 L-joint testing methodology, to facilitate differentiation of plywood for exterior applications. The proposed test set up is an adaptation of an accelerated L-joint method introduced by V...
J De Smet, I De Windt, J Van Acker


The Development of a novel method to preserve reeds using an environmentally friendly timber preservative and a unique engineering design.
2006 - IRG/WP 06-40335
Reeds are used in the construction of bush lodges in Northern Kwa- Zulu Natal, South Africa. Fungal, insect and ultra-violet damage to these reeds is posing a severe problem. Within a space of two years, the reeds are attacked and have to be subsequently replaced; a time consuming and costly exercise. A novel method has been used to successfully preserve these reeds with an environmentally friendl...
K Govender, K G Moodley


Accelerated assessment tests of new termiticides
2007 - IRG/WP 07-20353
One of the biological agents, which cause major damage to wood in Spain, is the subterranean termites. The systems used for controlling termites don’t eradicate them, and the products presently used to treat wood against them, due to their toxicity and their persistence in the environment, could be prohibited in the near future in Europe as consequence of the 98/8/EC Directive (usually called t...
M T Troya, M J Prieto, D Lorenzo, F Rubio


Accelerated Above-ground Testing of Wood Preservatives
2007 - IRG/WP 07-20358
The Canadian wood preservation industry is interested the introduction of new preservative formulations, some of which are intended only for above ground uses. Canada’s Pest Management Regulatory Agency requires data from field tests under Canadian conditions but these can take many years to generate results. Forintek has therefore developed an accelerated above ground test, under contract to a ...
P I Morris, S McFarling


Electrokinetic Accelerated Ingress of Boron After Surface Treatment of Wood
2007 - IRG/WP 07-40372
In this work electrokinetic acceleration of boron penetration after surface treatment is proposed in order to offer an alternative to the often low penetration rates based on diffusion. Electrodialytic experiments showed that boric acid could be transported as negatively charged complexes with tartaric acid in aqueous solutions at pH 4-5. Boric acid could not be transported when tartaric acid was ...
I V Christensen


The effect of wood moisture content and rod dosage on movement of boron through Douglas-fir heartwood
2007 - IRG/WP 07-30431
The potential for moisture sorption by boron rods following application to wood to affect subsequent boron diffusion was investigated in small Douglas-fir blocks conditioned to 30, 60 or 90% moisture content (MC). MCs tended to decline over the 180 day test period, but there was no evidence that the rods acted to draw moisture away from the wood. As expected, boron movement tended to increase with...
Y Cabrera, J J Morrell


Bamboo Protection Research: Contributions from India
2007 - IRG/WP 07-40355
Bamboo preservation has become more important in India because of Government’s directions to develop bamboo resources and adopt their rational utilization to conserve natural forests. This paper traces the development of various processes for treatment of bamboo and their effectiveness. Results obtained by various workers since 1947 when systematic work on bamboo protection was first published. ...
S Kumar


Developments in Borate Treatment of Canadian Species for Decay and Termite Resistance
2007 - IRG/WP 07-30443
The increased interest in boron treatment of wood over the past 20 years is mainly due to its environmental acceptability, potentially deep penetration in wood, and its efficacy against decay and termites. Based on Forintek’s research in the past two decades, the boron penetration and retention requirements for decay and termite protection in various national and international standards for Cana...
Jieying Wang, P Morris, S McFarling, T Byrne


Field Liners as physical barriers to prevent wooden utility pole decay in soil: An accelerated field simulation trial
2008 - IRG/WP 08-20384
Field Liners (FL’s), plastic sleeves used to protect in-ground wooden poles from fungal and termite damage, have been tested before as physical barriers to prevent contact between soil and wood and to retain wood preservative treatment. These earlier studies concentrated mostly on creosote preserved poles and early generation FL’s which were cumbersome in their application. The newer generatio...
A R Howgrave-Graham, L J Cookson, T Hale


Service life prediction of wood: scale-dependent tools within a bio-engineering framework
2008 - IRG/WP 08-20387
Service life prediction (SLP) is a complex yet essential method for the building industry. Accurate and precise assessment of the components is crucial for a strong position of wood on the market. As it is a biological material, wood has an inherent variability and is susceptible to fungal attack. Therefore a profound knowledge of these characteristics is the corner stone of SLP for wood products....
J Van den Bulcke, J Van Acker, M Stevens


Development of a Weatherometer to Accelerate the Surface Checking of Wood
2008 - IRG/WP 08-20388
There is significant interest in developing preservatives that are better at preventing wood from checking. Currently, however, there is no accepted test methodology for accelerating the development of checks in wood samples so information on the effectiveness of treatments at restricting checking can be obtained more quickly. This paper describes the development of a new type of weatherometer (Ac...
R Ratu, P D Evans


Soft Rot Determines Service Life of L-joints with Low Borate Loading
2008 - IRG/WP 08-30470
As part of a research program on the potential use of borates by the Canadian wood products industry, Forintek set up an L-joint test of untreated and borate-diffusion treated hem-fir (western hemlock and amabilis fir) in 1990. The treated material had a low initial retention of only 0.2% boric acid equivalent and analysis after 5 years revealed no detectable borate close to the tenon. Nev...
P I Morris, J Wang, J K Ingram


Penetration Depth of Borates in Historic Wooden Structures in Virginia City Montana
2008 - IRG/WP 08-30475
Virginia City, Montana contains some of the best preserved examples of gold boom construction in the United States. Unfortunately, even the dry climate and fortuitous lack of fire have not prevented decay from claiming parts of the historic fabric. This project aims to determine if borates should be integrated into the preservation plan of the Montana Heritage Commission. Solutions of disodium ...
A A Turner


Accelerated fixation of ACQ-D treated Chinese fir with different post-treatments
2008 - IRG/WP 08-40400
With the enhanced focus on the environmental impact of the preservative-treated wood in recent years, it is necessary to perform some post treatments to prevent contamination of soil and ground water and reduce copper losses from ACQ treated wood in service. In this study, the potential of hot air, hot water, steaming and microwave post treatments to accelerate the fixation of copper in ACQ-D trea...
Lili Yu, Jinzhen Cao, P A Cooper


Measurement of wood decay by dynamic MOE in an accelerated soil contact test
2008 - IRG/WP 08-20390
Current laboratory and field testing of preservatives involves various techniques to determine the extent of fungal attack, including visual inspection, mass loss, and static bending and compression strength measurements. The objective of this study was to compare decay measurement by conventional compression strength versus dynamic MOE, employing small wood stakes in an accelerated laboratory so...
Gan Li, D D Nicholas, T P Schultz


To decay or not to decay: An accelerated field test of the validity of the Scheffer index
2008 - IRG/WP 08-20392
The Scheffer Index was introduced in 1971 to predict the relative decay hazard of untreated wood exposed above-ground. Precipitation and temperature parameters are used in the calculation. A higher Scheffer Index value implies a greater risk of decay. An accelerated 18-month study using seven field sites with Scheffer Indices ranging from 35 to 400 and two wood types (Populus tremuloides and Pi...
G M Larkin, P E Laks


Accelerated weathering of nine tropical wood species from Cameroon
2009 - IRG/WP 09-10705
The natural durability of tropical species for building components has been a subject of recent concern and questioning, mainly the resistance to weathering. Weathering resistance of nine tropical species from Cameroon, namely Azobe, Bilinga, Bubinga, Teak, Dousie, Moabi, Musanga, Sipo and Padauk were evaluated using an accelerated weatherometer for 2016 hours. Measurement of moisture fluctuation,...
S Pankras, Jinzhen Cao, D P Kamdem


Accelerated H3 above-ground decay trials in Australia
2009 - IRG/WP 09-20411
An above-ground H3 fungal field trial was installed at five sites (3 in Australia, 2 in New Zealand), with the aim of finding a method that would shorten the time required for evaluating new preservatives and protection systems. One-quarter of the H3 preservative retentions were mostly installed, as first results suitable for registration occur when these reach 70% soundness. Chemical analysis of ...
L J Cookson, J Carr


Selection of an appropriate coating system for wooden boats to be used in fresh water
2009 - IRG/WP 09-40472
Properties of several, most commonly used protective low-price coatings, which are used by the pletnja boat owners in Bled, Slovenia, were extensively studied. The aim of this professional, practically oriented study was to compare various coating systems, and to recommend the most suitable one to the boat owners. Regarding specific use conditions, the following properties, including their resista...
M Petrič, B Kričej, A Logar, M Pavlič


Photostabilization of Wood with Higher Molecular Weight UV Absorbers
2010 - IRG/WP 10-30524
Higher molecular weight UV absorbers were created by reacting the epoxy-functionalized UV absorber 2-hydroxy-4(2,3-epoxypropoxy)-benzophenone (HEPBP) with maleic, phthalic or succinic anhydride. The ability of the UV absorbers to photostabilize wood was then examined. FTIR-spectroscopy confirmed that HEPBP reacted with phthalic anhydride to create a polyester that preserved the UV-absorbing benzop...
P D Evans, M J Chowdhury


Accelerated L-joint performance testing of organosilicon treated wood
2010 - IRG/WP 10-30551
In this research Scots pine sapwood L-joints were treated with organosilicons and organosilicons in combination with biocides. These L-joints were prepared and exposed according to the accelerated L-joint method. They were inspected each season for fungal discolouration and removed from the rack after three years outdoor exposure. Subsequently the moisture content, mass loss and decaline uptake we...
L De Vetter, J Van Acker


Influence addition of boron compounds to adhesives on the bonding quality and fungicidal properties of glued wood
2010 - IRG/WP 10-40497
Wood is one of the most important construction materials. However, users of wood face two issues: limited dimensions and insufficient durability. These issues have been overcome with the development of bonding and wood preservation. The preservation of glued wood is elucidated in this paper. Through the addition of boric acid to adhesives, we tried to improve the fungicidal properties of glued woo...
M Humar, B Lesar, A Ugovsek, M Kariz, P Kralj, M Šernek


Previous Page | Next Page