Effect of Scytalidium lignicola on decay resistance and strength of wood
1994 - IRG/WP 94-10061
We reported previously that in laboratory tests, pretreatment of Douglas-fir and Southern Pine blocks with Scytalidium lignicola prevented decay. In the present work, we determined 1) the ability of Scytalidium lignicola to colonize and survive in wood exposed in the field, 2) the decay resistance of blocks removed from previously treated Scytalidium lignicola wood and 3) the effect of Scytalidium...
T L Highley


Preliminary results of the treatment of wood with chlorosilanes
1981 - IRG/WP 3172
It is clear from the initial data reported here that the treatment of pine sapwood with chlorosilanes under the reaction conditions employed did not significantly reduce the decay by both white rot and brown rot fungi. Only the dichlorosilane compounds showed to possess some protective action against fungal attack. Before drawing conclusions on the application of organosilicon compounds as potenti...
M Stevens


BRE Experience in monitoring decay in out-of-ground exposure trials
1995 - IRG/WP 95-20077
The outdoor field trial has always been regarded as the ultimate test of performance for assessing the effectiveness of a wood preservative. For this reason, the Building Research Establishment (BRE) has invested much effort in such trials over many years. Emphasis in early trials was on ground contact tests which were the basis both for assessing the likely performance of a preservative in protec...
J K Carey, R J Orsler


Decay resistance of Siberian larch wood against brown rot fungi - Part 2. The effect of genetic variation
1998 - IRG/WP 98-10287
Wood natural decay resistance is mainly restricted in the heartwood part of tree and based on wood microstructure and chemical composition. However, the variation of decay resistant in different wood species is vide and the effect of genotype on decay resistance of Siberian larch wood grown in Finland is not known. The aim of this work was to find out the variation on decay resistance of Siberian ...
H Viitanen, L Paajanen, T Nikkanen, P Velling


Soluble nutrient content in wood and its susceptibility to fungal discoloration and decay in above ground and ground tests
2000 - IRG/WP 00-10336
The objective of this comprehensive study was to reveal the impact of soluble nutrients in wood on its susceptibility to fungal discoloration and decay in various tests, which is important for the test methodology and standardisation. Seven tests were carried out including pure culture above and ground contact tests, above ground field test and laboratory ground contact tests. The samples containi...
O M Caballero, N Terziev


Chemical evaluation of borate treated pine sapwood attacked by the subterranean termite Coptotermes acinaciformis
1993 - IRG/WP 93-20003
Sapwood of hoop (Araucaria cunninghamii Ait. ex D. Don) and slash (Pinus elliottii Englem.) pines were treated by Vacuum Pressure Impregnation (VPI) to provide test specimens. The concentration of boron was defined by chemical analyses of the timber, in the zone of primary attack by the termite being bioassayed. A common method of definition of preservative retention, weight uptake of preservative...
A R Moffat, B C Peters


Low polymer levels containing bioactive monomer polymerized in situ provide resistance to Gloeophyllum trabeum
1995 - IRG/WP 95-30066
Wood preservation based on in situ polymerization of potentially bioactive monomers has been studied. Tributyltin oxide acrylate (TBTOA) and pentachlorophenol acrylate (PCPA) were synthesized. Wood samples were treated at 2, 5, 10, 15 and 20% by weight solutions with varying amounts of crosslinker (trimethylolpropane trimethacrylate, TMPTM) and polymerized in situ in wood samples (2.54 x 2.54 x 0....
R E Ibach, R M Rowell


Evaluation of the pulsed-current resistance meter (Shigometer®) for determination of the internal condition of utility poles
1979 - IRG/WP 2128
A number of Telecom poles, which had been removed from service to be replaced by a radio link, were inspected using an electrical resistance meter (Shigometer®). These poles were creosoted, non-durable Victorian species in service in New South Wales. Six of these poles, chosen to represent various internal conditions typical of the range of the population tested, are discussed here. Data, from tr...
J D Thornton, W G Seaman, M McKiterick


Relative performance of copper/chrome/boron (CCB) and copper/chrome/arsenate (CCA) in ground contact
1992 - IRG/WP 92-3694
The performance of four retentions each of an oxide CCA formulation and a salt formulation of CCB in radiata pine and European beech was compared after 18 years' field exposure. In radiata pine CCA oxide was more effective (4 failures out of 40) than CCB (9 failures out of 40). However, in European beech CCB was substantially more effective (22 failures) than CCA oxide (all failed). Analy...
M E Hedley


The natural durability of wood in different use classes
2003 - IRG/WP 03-10457
The natural durability of important European wood species has been tested on 3970 specimen in field trials. The wood was exposed at five test fields in Germany with different climates at each site in European hazard class 4 and 3 (with and without soil contact). Within EHC 3 it was distinguished between tree different expositions (end grain sheltered, unsheltered and with water trap). The test is...
U Augusta, A O Rapp


L-joint trials: Part 2: The relationship between colonisation by decay fungi and long-term performance
2002 - IRG/WP 02-20251
Many of the L-joint trials conducted at BRE were assessed during the early stages to establish the rate of colonisation by fungi, principally basidiomycetes. At that time, a system of assessment incorporating colonisation studies was proposed for inclusion within the European Standard EN 330 but was rejected for the final version of the standard. The long-term trials associated with the colonisa...
J K Carey


Determination of the water sorption properties and preliminary results from field tests above ground of thermally modified material from industrial scale processes
2004 - IRG/WP 04-40279
In this study the differences in moisture behavior and durability above ground of heat treated wood originating from different European industrial heat treatment plants by means of the water sorption properties as well as field tests were examined. The manufacturers of heat treated material were: PLATO Hout B.V./Netherlands, Thermo Wood (Premium wood)/ Finland and Menz Holz/ Germany, where Oil-...
C R Welzbacher; A O Rapp


Durability of Bamboos in India against termites and fungi and chemical treatments for its enhancement
2005 - IRG/WP 05-10553
Bamboo is a very important forest resource that benefits the life of people in a myriad ways including meeting the need for structural uses like posts, pole fencing, scaffoldings, house building, etc. Although it is one of the strongest structural material available, often succumbs to fungal decay and biodeterioration by insects (termites and powder post beetles) during storage and usage. Studies...
O K Remadevi, R Muthukrishnan, H C Nagaveni, R Sundararaj, G Vijayalakshmi


Termite-tunnels formation on the surface of termite-resistant wood species in field sites
2001 - IRG/WP 01-10400
In this report, termite-tunnels formation by the subterranean termite, Coptotermes formosanus Shiraki on the surface of termite-resistant wood species, namely, Hinoki (Chamaecyparis abtsu), Yoshino Hinoki (Chamaecyparis abtsu), Miyazaki Hinoki (Chamaecyparis abtsu), Hiba (Chamaecyparis abtsu) and Japanese cedar (Cryptomeria japonica) was conducted in field sites. Westernhemlock (Tsuga heterophylla...
Y Kadekaru, K Kinjo, S Yaga


Resistance of painted wood to mould fungi. Part 3. The effect of weathering, wood substrate and fungicides on mould growth
1998 - IRG/WP 98-10284
The effect of 6 month outdoor weathering on the resistance of acrylate paint systems on different types of pine and spruce sapwood to mould fungi was studied. Dipping into the preservative prior to painting, a primer with and without a fungicide (propiconazole + IPBC 0.50 + 0.2%) and a topcoat with and without a fungicide (propiconazole + IPBC 0.25 + 0.12%) were combinations of the treatments stud...
H Viitanen, P Ahola


Japanese standardized methods for testing effectiveness of chemicals against termite attack
1986 - IRG/WP 1290
Japanese standard termiticide testing methods are reviewed. There are some standard testing methods provided by Japan Termite Control Association (JTCA) and Japan Wood Preserving Association (JWPA), though most of them are common to two organizations. Methods were standardized between JTCA and JWPA in 1981, and more recently examining system was established for authorizing efficacy of wood preserv...
K Tsunoda, K Nishimoto


Accelerated laboratory testing of preservatives on 13 North American wood species
1999 - IRG/WP 99-30201
The ability of selected water and solvent based biocides to protect wood against fungal attack was evaluated on 13 North American wood species using 7 decay fungi in a modified soil block test. Most preservatives were capable of providing protection at their recommended above ground and soil contact use levels. Many decay fungi caused substantial weight losses on blocks treated with chlorothalonil...
J J Morrell, C M Freitag


The full guideline for the “double layer test method” - A field test method for determining the durability of wood out of ground
2004 - IRG/WP 04-20290
This guideline describes a test method for wood to be exposed to the weather out of ground contact. The main objective of the method is to evaluate the durability of wood in above ground exposure as shifted overlaid stakes, which form the so called double layer. The method is applicable to the testing of untreated, treated and modified wood. Initially it was developed and found to be most useful ...
A O Rapp, U Augusta


A comparison of the leaching resistance of diammine-copper complexes and copper carbonate precipitated in wood
1997 - IRG/WP 97-30158
Previous studies have shown that during treatment of wood with ammoniacal copper solutions, both simple copper precipitates and diammine-copper complexes are formed. The objective of the present study is to determine the relative importance of both forms of copper, on such aspects as preservative leachability and biological performance. In the current experiment, the leachability of copper carbona...
Xiao Jiang, J N R Ruddick


Curing conditions for a low formaldehyde etherificated melamine resin
1998 - IRG/WP 98-40108
Waterbased methanol etherificated melamine formaldehyde resins have the potential to increase the resistance of impregnated wood against wood destroying fungi. Previous studies indicated that the resin with the lowest formaldehyde content tested showed the best results regarding fungal resistance, dimensional stability and formaldehyde emissions after curing. In the present paper the influence of ...
D Lukowsky, R-D Peek, A O Rapp


Biocidal screening method of wood extractives by a direct use of cellulose TLC plate
2001 - IRG/WP 01-20226
Most of the methods to evaluate the biological durability of woods have focused on decay fungi and termite as deteriorating organisms and it is well known that one of the most important factors affecting the biological characteristics of wood is extractives. Bioassays for evaluating the biological activities of wood extractives have been mainly conducted with treated filter papers for termites or ...
R Yusiasih, T Yoshimura, T Umezawa, Y Imamura


A rapid method for collecting large numbers of subterranean termites from wood
1982 - IRG/WP 1165
A corrugated fiberboard trap is described which attracts large numbers of subterranean termites from infested logs. Single-trap collections in excess of 63 grams (wet wt.) for Reticulitermes virginicus (Banks) and 43 grams for Coptotermes formosanus Shiraki were taken one to three days following discovery by termites. If traps are removed from the source logs shortly after beeing attacked, termite...
J P La Fage, N-Y Su, M Jones, T Lawrence


Establishing standard principles for laboratory bioassays of termiticides with subterranean termites - progress, problems and prospects
1993 - IRG/WP 93-10013
Laboratory bioassays of termiticides, including wood preservatives, aim to give an indication of the likely concentrations effective in preventing damage to timber products and other materials in the field. In laboratory bioassays field conditions should be simulated as closely as possible. With a wide range of procedures in use around the world it may often be difficult to compare results between...
M Lenz, J W Creffield, Zhong Yun-hong, L R Miller


Options for termite management using the insect pathogenic fungus Metarhizium anisopliae
1996 - IRG/WP 96-10142
The insect pathogenic hyphomycete fungus Metarhizium anisopliae (Metschnikoff) Sorokin is promising as a biological insecticide for many species of subterranean termites. In Australia, a survey of termite mounds and feeding sites using a selective medium showed that this fungus is widespread but rarely causes mortality of termites under natural conditions. One isolate, codenamed FI610, has been se...
R J Milner, J A Staples, M Lenz


L-joint trials: Part 3: Relative performance of a range of preservative products
2002 - IRG/WP 02-30292
Long-term trials using the L-joints described in BS EN 330 and AWPA Standard E9-97 have been in progress at BRE since 1982. This paper records the current assessments of decay of L-joints in trials started between 1982 and 1994 with treatments applied to both Scots pine sapwood (Pinus sylvestris) and spruce (Picea sp.). Data are provided on a range of active ingredients including TnBTO, PCP, a...