Determination of toxicity data for preservatives against Basidiomycetes by measuring the reduction in compression strength of wood
1988 - IRG/WP 2297
Blocks of Pinus radiata D. Don were treated to 12 retention levels with CCA and NaPCP. These were exposed for 12 weeks in agar jars to the dry rot (brown rot) Serpula lacrymans (Schum. ex Fr.) S.F. Gray. After mass loss determination, the same blocks were tested for reduction in compression strength parallel to the grain. Using both these parameters, together with interpolated 6 week strength loss...
J Wazny, J D Thornton


Wood protecting chemicals for the 21st century
1993 - IRG/WP 93-30018
After assessing the past research with protection chemicals, this paper proposes future avenues for research and development in wood protection. Three scenarios are put forward for consideration. First, more is not better and future systems will emphasize combination formulations which enhance properties while providing biological efficacy. Second, current systems, especially those based on copper...
H M Barnes


The resistance of timbers to impregnation with wood preservatives
1979 - IRG/WP 3137
It is anatomical structure which determines liquid flow rate within different timber species. This cannot be deduced from properties such as density or rate of growth, and can only be found by experiment. A standard test has been in use at the Princes Risborough Laboratory for many years, employing a pressure-impregnation treatment, and a large number of timbers have been studied. The test consist...
Anonymous


A comparison of analytical and visual techniques used for assessment of weathering properties of chromium and copper azole treated timber
1994 - IRG/WP 94-20023
The weathering properties of preservative treated timber were studied by measuring surface lignin loss and by microscopic examination after weathering, and results were related to qualitative assessments of visual appearance after weathering. Measurement of relative rates of delignification of untreated and preservative treated timber obtained by FTIR analysis, and weight loss determined on thin v...
J A Cornfield, M D C Hale, G Fettis


Effect of aqueous polymer treatments on wood properties. Part 1: Treatability and dimensional stability
1990 - IRG/WP 3610
Partially air-dried sapwood of sweetgum (Liquidambar styraciflua) and southern pine (Pinus spp.) was treated with either aqueous polyacrylate or aqueous dimethyloldihydroxyethyleneurea (DMDHEU) solutions. Tests for dimensional stability were conducted on matched treated and untreated pieces. Measurement of the antishrink efficiency indicated that DMDHEU was a better stabilizer than the polyacrylat...
Z Ashaari, H M Barnes, R C Vasishth, D D Nicholas, D E Lyon


Preliminary pole treatment trials with chlorothalonil in hydrocarbon solvent
1994 - IRG/WP 94-40027
A series of 460-mm long, end-sealed southern pine pole stubs were treated with chlorothalonil in hydrocarbon solvent. Over sixty sections were treated using various combinations of initial seasoning (kiln-drying, steam-conditioning), treating temperature (ambient, 200°F), initial air pressure, and final conditioning (steam flash + vacuum, expansion bath + vacuum, steam distillation + vacuum). Dis...
H M Barnes


International co-operation in wood preservation research
1979 - IRG/WP 3145
If one searched the literature, one could find many examples of international co-operation in the field of research in wood preservation. For example, individual workers in different countries in Europe have got together and made replicate tests with both fungi and insects on various preservatives of common interest and their results have been published. Much co-operation has not had its results p...
R Cockcroft


Non agricultural biocide directive. Practical proposals of implementation in the case where biocides are wood preservatives
1995 - IRG/WP 95-50040-24
This project of non-agricultural biocide directive has currently an extremely wide scope of pre-marketing authorization of substances and preparations used in numerous applications, other than agricultural. Elaborated on the 86/414/EEC model of the phytopharmaceutical product directive, the "NAB" draft directive aims to cover situations as different as plant or wood protection: in the case of plan...
G Ozanne


Life cycle approached environmental information to promote treated timber
2005 - IRG/WP 05-50224-13
This paper exemplifies the possibilities to compare products and product systems with help of life cycle assessment (LCA) as a tool for environmental assessment. IVL Swedish Environmental Research Institute has developed a concept for evaluation of environmental impacts based on normalisation, based on so called environmental quality objectives (EQO). This concept makes it possible to compare a pr...
M Erlandsson


Performance of Copper-Chrome-Arsenic (CCA) and Copper-Chrome-Boric (CCB) treated panels of Bombax ceiba and Paraserianthus falcataria against bio-deterioration at Krishnapatnam harbour, east coast of India
2003 - IRG/WP 03-30310
Results of investigations on the durability of light weight timber species (Specific gravity below 0.4) i.e., Bombax ceiba and Paraserianthus falcataria in treated and untreated condition conducted at Krishnapatnam harbour (Lat 13o28’ to 13o59’ N; Long: 80o10’ to 80o16’E) along the east coast of India are reported in the paper. Exposure trails were conducted with panels (Size: 30 x 3.8 x...
B Tarakanadha, N R Raveendra Prasad, K S Rao


Le pin: Matériau à contact alimentaire [Pine wood as a material for food contact]
1995 - IRG/WP 95-50040-01
Monoterpenes emitted to air from woods of pine (Pinus nigra, Pinus laricio, Pinus pinaster and Pinus sylvestris) were determined on the one hand by static analysis and by other hand by sampling on the Tenax adsorbent, followed by analysis using thermal desorption, both being combined with gas chromatography coupled with mass spectrometric detection. The major monoterpenes were alpha-pinene and 3-c...
A Waymel, M Lamour, G Labat


Permeability measurements on surface layers for detecting wood with abnormally high permeability
1988 - IRG/WP 2298
Wet storage of timber during the warm period of the year may lead to an increased permeability of the wood, an undesirable phenomenon for several wood industries and also for many end-uses. Neither before nor after drying, such wood with "wet storage damage" can be visually distinguished from wood with a normal permeability. A non-destructive method for inspecting the permeability of surface layer...
J B Boutelje, G Hägglund


Permatek IM 30 as a termiticide treatment for veneer-based wood products
2003 - IRG/WP 03-30325
Permatek IM 30 is a termiticide designed for incorporation into wood products during manufacture. Whereas existing approved products in Australia are based predominantly on synthetic pyrethroids carried in solvents, Permatek IM 30 is based on imidacloprid, a neonicotinoid insecticide. The formulation has very low mammalian toxicity, is free of VOCs, and has been successfully tested as a glueline ...
J Doyle, K Webb, W R Rae, A F Siraa, J Malcolm-Black


Comparative study of blue stain resistance of various types of wood stains after artificial and natural weathering
1992 - IRG/WP 92-2411
For the determination of the protective effectiveness of a preservative treatment against blue stain in service, artificial weathering has been proposed as an alternative for the natural weathering period of 6 months in the European standard EN 152. Research on a range of products and on complete finishing systems for external joinery was conducted during 1986-1990. It revealed that the decisions ...
J Van Acker, M Stevens, M Nys


Effect of leaching temperature and water acidity on the loss of metal elements from CCA treated timber in aquatic applications. Part 1: Laboratory scale investigation
1995 - IRG/WP 95-50046
In order to investigate the applicability of current prestandard leaching test methods, a series of experiments has been performed on CCA impregnated wood dealing with the influence of pH, temperature and agitation of the surrounding water. The leaching method used in this first part of the investigation is the European prestandard drafted by CEN/TC38/WG11, a short term dynamic leaching test under...
G M F Van Eetvelde, R J Orsler, G E Holland, M Stevens


Neem leaves, a potential source for protection of hardwood against wood decaying fungus
2005 - IRG/WP 05-30370
Neem leaves are widely recognized for their insecticidal, pesticidal, fungistatic and fungitoxic ability. The present study is to investigate the efficacy of neem leaves extractives against wood destroying microbes, a brown and a white rot. Neem leaves extractives prepared in various solvents such as petroleum ether, acetone, ethanol, methanol and hot water were tested at a concentration levels of...
S Dhyani, S Tripathi, V K Jain


Degradation of resin constituents in various wood species by the white rot fungus Bjerkandera sp. strain BOS55
1999 - IRG/WP 99-10301
In previous studies, the white-rot fungus Bjerkandera sp. strain BOS55 was shown to cause extensive degradation of lipophilic extractives (resin) in Scots pine wood. Further research was carried out in order to investigate the ability of Bjerkandera sp. for reducing resinous constituents in various softwood (Douglas fir, larch and spruce) and hardwood species (birch, beech and poplar). The greates...
J Dorado, T A Van Beek, F W Claassen, R Sierra-Alvarez


Fluoride and chromium concentrations in soil adjacent to remedially treated distribution poles
1996 - IRG/WP 96-50066
Soils adjacent to Rentex treated 'on-line' distribution poles were analysed for total fluoride and chromium content for comparison with background values of these elements. Soil samples 6 cm and 25 cm downslope of selected poles were recovered at 1 week, 1 month, 6 and 12 months after treatment. Background soil samples were taken 50 m from the poles at sampling times. Fourteen po...
D C R Sinclair, G M Smith, A Bruce, H J Staines, P Durrant


Compatibility of deltamethrin with wood adhesives
1993 - IRG/WP 93-30031
This work presents the studies conducted on the compatibility of deltamethrin when mixed with wood adhesive to manufacture plywood in order to protect the wood against wood-borers insects and termites. The following types of adhesive were tested: PVA, Urea-formaldehyde, phenol-formaldehyde and a formulation based on tannin. The experiments were made in the adhesive manufacturers' laborato...
A M F Oliveira


Examination of preservative-treated Pinus sylvestris using electron paramagnetic resonance
1992 - IRG/WP 92-3710
EPR is currently being used to help elucidate the nature and extent of the chemical reactions occurring between wood and copper based timber preservatives. In the work reported here treated Scots pine samples were examined at room temperature and in the frozen state. Plots of the electronic parameters A|| vs. g|| were found to be a useful index of the electronic properties of the various formulati...
A S Hughes, R J Murphy, J F Gibson, A J Cornfield


IRG marine wood preservation questionnaire
1994 - IRG/WP 94-10089
During the IRG meeting at Bali of the working party on marine borers, participants decided to update the status of marine wood preservation around the world. This information will help reveal what areas are the major problems in need of attention, show what practical industry solutions or practices are in use, and give an idea of the research directions that different groups are pursuing. This que...
L J Cookson


Application of oscillating pressure to improve treatability of refractory species
1987 - IRG/WP 3449
Under practical conditions a minimum moisture content of 80% demande by the German quality standard RAL-RG 411 can not be guaranteed throughout the year. Storage of logs with bark prolonges the drying process; a storage without bark must be avoided. A sufficient penetration according the standard can be achieved at least with a moisture content of 60%, optimal conditions may prevail between 100% a...
R-D Peek


The influence of timber species and preservative treatment on spore germination of some wood-destroying Basidiomycetes
1988 - IRG/WP 2300
Basidiospores from six wood decay fungi exhibited varying germination rates on untreated softwood and hardwood blocks. Germination inhibition of all test fungi was recorded on pine sapwood. No preference for a certain timber species by a particular fungus was evident. Whereas almost complete inhibition of germination occurred on wood treated with a quarternary-ammonium based wood preservative, mos...
B M Hegarty, G Buchwald


Algal growth resistance of paints for coating of wood; a laboratory study
1997 - IRG/WP 97-10213
Twelve paints were tested for resistance against algae. In addition, one algicidal compound commercially used for remedial treatments of algal growth on paints was tested for its effectiveness for prevention of algal growth. An agar diffusion bioassay was employed in which paint films on filter paper discs were placed on mineral salt medium and sprayed with an algal suspension containing a mixture...
J Bjurman


Effect of fungal degradation on the chemical composition of acetylated beech wood
2003 - IRG/WP 03-40267
This study investigated the impact of fungal attack on the chemical composition of acetylated wood. Beech wood acetylated to different degrees was exposed to decay by the white-rot fungus Trametes versicolor under solid-state fermentation conditions. Laboratory soil-bed assays were also conducted to study the degradation of acetylated wood by soft rot fungi and other soil-inhabiting microorganisms...