The effect of aqueous leaching on moisture uptake by CCA-treated blocks during soil burial
1987 - IRG/WP 2283
Mass loss, moisture content and nitrogen data from two soil burial experiments with untreated and CCA-treated Scots pine (Pinus sylvestris L.), Sitka spruce (Picea sitchensis Carr) and lime (Tilia vulgaris Hayne) are presented. These show that aqueous leaching of CCA-treated wood prior to burial significantly reduces its subsequent moisture uptake from soil. In the case of lime, a reduction in the...
C A Green, G M Smith, B King


Standard and accelerated testing of boron-additive wood protection systems
2005 - IRG/WP 05-30381
The main objective of this research was to determine the effectiveness of boron-additive protection systems for above ground applications by means of field testing. The two field test procedures used are based on the L-joint test described in the European standard EN 330. For the first set up the boron treated timber was coated in accordance with the standard EN 330 system. The second set up is ba...
A Mohareb, J Van Acker, M Stevens


A comparison of the leaching resistance of copper 2-ethanolamine and copper ethylenediamine treated Scots pine
2000 - IRG/WP 00-30233
The depletion of copper from copper 2-ethanolamine and copper ethylenediamine treated Scots pine blocks was investigated. A greater leaching resistance was found for copper 2-ethanolamine, which retained ca. 86% and ca. 50% copper after water and buffer leaching, respectively. Leached amine treated blocks also contained significant residual amine. This was consistent with other observations linked...
Xiao Jiang, J N R Ruddick


Comments on soft rot attack in timbers treated with CCA preservatives: A document for discussion
1982 - IRG/WP 1167
This paper is not based on any particular results but rather on several observations of soft-rot during many years of studies, and on a review of the existing literature. The short time available has unfortunately not permitted a detailed review of the literature. Data and knowledge of important facts are lacking for several aspects of soft-rot attack and for reactions occurring in the wood as a r...
T Nilsson


A quantitative weathering study of wood surfaces modified by chromium VI and iron III compounds
1989 - IRG/WP 2330
Thin veneers of Pinus radiata were treated with dilute aqueous solutions of chromium VI and iron III compounds and exposed to natural weathering for 35 days. Zero-span tensile strength and weight losses of treated veneers were compared with losses observed in untreated specimens In a study designed to demonstrate the applicability of strength and weight loss measurements to the rapid quantitative ...
P D Evans, K J Schmalzl


Co-operative studies on determining toxic values against wood-destroying basidiomycetes: Progress report to April 1990
1990 - IRG/WP 2357
This document reports progress on the co-operative study between nine laboratories, set up following the proposals contained in Document IPG/WP/2316 (1988). Results have been received from eight laboratories. Toxic values data have been established successfully for the test fungus Coniophora puteana with soil, malt agar and vermiculite methods and with the test fungi Gloeophyllum trabeum and Poria...
J K Carey, A F Bravery


Wood detection by the marine isopod Limnoria.markup
1995 - IRG/WP 95-10134
The search for alternative control methods for Limnoria, should perhaps focus on the most vulnerable stage during the isopod life cycle - during dispersal when adulls leave their tunnels to find new wood. Dispersal is known to be triggered by environmental conditions, although how Limnoria locate fresh wood is unknown. Literature available on Limnoria dispersal, their sensory capabilities during d...
S M Henderson, S M Cragg, A J Pitman


The natural history of teredinid molluscs and other marine wood borers in Papua New Guinea
1975 - IRG/WP 410
The teredinids, commonly known as teredos or shipworms, are bivalve molluscs adapted to boring into wood. They are most closely related to the Family Pholadidae, or piddocks, which bore into mud, stone and coral. The teredinids have a relatively small, hemi-spherically shaped shell, the elongated body extending beyond the posterior end of the shell valves. The soft body, protected by the wood and ...
S M Rayner


The durability of wood polymer composites against fungi and insects
2000 - IRG/WP 00-40161
New materials such as wood polymer composites are used more in France. These materials are obtained by mixing wood and thermoplastics in different ratios. These kind of material must be considered as new materials and some characteristics such as durability must be evaluated for outdoor applications. On the other hand, some recycled fibers from wood waste could be used as raw materials. Some woodp...
G Labat, I Le Bayon, J Gerard, F Amin


Information from the COIPM Wood Group
1988 - IRG/WP 4146
Abstract from the COIPM minutes: Wood in marine environment: Mrs Gambetta stated that the main item discussed by the Group was the collaborative work to test the durability of heat shrinkable polyolephin sheating materials for the protection of wood against marine organisms. The work began last year when wood samples were sent out to the participants. Three samples of Pinus sylvestris wrapped in ...
A Gambetta


The effect of acid rain on CCA treated timber
1990 - IRG/WP 3579
The effect of acid precipitation on the leaching of copper, chromium and arsenic from timber treated with different CCA preservatives was studied in the presence of three types of soil under simulated field conditions. Pine sapwood, embedded in soil, was subjected to simulated rainfall at three different levels of acidity. The CCA preservative formulations tested were:- American Wood Preservers&am...
R J Murphy, D J Dickinson


Evaluation of the protective means of some wood preservatives by means of accelerated tests
1973 - IRG/WP 232
In site conditions of the eastern site in the forest-steppe part of the Krasnovarsk region, the relative effectiveness of a series of wood preservatives was obtained by means of field tests. To obtain a more accurate evaluation of the protective qualities of these accelerated tests were carried out in laboratory conditions. In 9 boxes filled with non-sterile soil taken from the site, 72 samples of...
I A Petrenko


Determination of fungitoxic value of preservatives in laboratory wood-block tests. Part 2: Statistical estimation
1989 - IRG/WP 2327
Laboratory modified agar-block tests were made to determine the fungitoxic value of the wood preservative CCA against the test fungus Serpula lacrymans using statistical methods. With the aid of statistical computer programmes based on the least square method. the regression equation was found for the dependence between sample mass loss and preservative retention both in terms of percentage and fo...
J Wazny, J D Thornton, K J Krajewski


Development and Implementation of a DNA – RFLP Database for Wood Decay and Wood Associated Fungi
2004 - IRG/WP 04-10527
We are developing Restriction Fragment Length Polymorphism (RFLP) and Internal Transcribed Spacer (ITS) sequence databases for wood decay basidiomycetes and other fungi associated with wood. These databases currently house information for 39 fungal species consisting of 9 brown-rot basidiomycetes, 12 white rot basidiomycetes, 1 soft rot, 1 stain fungi, and 16 molds or other ascomycetes or imperfe...
S V Diehl, T C McElroy, M L Prewitt


Metal plate fasteners in trussed rafters treated with preservatives or flame retardants - corrosion risks
1977 - IRG/WP 3104
In designing roof trusses employing metal plate fasteners it is generally assumed that the roof will remain dry in service. Whilst this is generally true, damp conditions do arise under some circumstances, although it is not possible to quantify the extent of the risk. It is only possible, therefore, to give general recommendations which must be interpreted in the light of local experience of serv...
R A Laidlaw, L C Pinion


Wood durability in the light of recent trends and research on the durability of building materials and components
2000 - IRG/WP 00-20195
Building-related research of today demonstrates a clear shift in focus from the design and production phases to usage and to the entire life time. A consequence is that the performance criteria of materials, components and of the entire building must be regarded over the life time rather than at the time of production or delivery. As one example can be mentioned the Building Construction Directive...
K Ödeen


Tool wear for vapor boron-treated composites
2001 - IRG/WP 01-40209
A series of composites, including oriented strandboard and medium density fiberboard, were treated via vapor boron technology. Treated samples were compared to untreated composites using a tool force measuring technique. Tool forces measured with a dynamometer indicated a positive effect of boron addition. Visual and SEM examination indicated a wider wear zone on the rake face of the tool for the ...
W A Jones, H M Barnes, H A Stewart, R J Murphy


Wood preservation requirements in Queensland, Australia
1983 - IRG/WP 3227
In Queensland the preservative treatment and utilization of timber must comply with the Timber Users' Protection Act. Preservative retention levels and penetration patterns must be complied with. Analytical zones are specified for removing samples for chemical analysis of preservative retention. The required retention levels have been expressed as percent weight of oven dry wood weight. T...
L E Leightley, M J Kennedy


Biological resistance of electrolessly plated wood (1). Preliminary report
1994 - IRG/WP 94-40024
Surface metal coating is considered to improve biological resistance of wood as some metal ions are fungitoxic. Six wood species (three softwoods: Cryptomeria japonica, Tsuga heterophylla and Larix spp; three hardwoods: Fagus crenata, Acer mono and Betula platyphylla) were electrolessly plated with nickel or copper, and those were served for laboratory evaluation of their resistance against decay ...
M Hasegawa, K Tsunoda, T Yoshimura


Effect of post-treatment processing on leachability of ACZA-treated douglas-fir lumber
1998 - IRG/WP 98-50109
The effect of post-treatment procedures that more rapidly precipitate copper, zinc, and arsenic in douglas-fir treated with ammoniacal copper zinc arsenate (ACZA) on subsequent leaching resistance were investigated at two retentions (6.4 and 40 kg/m3). Total leaching was greater from boards treated to the higher retention. At both levels, copper was lost at the highest rate. Post-treatment process...
J J Morrell, C S Love, S Kumar, C M Freitag


Biological and chemical investigations for the assessment of the environmental impact of wood preservative components
1999 - IRG/WP 99-50127
This study was carried out in order to investigate the suitability of biological and chemical techniques to evaluate the environmental impact of wood preservatives depleted from impregnated wood. Small specimens (15*25*50 mm3) of Scots pine sapwood (Pinus sylvestris) were treated with a CCB salt. After fixation the treated and untreated samples were washed-out according EN 84, and the different le...
E Melcher, H-W Wegen


Studies and experiences of occurrence and development of soft rot in salt-treated poles of pine (Pinus sylvestris) installed in Swedish transmission lines in the years 1940-1945
1977 - IRG/WP 277
The present work describes the result of microscopic examinations of some 2,000 borings extracted from 20 to 23-year-old salt-treated poles (Scots pine) from the southern and central parts of Sweden. The purpose was to map out the occurrence of soft rot in Sweden and its influence on the mechanical strength of the poles as well as to contribute to the development of new and more satisfactory metho...
H Friis-Hansen


The involvement of extracellular substances for the generation of hydroxyl radical during wood degradation by white-rot fungi
1997 - IRG/WP 97-10218
The activities of one-electron oxidation, hydroxyl radical generation, and phenol oxidase during the incubation of cultures of four white-rot fungi containing either glucose or wood were periodically measured. Further, their degradation activities against wood were examined during the course of cultivation. The generation of hydroxyl radical was correlated to the activity of wood degradation and i...
H Tanaka, S Itakura, A Enoki


Wood preservation in Brazil
1984 - IRG/WP 3321
The report gives statistics on the wood products industries, the forest products exported, the production of treated sleepers, poles, crossarms, fence posts and other wood products in Brazil for the years 1977 to 1981. The total numbers of vacuum/pressure plants, through the years 1902 to 1984, indicate that from 1960 there has been a steady increase in treatment requirements. Most of the plants a...
M S Cavalcante, R Cockcroft


Effects of the specimen position on fungal colonisation and wood decay by en 113 test fungi
1998 - IRG/WP 98-20136
For testing wood preservatives according to EN 113 it is common practice to plant the test blocks on neutral supports in order to prevent (1) a diffusion of chemicals into the agar medium and (2) an excessive moistening of the specimens. The procedure was employed in EN 350-1 for testing the natural durability of solid wood. It turned out to be of problematic nature because of the individual requ...
G Kleist, M-T Lenz, R-D Peek