IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 3393 documents. Displaying 25 entries per page.


Microbial ecology of treated Lap-joints exposed at Hilo, Hawaii for 24 months
1997 - IRG/WP 97-20107
This paper is a continuation of previous work reported in IRG/WP 96-20089 by Molnar et al. (1996) in which Lap-joints, made from Southern yellow pine and treated with ACQ, DDAC or propiconazole were sampled over 12 months exposure at Hilo, Hawaii. 18 and 24 month samplings have since taken place and are reported here. TnBTO treated Lap-joints made of scots pine which were exposed later as a standa...
S Molnar, D J Dickinson, R J Murphy


Selecting fumigants for treatment of internal decay in wood
1986 - IRG/WP 3370
A number of potential fumigants were screened with respect to their toxicity to decay fungi, (Poria carbonica, and Lentinus lepideus) and their sorption characteristics on Douglas Fir (Pseudotsuga menziesii Mirb. Franco) wood. Wafers of infected wood were exposed to different fumigant concentrations for various times then cultured to determine viability. The lethal concentration X time (ct) factor...
P A Cooper


Moisture Adsorption Behaviour of Rubber Wood Decayed by Brown and White rot Fungi
2005 - IRG/WP 05-40306
Moisture adsorption behaviour of rubber wood blocks decayed by each brown rot and white rot fungi was studied. The adsorption isotherms of decayed wood were compared with the isotherm of undecayed wood. The wood decayed by brown rot adsorbed less moisture as compared to sound or undecayed wood at all humidity levels. No significant difference was observed in adsorption behaviour of white rot dec...
S S Chauhan, H C Nagaveni


Collaborative soft rot tests: Specific gravity loss resulting from soft rot
1973 - IRG/WP 227
It was proposed at the 5th meeting of Working Group II of the IRG in June 1973 in Lahti, Finland, that the specific gravity (swollen volume basis) of test blocks used in the IRG Collaborative Soft Rot Tests should be determined on all the blocks at the completion of the exposure period. Specific gravity determined on the basis of the oven dry weight and water swollen volume was selected because (1...
C R Levy


The use of organic wood preservatives in ground contact and the suitability of laboratory test procedures to determine their efficacy
1999 - IRG/WP 99-20175
Organic fungicides, such as propiconazole, have proven to be highly effective when used as a co-biocide in recently developed wood preservative formulations. They have however been ineffective when used as a stand alone preservative, particularly when used in ground contact (European Hazard class 4). Previous research, using the test methods of ENV 807 (1993), provided conflicting evidence regardi...
I J Herring, D J Dickinson


Characterization of wood decay enzymes by MALDI-MS for post-translational modification and gene identification
2002 - IRG/WP 02-10442
The recent sequencing of the Phanerochaete chrysosporium genome presents many opportunities, including the possibility of rapidly correlating specific wood decay proteins of the fungus with the corresponding gene sequences. Here we compare mass fragments of trypsin digests, determined by MALDI-MS (Matrix Assisted Laser Desorption Ionization-Mass Spectrometry), with predicted mass fragments derive...
T H de Koker, P J Kersten


Electrodialytic remediation of a soil from a wood preservation industry polluted by CCA
1998 - IRG/WP 98-50101-14
Soil contamination is often found at wood preservation sites due to spills, dripping of excess preservatives and deposition of sludge associated with dissolved salts of copper, chromium and arsenic (CCA). The electrodialytic process is a promising heavy metal soil remediation technique. It is based on a combination of the electrokinetic movement of ions in soil with the principle of electrodialysi...
A B Ribeiro, A Villumsen, G Bech-Nielsen, A Réfega, J Vieira e Silva


The effects of pH on leaching of copper-chrome-arsenate (CCA) from pressure-treated Kenyan-grown Eucalyptus saligna and Acacia mearnsii: Initial findings.
2002 - IRG/WP 02-30298
The effects of pH on leaching of CCA from pressure-treated Kenyan-grown Eucalyptus saligna and Acacia mearnsii were tested under laboratory conditions. Small samples of the two species (100mm x 30mm x 40mm) were smooth sawn from 8-year old trees to represent equal amounts of both sapwood and heartwood, air-dried to 12% moisture content, end-sealed, and pressure-treated at a commercial treatment p...
R Venkatasamy


Co-operative tests concerning the influence of solvent and drying method on the toxic limit of wood preservatives against Coniophora cerebella
1972 - IRG/WP 216
In the working group II of the IRG it was agreed that more knowledge was necessary concerning the influence of the solvent on the toxic limit of organic solvent types of wood preservatives against Basidiomycetes. A test program was drawn up and after discussion in the mentioned working group the final program was accepted by the co-operating institutes in 1969. In the test program two fungicides, ...
T Hof


Effect of humidity and temperature on fastener withdrawal resistance from CCA and ACZA treated Douglas-fir
2000 - IRG/WP 00-20209
The effects of preservative treatment on fastener withdrawal was investigated in Douglas-fir lumber conditioned to two moisture regimes. In general, conditioning samples to 19% moisture content produced more substantial changes in withdrawal resistance of galvanized fasteners than did conditioning to 12%. Treatment had little or no effect on withdrawal resistance of stainless steel fasteners. With...
Sung-Mo Kang, J J Morrell


The effect of kerfing on check formation in treated white spruce (Picea glauca) poles
1981 - IRG/WP 3167
62 white spruce poles, 6 m in length, were cut from full size utility poles commercially pressure treated with preservative. 21 of the poles were treated with pentachlorophenol, while of the remainder, all of which were treated with ammoniacal copper arsenate, 22 were kerfed and 19 were unkerfed. The poles were installed in the Westham Island field test site, near Vancouver, and inspected annually...
J N R Ruddick


Water transfer in wood in relation to fungal attack in building - Effect of condensation and diffusion
1992 - IRG/WP 92-1543
Wood is continuously exchanging moisture with the surrounding atmosphere, the temperature and relative humidity are important factors. Wood moisture in this case is not enough to provoque decay by fungi. However, when, during the night, condensation appears cyclically, wood absorbs water and moisture content may be sufficiently high to allow development if drying does not take place. The water tra...
D Dirol, J-M Vergnaud


Potential use of an emulsified tar oil fraction as a wood preservative: Preliminary technological and environmental assessment
1994 - IRG/WP 94-50028
In order to meet the recent environmental concern specifications of creosote are altered, the B[a]P content is limited and restrictions on the emission of volatile organic compounds (VOC) and higher polyaromatic hydrocarbons (PAH) are expected in some countries. Research has been conducted on an emulsion of a selected tar oil fraction. Using a waterborne formulation opens new perspectives for targ...
G M F Van Eetvelde, R Leegwater, M Stevens


Bethoguard; A new wood protecting fungicide for use in metal free ground contact wood preservatives
2002 - IRG/WP 02-30301
Research has identified the limitations in both the spectrum of activity and permanence of organic biocides placed in wood in high hazard environments, particularly in the absence of heavy metals such as copper. More specifically, the control of soft rot decay in wood in soil contact has proven to be most problematic. The new organic biocide, Bethoguard; an oxathiazine, has demonstrated excellen...
S C Forster, G R Williams, M Van Der Flaas, M Bacon, J Gors


Aggressiveness of Reticulitermes species in laboratory test
1993 - IRG/WP 93-10026
In European Standards concerned with the preventive action of wood preservatives against termites, i.e. EN 117, EN 118 the obligatory test species is Reticulitermes santonensis. It is argued that this species is more aggressive than the second European Reticulitermtes species, Reticulitermes lucifugus. Since Reticulitermes santonensis is confined to certain smaller areas in France and thus not rea...
H Hertel, S Pantos, D Rudolph


Soft rot - Soil burial - Tests. Influence of the addition of nitrogen compounds to the soil on wood decay by soft rot
1972 - IRG/WP 213
The decay of wood specimens buried in soil is influenced by various factors. Decisive are the water content, the content of organic substances, the pH-value, the content of mineral nutritive salts, nitrogen content, etc. of the soil. These tests were carried out in order to investigate if the decay of wood in the soil will be influenced by additions of various nitrogen-compounds in different conce...
O Wälchli


Antagonism of Gliocladium virens against wood decay fungi
1995 - IRG/WP 95-10102
Antagonistic abilities of a commercial biofungicide, Gliocladium virens (GL-21, Grace) were evaluated against three white-rot fungi, Trametes versicolor, Phlebia brevispora, Irpex lacteus, and three brown-rot fungi, Postia placenta, Neolentinus lepideus, Gloeophyllum trabeum. In dual culture of Gliocladium virens and wood decay fungi, Gliocladium virens rapidly overgrow the decay fungi and killed ...
T L Highley, L Ferge


Diagnostics methods and routes proposalsto define selective sorting of demolition wood wastes
2001 - IRG/WP 01-50177
Wood wastes are more and more often used in different wood waste valorisation industries (panels, wood energy, cement factories, ...). These industries are in progress to include in their processes, wood wastes coming from demolition wood. A state of the art and an analysis have been made to propose : (1) diagnostics methods to carry out a classification of wood wastes on demolition sites and in t...
G Labat, E Bucket, C Fréret, G Deroubaix


Changes of copper and chromium content after leaching in wood impregnated with the CCB and CB preservatives
2000 - IRG/WP 00-50147
The objective of the study was impregnated with CCB and CB preservatives pine wood of moisture content varying from 12% to 55% subjected to leaching. Losses of copper and chromium were determined for individual layers of wood up to 3 cm from the girth. The results were compared to the total amount of metals determined in water extracts. The degree of leaching of metal ions from wood of 55% moistur...
B Mazela


Wood preservation in Croatia
2004 - IRG/WP 04-30360
Croatia, as all the other countries in transition, however also because of its specific and well-known reasons, is on a path to gradual drawing nearer to the European standards. Only the scientists working at the Faculty of Forestry in Zagreb are engaged in scientific work relating to wood preservation. The construction and wood industry, which should enhance the chemical industry, also have subs...
R Despot, M Hasan


Characterization and differentiation of wood rotting fungi by protein and enzyme patterns
1999 - IRG/WP 99-20177
Standardized tests for wood preservatives are performed with defined fungal strains to ensure comparability between laboratories. However, changes of virulence and variation of results are well known events. Suitable and reliable measures to control the stability of the test organisms are necessary.Comparison of protein patterns produced by SDS-electrophoresis was already described by several auth...
U Schoknecht


Wood preservation in Canada - Regulation and Registration
2001 - IRG/WP 01-50166-02
The Canadian wood preservation industry is at a critical juncture now as a number of initiatives converge on the industry over the next few years. Issues facing the industry include: Re-evaluation of the conventional wood preservative chemicals - inorganic arsenicals, creosote and pentachlorophenol targeted for July 2001. Delayed registration of new actives as a result of re-evaluation activity an...
P A Cooper


A determination of the toxic level of ACQ2100 wood preservative for the powder post borer Lyctus brunneus (Stephens)
1994 - IRG/WP 94-20029
The sapwood of two Lyctus susceptible Australian hardwoods, messmate (Eucalyptus obliqua L'Herit.) and black bean (Castanospermum australe A. Cunn. et Fraser ex Hook) were pressure impregnated with ACQ2100, a wood preservative, to produce replicates of a range of retentions. Preservative retentions were determined by solution weight uptake at treatment and chemical analyses of selected sa...
A R Moffat


Exclusion of anions from the wood cell wall
1991 - IRG/WP 3661
Anionic components of wood preservatives and fire retardants such, as arsenates and phosphates, equilibrate at much lower concentrations in the cell wall bound water than in the free solution in the cell lumens. A degree of anion exclusion is expected in wood, due to the Donnan membrane effect. Fixed anions in the wood cell wall, produced by pH-dependent dissociation of the weak acid groups in woo...
P A Cooper


Analysis of the boron content of preservative treated oak and pitch pine heartwood before and after leaching
1992 - IRG/WP 92-3697
Studies to determine the effects, if any, of a variety of boron formulations on heartwood of English oak and American Pitch pine have been previously reported (King et al (1991)). Small wood blocks were treated, at 10°C or 45°C, with borax, polybor or Boracol 20 for periods of 1 month or 4 months then analysed or continuously leached with tap water for a period of 1 month. Reported results showe...
S McCutcheon, G M Smith, J W Palfreyman, B King


Previous Page | Next Page