The high decay resistance in the sapwood of the naturally durable Malaysian hardwood Belian (Eusideroxylon zwageri)
2001 - IRG/WP 01-10410
It has long been assumed that the observed natural durability of the heartwood in certain timbers is perhaps associated with a relatively lower decay susceptibility also of the sapwood of these species. While the heartwood of Belian is reputedly highly decay resistant among the tropical hardwoods of Southeast Asia, laboratory decay tests reported in this paper have also confirmed the high decay re...
A A H Wong, A P Singh


Ponding of radiata pine (Pinus radiata) - 2. The effect of ponding on coating penetration into wood
1998 - IRG/WP 98-10249
Radiata pine (Pinus radiata) wood panels which had been ponded for periods ranging from 2 to 12 weeks, dried and subsequently coated with a primer and examined by light microscopy after staining sections with Sudan IV to enhance the contrast of the primer material. A correlation between the extent of ponding and the extent of coating penetration into wood was observed. The coating penetration var...
A P Singh, S S Gallagher, U Schmitt, B S Dawson, Yoon Soo Kim


A comparison between high and conventional incision densities for improving preservative treatment of Douglas-fir heartwood lumber
1993 - IRG/WP 93-40009
Incising is required for the preservative treatment of most wood species from the western United States; however, there is considerable debate about the density of incisions required to achieve adequate treatment. Previous studies have shown that the incision effect on treatment is relatively narrow, suggesting that incision densities should be significantly increased over current practices and st...
S T Lebow, J J Morrell


Intraspecific variability of durability of Wapa courbaril (Eperua grandiflora) against Antrodia sp. and Coriolus versicolor: effect of radial and height position in the stem
2004 - IRG/WP 04-10531
The variation of a lesser-used species, Eperua grandiflora attacked by brown and white rot has been examined. Trees of this specie showed differences in their behaviour against the type of rot used and also showed evidence of intra and inter tree variation. The “tree” effect is very significant concerning natural resistance. In the same way, there is variation of durability observed according ...
N Amusant, J Beauchêne, M Fournier


Sawn timber of fir (Abies alba Mill.) - Treatability and usability for the Hazard Classes 3 and 4
1999 - IRG/WP 99-40147
Within a national research project, tests on the treatability on sawn timber of fir (Abies alba Mill.) in oscillation pressure, vacuum pressure and double-vacuum processes have been worked out with 95 trunks taken from 3 different altitude levels (up to a height of 590 metres, 600 to 990 metres and over 1000 metres) and from 4 different regions of Switzerland. As the treatability of round wood can...
E Graf, T Bör


The Effect on Biological and Moisture Resistance of Epichlorohydrin Chemically Modified Wood
2002 - IRG/WP 02-40224
Southern pine solid wood and fiber were chemically modified with epichlorohydrin to help in understanding the role of moisture in the mechanism of biological effectiveness of chemically modified wood. The solid wood had weight gains from 11% to 34%, while the fiber had weight gains from 9% to 75%. After modification, part of the specimens were water leached for 2 weeks or extracted for 2 hours ...
R E Ibach, B-G Lee


Microwave digestion of preserved wood for the determination of Cu, Cr, As, B and P in quality control
1991 - IRG/WP 2364
A microwave digestion method for the determination of copper, chromium, arsenic, boron and phosphorus in preserved woods is described. Samples were digested with nitric acid in pressure-relief type teflon PFA vessels by microwave heating in a commercial laboratory microwave oven. Fast, efficient and complete digestion was achieved within 29 min for 12 samples. The digestion time compared favourabl...
N Bernth, L B Sheard


Bacterial degradation of Pinus radiata compression wood
1996 - IRG/WP 96-10153
An inspection of twelve year old, CCA-treated Pinus radiata wood from an industrial cooling tower showed extensive surface decay of wood. Electron microscopic examination of decaying compression wood indicated that compression wood cells were attacked exclusively by bacteria, which were of erosion and tunnelling types. As compared to the normal wood, compression wood appeared to be more resistance...
A P Singh, R N Wakeling


Effect of humidity fluctuations on mould growth on pine wood
1989 - IRG/WP 1412
Most studies on mould development on wood material have been made at constant moisture conditions during the experimental period. As a consequence of such studies, a maximum permittable humidity level to avoid mould problems in wood constructions has been recommended. In the practical situation, the constructions are seldom subject to constant humidity or temperature. In the present paper, we repo...
J Bjurman


International collaborative laboratory comparison of two wood preservatives against subterranean termites: Second update
1995 - IRG/WP 95-10117
As was agreed by members at the termite workshop at the 24th annual meeting of IRG in Orlando, USA, in May 1993 to initiate an international subterranean termite laboratory bioassay to compare the various preferred termite protocols used by IRG termitologists was initiated. The author was nominated to co-ordinate this comparative laboratory evaluation of two wood preservatives (CCA and Cu-naphthen...
J R J French


Window test. Direct testing of wood resistance to decay: A study of its fitness, its reliability and its accelerating factor
1984 - IRG/WP 2219
This is the results of an experiment using the window-test specimens, exposing the specimens to three different types of testing procedure: 1. Natural infestation in the open air; 2. Artificial infestation and exposure in the open air; 3. Artificial infestation in a green-house. The results show good similiraties of the three parallel tests in term of decay, and assess the reliability of the windo...
G R Y Déon, L N Trong


Effects of heat treatment on modulus of elasticity of beech wood
2002 - IRG/WP 02-40222
Heat treatment is the oldest, simplest and cheapest method for reducing hygroscopicity of wood. The heat treatment protects wood against to biological organisms as well as giving wood dimensional stabilization without damaging environment. The effects of heat treatment on modulus of elasticity (MOE) of beech wood (Fagus orientalis Lipsky) naturally grown and intensively used in forest products in...
S Yildiz, G Çolakoglu, Ü C Yildiz, E D Gezer, A Temiz


Nasutitermes exitiosus and wood-rotting fungi in Eucalyptus regnans, E. acmenioides, E. wandoo, and E. marginata: force-feeding, laboratory study
1985 - IRG/WP 1231
Under a force-feeding regime, the termitid Nasutitermes exitiosus was fed on four eucalypt timbers infested with several fungal species to investigate the influence of such fungus-infested timbers on mass of wood lost, termite biomass, fat content and water content. The results showed that wood mass losses were markedly affected by species of fungi and timber. The interaction of fungi and timbers ...
D B A Ruyooka


Improved preservative penetration of spruce after pre-treatment with selected fungi. II. Creosote treatment, analysis and strength testing
1998 - IRG/WP 98-40106
This paper describes the creosote treatment and analysis of logs pre-treated with selected fungal agents as a method of increasing the porosity of the wood prior to preservative treatment. The paper also reports the subsequent strength testing of the timber to evaluate the effects of the fungal pre-treatment on the structural integrity of the wood. European spruce logs were pre-treated with eithe...
E J Tucker, A Bruce, H J Staines, B Rosner, K Messner


Wood decay of Pinus sylvestris L. and Fagus sylvatica L. by marine fungi. Part 2
1991 - IRG/WP 1471
The water-logged wood conservation requires a good knowledge of the wood decay organims which produce the degradation. Previous conducted studies (ESCORIAL, TROYA, GARCIA DE LOS RIOS, 1990) have shown that the incubation times normally used for in vitro laboratory tests are not sufficients for a significant wood degradation. This has been the reason why the aim of this work was the study of such d...
M T De Troya, A M Navarrete, M C Escorial


Organic nitrogen in wood: Growth substrates for a sapstain fungus
1993 - IRG/WP 93-10019
The nitrogen content of mature wood from lodgepole pine was 0.046% as determined by micro-Kjeldahl. Low molecular weight proteins between 14 and 21 kDa were identified in mature wood, branch wood and sap pressed from wood chips. Amino acids were quantified in acid-hydrolyzed wood samples and accounted for between 19 and 35% of the nitrogen in wood. The sapstaining ascomycete Ophiostoma piceae stra...
L D Abraham, C Breuil


Evaluation of copperised Cashew nut shell liquid and Neem oil as wood preservatives
2005 - IRG/WP 05-30368
An effort has been made to develop eco-friendly wood preservatives using naturally available plant by-products with less toxicity. Copper was incorporated into Cashew nut shell liquid (CNSL) and Neem seed oil. Rubber wood samples were treated with these solutions employing dipping and pressure techniques in 3 different levels. These samples have been evaluated to find out the effectiveness as wood...
D Venmalar, H C Nagaveni


Biological control of wood decay
1992 - IRG/WP 92-1531
This paper provides a general discussion of the principles underlying the concept of using biological control agents for the protection of wooden materials from decay. The rationale for the current upsurge in interest in biological control is discussed and a critical appraisal of the technology compared with the use of chemical wood preservatives is included. The advantages and limitations associa...
A Bruce


Mechanistic aspects of the reactions of copper complexes with lignin in the presence of hydrogen peroxide and lipid hydroperoxide model compounds as proposed for white rot fungi
2001 - IRG/WP 01-10399
The structural principles and the oxidative reactions of the catalytic system consisting of copper, hydroperoxides, and copper coordination compounds that contain aromatic nitrogen atoms are similar to those of catalytic centers of oxidative enzymes involved in delignification reactions of white rot fungi. The system is capable of selectively degrading lignin and its low molecular weight would all...
K Fackler, P Lamaipis, E Srebotnik, M Humar, C Tavzes, F Pohleven, M Sentjurc, T Watanabe, K Messner


Improved preservative penetration of spruce after pre-treatment with selected fungi. I. Fungal pre-treatment of pole sections
1998 - IRG/WP 98-40117
European spruce logs were pre-treated with either Phanaerochete chrysosporium, Dichomitus squalens, Trichoderma viride and Trichoderma aureoviride for incubation periods of between 1-4 weeks prior to pressure treatment with creosote in a commercial treatment plant and analysed for strength and creosote uptake (see part II Tucker et al.). A method to pre-treat logs was optimised. The pole sections ...
B Rosner, K Messner, E J B Tucker, A Bruce


Investigation of extracellular mucilaginous material in some wood decay fungi
1996 - IRG/WP 96-10188
The external morphology of the extracellular mucilagenous material (ECM) produced by Coriolus versicolor and Coniophora puteana during colonization of Scots pine and beech was studies using SEM. Specimens were examined in the frozen hydrated, freeze-dried and critical point dried state. All technics produced artefacts but the ECM was best preserved when examined the frozen hydated state. Critical ...
A R Abu, D J Dickinson, R J Murphy


The suitability of isothiazolone microemulsions as long term wood preservatives
1997 - IRG/WP 97-30150
Microemulsion formulations of 4,5 dichloro-2-n-octyl-4-isothiazolin-3-one were investigated to determine the leaching potential of these formulation types as well as their efficacy against decay fungi. These patented low leaching formulations exhibited good anti fungal efficacy in standard tests combined with minimal leaching of the active ingredient from the wood. The data suggests that the excel...
B M Hegarty, Bing Yu, L E Leightley


Evaluation of the insecticidal efficacy of deltamethrin and the fungicidal efficacy of its association with TCMTB + MBT in the field of wood preservation
1986 - IRG/WP 1289 E
Deltamethrin possesses many advantages for the insecticidal protection of wood: relatively low toxicity, very reduced evaporation, very prolonged retention in the wood, very slight leaching after having penetrated the wood, and absence of odour. Its association with other active agents or solvents is being studied with regard to chemical compatibility. Compatibility studies have proved positive fo...
J S Duguet


Estimates of wood-consumption rates by termites
1983 - IRG/WP 1201
Effects of 2 components; termite-biomass and experiment duration on estimates of wood-consumption rates (mg wood/g termite/day), were examined. Three models; (1) no mortality, (2) linear mortality and (3) nonlinear mortality were used to calculate mean standing-crop biomass of termites. Model (1) predicted a significantly lower wood-consumption rate than those based on models (2) and (3). No signi...
N-Y Su, J P La Fage


Serial techniques for producing fire-retardant wood products
1997 - IRG/WP 97-30127
A series of techniques including fire-retarders denoted by WFR-1, WFR-2. WFR and their applications in producing fire-retardant wood (WFR wood), fire-retardant plywood (WFR plywood), fire-retardant particleboard (WFR particleboard) and fire-retardant MDF (WFR MDF) were investigated The fire retarders were low toxic, decay resistant and less leachable. The treated wood and WFR panels were of excell...
Zhu Jia Qi, Liu Yan Ji, Gao Chao Ying