Effects of Murgul Copper Process flue gases (SO2) on compression strength parallel to the grain of Beech (Fagus orientalis Lipsky.) wood
2008 - IRG/WP 08-40404
In this study was investigated the effect on the compression strength parallel to the grain as mechanical properties of Fagus orientalis Lipsky. wood exposed to SO2 gas and non-exposed. In the experiments the two of four (total) were obtained from Artvin-Ortaköy region and the other two from Artvin-Murgul region. The compression strength parallel to the grain was calculated at the compare of ...
N Ay, E Topaloglu, A Uncu


Effect of CCA and Tanalith E on the performance of surface finishing
2008 - IRG/WP 08-40405
Effect of CCA and Tanalith E treatment on the performance of surface finishing properties was the objectives of this study. Sapwood of scots pine, (Pinus sylvestris L.) and oriental beech (Fagus orientalis Lipsk.) specimens (300 x 100 x 15 mm along the grain) were impregnated with aqueous solution of CCA 2% and Tanalith E 2%. Surface roughness, dry film thickness, adhesion strength, gloss measur...
T Ozdemir, A Temiz, I Aydin


The effect of treatments in boron steaming medium on boron leaching and strength properties of wood
2008 - IRG/WP 08-40409
The combined effect of boric acid impregnation together with boron steaming and steaming heat treatments were evaluated in this study. Boric acid pre-treated wood samples and untreated ones subjected to steaming heat and direct steaming treatment in a close reactor at 13 bar pressure and 180 ºC for 30 minutes. Compression strength parallel to grain of wood samples, leaching test and pH measuremen...
E D Tomak, Ü C Yildiz, S Yildiz, E Pesman


Measurement of wood decay by dynamic MOE in an accelerated soil contact test
2008 - IRG/WP 08-20390
Current laboratory and field testing of preservatives involves various techniques to determine the extent of fungal attack, including visual inspection, mass loss, and static bending and compression strength measurements. The objective of this study was to compare decay measurement by conventional compression strength versus dynamic MOE, employing small wood stakes in an accelerated laboratory so...
Gan Li, D D Nicholas, T P Schultz


Laboratory and field exposures of FRT plywood: Part 1. Physical test data
2008 - IRG/WP 08-40426
Our understanding of the laboratory induced degradation with fire retardant systems is currently limited since we are unable to correlate laboratory steady-state experiments with actual in-service field degradation. Current model studies have generally been limited to isothermal rate studies with selected model FR chemicals. Other factors also play a major role in the degradation of FR-treated woo...
H M Barnes, J E Winandy, C R McIntyre


Effect of a biological treatment on below ground decay of Douglas-fir pole sections
2008 - IRG/WP 08-40433
The use of exogenous sugars to accelerate microbial growth and eventually limit available oxygen in soil surrounding wood in soil contact was investigated on untreated Douglas-fir poles exposed over a 3 year period in Western Oregon. Isolation frequencies differed markedly between treated and untreated poles and the treatment did appear to shift the frequency of some basidiomycetes. The treatment ...
C Freitag and J J Morrell


Categorization of 300 timber, bamboo and cane grown in Bangladesh based on their families, origins, growths, physical and mechanical properties
2009 - IRG/WP 09-10684
In this study the 300 timber, bamboo and cane plants grown in Bangladesh have been classified into various categories based on their taxonomic families, origin of species, rate of growth, color of wood, texture of wood, shrinkage of wood, equilibrium moisture content (EMC) of wood, flammability of wood, cutting and sawing properties of timber, finishing and polishing qualities of wood, machining p...
A K Lahiry


Mechanical and chemical properties of blue stained wood
2009 - IRG/WP 09-10686
Discoloration of wood is frequently caused by blue-staining fungi. In the previous researches there was general opinion that blue-stain fungi do not influence mechanical properties. On the other hand, there were some opposite results reported as well. In order to elucidate this issue, specimens made of Pinus sylvestris sapwood were exposed to two the most frequent and important blue stain fungi Au...
M Humar, V Vek, B Bučar


Impact of decay and blue stain causing fungi on the structural integrity of wood
2009 - IRG/WP 09-10699
The potential influence of diverse decay patterns caused by different brown rot provoking basidiomycetes on the structural integrity of wood was investigated. Additionally the potential impact of blue stain on the structural integrity was examined. Therefore decayed Norway spruce (Picea abies Karst.) specimens representing a wide range of mass loss, caused by four different brown-rot fungi and one...
C Brischke, C Welzbacher, T Huckfeldt, F Schuh


Degradation of wood veneers by Fenton’s reagents: effects of low molecular weight phenolic compounds on hydrogen peroxide decay and tensile strength loss
2009 - IRG/WP 09-20400
Pine wood (Pinus sylvestris) veneers strips were incubated in acetate buffer containing hydrogen peroxide and iron to mimic mechanisms of brown rot decay and assess the degradation of cellulose through analysis of the tensile properties of the decayed wood. The tensile properties of thin wood strips treated with Fenton system reagents or precursors were determined and correlated to weight loss as ...
Yanjun Xie, R Well, Zefang Xiao, B Goodell, J Jellison, H Militz, C Mai


Effects of concentration and temperature of CCA and CCB on wood strength of Turkish fir (Abies bornmulleriana Mattf.)
2009 - IRG/WP 09-40450
The purpose of this study was to present evidence for the effects of concentration and temperature of solutions of water-borne preservatives (chromated copper arsenate, CCA and chromated copper boron, CCB) on the static bending properties (modulus of elasticity, MOE and modulus of rupture, MOR) of Turkish fir (Abies bornmulleriana Mattf.). Wood samples were mechanically tested after a mild full ce...
I Usta, M Hale


Wettability and bonding strength of wood thermally-treated with different combinations of soy oil and chemical additives
2009 - IRG/WP 09-40454
Thermal treatment is a method which has gained wider acceptability as an alternative to the chemical treatment in wood preservation. In order to maximize the benefits of this technique several options have been adopted including the use of soy oil in transferring the heat to the wood. Available information on thermal treatment in general and the oil method in particular show that there are still n...
L Awoyemi, P A Cooper, T Ung


Control of Reticulitermes grassei as a pest in Spain: Termite distribution in an urban area
2010 - IRG/WP 10-10719
The European subterranean termite Reticulitermes grassei Clément, 1978, has been an important pest in Palenciana, a locality in the southern province of Cordoba (Spain) for a long time. The different stages of the pest elimination process have been studied and are presented here. Firstly, a through inspection of all town dwellings was conducted in order to determine a theoretical affected area of...
E Alcaide, R Molero, J Diz, M Gaju


The Use of Micro-Tensile Testing to Assess Weathering Decay and Oxidative Degradation of Wooden Items
2010 - IRG/WP 10-20433
This paper presents a method to study the weathering performance of wooden items and to assess the oxidative degradation of wood via the Fenton reaction. Weathering resistance and photo-stability of wood was tested using pine wood (Pinus sylvestris) veneer strips measuring approximately 60 µm in thickness. The veneer strips were treated using a reactive chemical to impart surface protection. The ...
C Mai, Yanjun Xie, Zefang Xiao, P D Evans, H Militz


Photostabilization of Wood with Higher Molecular Weight UV Absorbers
2010 - IRG/WP 10-30524
Higher molecular weight UV absorbers were created by reacting the epoxy-functionalized UV absorber 2-hydroxy-4(2,3-epoxypropoxy)-benzophenone (HEPBP) with maleic, phthalic or succinic anhydride. The ability of the UV absorbers to photostabilize wood was then examined. FTIR-spectroscopy confirmed that HEPBP reacted with phthalic anhydride to create a polyester that preserved the UV-absorbing benzop...
P D Evans, M J Chowdhury


Evaluation of ACQ-D treated Chinese fir and Mongolian Scots pine with different post-treatments after 20 months of exposure
2010 - IRG/WP 10-30530
The performance of alkaline copper quat-type D (ACQ-D) treated Chinese fir (Cunninghamia lanceolata Hook.) and Mongolian Scots pine (Pinus sylvestris Linn. var. mongolica Litv.) stakes after 20 months exposure in Chengdu and Guangzhou of southern China were evaluated according to AWPA standard E07-07. The ACQ-D treatments used two concentration levels (0.5 and 1.0%) and four different post-treatme...
Lili Yu, Jinzhen Cao, Wei Gao, Haitao Su


Hydrothermal modification for upgrading the durability properties of soft deciduous wood
2010 - IRG/WP 10-40494
To extend the application potentialities of soft deciduous wood, upgrading the durability properties, hydrothermal modification (HTM) of aspen alder and birch wood was investigated. The treatment was conducted in a multifunctional laboratory device WTT. In the previous cases it has been found that the treatment at 160oC improves the durability insufficiently. The modification at 180oC ensured a hi...
B Andersons, I Andersone, V Biziks, I Irbe, J Chirkova, E Sansonetti, J Grinins, H Militz


Influence addition of boron compounds to adhesives on the bonding quality and fungicidal properties of glued wood
2010 - IRG/WP 10-40497
Wood is one of the most important construction materials. However, users of wood face two issues: limited dimensions and insufficient durability. These issues have been overcome with the development of bonding and wood preservation. The preservation of glued wood is elucidated in this paper. Through the addition of boric acid to adhesives, we tried to improve the fungicidal properties of glued woo...
M Humar, B Lesar, A Ugovsek, M Kariz, P Kralj, M Šernek


TMT–Interlab–Test to establish suitable quality control techniques - Structure and first results
2010 - IRG/WP 10-40503
As a result of growing quality demands from manufacturers and end-consumers of thermally modified timber (TMT) recent scientific research activities are increasingly focussed on modification mechanisms and by this on the development of suitable quality control methods. To deepen the knowledge in modification mechanisms and to obtain a larger variety of scientific data for TMT depending on the trea...
C R Welzbacher


Preliminary Observations of the Photostabilization of Wood Surfaces with Cerium Oxide Nanoparticles
2010 - IRG/WP 10-40504
Reactive transition metal compounds, wood modification and grafting of UV absorbers have all been used to photostabilize wood. Some of these approaches are promising, but the toxicity of certain reactive transition metal compounds and the cost of wood modification and grafting have restricted their commercial applications. Hence, more cost-effective and environmentally friendly methods of protecti...
Chunling Liu, A Ahniyaz, P Evans


Effect of borax-boric acid Treatment of simul (Bombax ceiba) Veneers on Glue-Bond Quality of Plywood
2010 - IRG/WP 10-40525
The glue-bond quality of plywood made of treated simul (Bombax ceiba) veneers was investigated. The veneers were treated with cold and hot water solution of borax-boric acid (BB) of different concentrations and treatment durations. The plywoods were made at three different pressures in hot press using urea formaldehyde glue. The glue-bond strength of untreated plywood in dry shear-test was found t...
K Akhter, Md Abul Hashem, S Akhter


Effect of Nano-Silver Treatment on Densified Wood Properties. Part One: Swelling, Recovery Set, Bending Strength
2010 - IRG/WP 10-40533
In this research the effect of Nano-Silver treatment on compressed wood properties, was studied. Wood specimens were cut from Popolus alba (poplar) and impregnated with Nano-Silver and water. Then the saturated samples were compressed through radial direction in a hot press under pressure of 6 MPa, for 1 and 4 hours. The temperatures of press were 150°C and 175°C. Swelling (24h), recovery set ...
G Rassam, H Reza Taghiyari, B Jamnani, M Ali Khaje


Comparative Study of Heat Treatment of Beech Wood in Hot Water and Steam Medium
2010 - IRG/WP 10-40536
Heat treatment of wood is an effective method to improve the dimensional stability and durability against biodegradation. Heat treatments of beech wood in 2 different mediums (hot water and steam) in 180ºC were compared in physical, mechanical and anatomical properties. Mass loss in hydrothermally treated wood was higher than hygrothermally treated samples. Mechanical properties (MOR, MOE and CS)...
A Talaei, K Yaghoobi, A N Karimi


Natural durability of wood tested in different environments in Northern Europe
2011 - IRG/WP 11-10747
Moisture is often recognised as a key factor regarding the long time performance of wooden products, and one of the main challenges for timber products is to predict accurate service life in use class 3 (not covered above ground) and use class 4 (in soil or fresh water contact). A range of durability classification studies have been performed both in field and laboratory. But for several wood spec...
P O Flæte, G Alfredsen, F G Evans


Wood protection by nano silver against white rot
2011 - IRG/WP 11-30554
This research was done with the aim of investigation on the natural durability of poplar (populous deltoides) in natural situation and treated with nano silver against the white rot. Testing samples was treated with the method of modified soaking and nano silver in 3 treating level of 0,200 and 400ppm. In this study effect of coriolus versicolor fungus (identificated as white rot) on populous del...
V Tazakor Rezai, A Usefi, M Soltani