IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 3559 documents. Displaying 25 entries per page.


Wood Preservation in the Federal Republic of Germany
1981 - IRG/WP 3157
The report gives some statistics about the forest products industries in the Federal Republic and a general review of the wood preservation industry. The trend in the use of wooden railway sleepers is decreasing, as is the use of poles. The sale of other pre-treated timber, mainly fence posts, palisades and domestic fences, is however slightly increasing. Apart from the use of pressure treatments ...
R Cockcroft, H Willeitner


Effect of wood species on colonization by an unknown wood boring organisms in marine waters
1995 - IRG/WP 95-10108
The effect of wood species on the initial settlement by surface fouling organisms in marine environments was investigated by exposing heartwood panels of Douglas-fir ((Mirb.) Franco), western redcedar (Donn.), and Oregon white oak (Dougl. ex. Hooke) in an estuary located on the coast of Oregon. The oak and western redcedar panels were sparsely colonized over the first 39 days of exposure, while th...
K S Rao, P F Schnieder, J J Morrell


Evidence for actinomycete degradation of wood cell walls
1990 - IRG/WP 1444
Several unique patterns of degradation occurring in wood cell walls have been observed in wooden stakes inserted in unsterile soil in the laboratory. Some of the patterns have also been observed in coniferous wood taken from forest floors. All the observed attack types occur within wood cell walls, mainly within the S2 layer. Attack is characterised by channels of varying diameter or small fusifor...
T Nilsson, G F Daniel, S L Bardage


Colonization of treated and untreated ponderosa pine exposed in Hilo, Hawaii
1995 - IRG/WP 95-20068
The rate of decay in above ground exposures is largely controlled by rainfall and temperature, factors which can be used to construct a climate index of decay hazard in above ground exposures. Developers of new biocide formulations have utilized this knowledge by establishing test sites in sub-tropical regions such as the Gulf Coast of the United States. More recently, field sites have been locate...
C M Freitag, J J Morrell, K J Archer


Basilit CCFZ. Further studies on ecotoxicological behaviour
1992 - IRG/WP 92-3722
Basilit CCFZ is a new developed water based preservative for the protection of timber in hazard class 4 and 5 (ground-, fresh- and salt-water contact). The active components of this salt are copper, chromium, zinc and fluorine. In addition to primarily studies on the acute toxicity against organisms of the aquatic food chain a long term ecotoxicological study was performed. In a prolonged toxicity...
H W Wegen


The ecotoxicology assessment of wood preservatives and their active ingredients by means of germination tests using cress - A critical consideration
1999 - IRG/WP 99-50125
With putting the Biocidal Products Directive 98/08/EC (BPD) in place an environmental risk assessment for wood preservatives and impregnated timber is requested. To assess possible risks, suitable test methods are required, which reveal the ecotoxicological profile including environmental fate and behaviour of treated commodities. Germination and growth tests could contribute to the determination ...
P Jüngel, A O Rapp, E Melcher


Colonisation of painted wood by Aureobasidium pullulans - Analysis of features and consequences for failure in service
1996 - IRG/WP 96-10144
Wooden blocks of spruce were painted with different paint formulations. Water- and solvent-borne model and commercial paints were used. The painted wooden blocks were inoculated with a spore suspension of Aureobasidium pullulans (de Bary) Berkg. and placed in an environment of high humidity for 14 months. Different colonisation and growth patterns were observed on the different paint surfaces. The...
S L Bardage


Further studies on soft rot decay in CCA treated Eucalyptus power transmission poles in Queensland, Australia
1980 - IRG/WP 1115
Preliminary results on the examination of fungi isolated from CCA treated Eucalyptus power transmission poles were presented at the 10th Annual IRG Meeting. Since then further examination and identification of fungal isolates has been completed together with screening tests for wood decay ability and tolerance to creosote and CCA and its components. Chemical analyses for CCA retention have also be...
L E Leightley


Eradication of wood decay fungi by means of radio frequency
1998 - IRG/WP 98-10292
High frequency electromagnetic fields i.e. radio frequency (RF) are used in wood industry for heating, gluing and bending of wood and are also appropriate for eradicating of wood decay fungi and insects. We investigated the effects of RF exposure on wood samples which were in vitro infected by Coniophora puteana, Gloeophyllum trabeum and Lentinus lepideus. For each fungus, the lethal temperature a...
F Pohleven, J Resnik, A Kobe


Silicic acid-Boric acid complexes as wood preservatives
2001 - IRG/WP 01-30273
A silicic acid monomer aqueous solution (SAMS) or colloidal silicic acid solution (CSAS) was combined with various metal compounds or boric acid. Agents where SAMS or CSAS was combined with boric acid gave good protection against decay caused by the brown-rot fungus Fomitopsis palustris, the treated wood (Cryptomera japonica D. Don) specimens after the leaching test maintained a high resistance to...
H Yamaguchi


Report on the efficacy and performance of the insecticide candidate termiticide in H2 field trials
2004 - IRG/WP 04-10516
This paper explains the field results of phenol pyrazole treated timber against in an above ground mound colonies of Coptotermes acinaciformis (Froggatt). C. acinaciformis (‘termites’) are the major pest of human structures throughout tropical and sub tropical regions, causing billions of dollars in damage to timber-in-service worldwide. The result of this field test have shown that candidate ...
B M Ahmed, P Vinden, J Hann, J R J French


On the nature of the tertiary wall in wood cells. Summary of lecture given at 9th Annual Meeting, Noordwijk-aan-Zee, Holland
1977 - IRG/WP 169
During recent discussions on the possible causes of failure of treated hardwood species by soft rot fungi, the uneven micro distribution of toxic components was found to be of importance; this might be attributed to a restricted diffusion of the preservative from the cell lumina into the cell wall.·In this context, the nature of the tertiary wall as the inner lining of wood cells merits special a...
W Liese


Bending properties of wood after its decay with Coniophora puteana and subsequent modification with selected chemicals
1999 - IRG/WP 99-40146
Mechanical properties of wood are often decreased due to decay processes caused by biotic and/or abiotic factors. Damaged wooden elements (e.g. historical structures) can be reinforced by more methods, including their modification with convenient chemicals. This paper presents influences of selected chemicals on basic bending properties (modulus of elasticity - MOE, modulus of rupture - MOR) of so...
L Reinprecht, S Varinska


Analysis of volatile organic compounds (VOC's) from Trichoderma spp.: effect of media composition on VOC production and level of inhibition of wood decay fungi
1997 - IRG/WP 97-10207
Production of volatile organic compounds (VOC's) by two Trichoderma isolates grown on either malt extract or minimal media was examined and statistically assessed to identify which VOC's were predominantly produced on each of the two media types. The VOC's were captured onto chromatographic absorbent from above the cultures of the fungi before being analysed by integrate...
A Bruce, R E Wheatley, C Hackett, A Kundzewicz


Wood and filter paper degradation, phenol oxidase and one-electron oxidation activities by the white rot fungus Ceriporiopsis subvermispora
2003 - IRG/WP 03-10486
The activities of one-electron oxidation and phenol oxidase during incubation of cultures of the white-rot basidiomycete Ceriporiopsis subvermispora containing either glucose or wood were periodically measured. Further, the degradation activities against wood and filter paper were examined during the course of cultivation. Weight losses of Japanese beech wood and Japanese cedar wood after 12 wee...
H Tanaka, S Itakura, A Enoki


Stability, performance and distribution of propiconazole (R 49362) in acceleratedly aged wood
1991 - IRG/WP 3647
The permanency of propiconazole (R 49362 - WOCOSENÔ technical - Janssen Pharmaceutica) in wood was examined in an 18 month storage test, an evaporative ageing study (EN 73), a volatilization stress experiment, and water-leaching studies (EN 84). The biological efficacy against two brown rot fungi: Coniophora puteana BAM Ebw. 15 and Gloeophyllum trabeum BAM Ebw. 109 was assessed according to the E...
A R Valcke, M Stevens


Co-operative tests concerning influence of solvent and drying method on the toxic limit of wood preservatives against Basidiomycetes. Preliminary report
1971 - IRG/WP 204
In the Working Group II of the Organization for Economic Co-operation and Development working group on wood preservation (now International Research Group on wood preservation) it was agreed that more knowledge was necessary concerning the influence of the solvent on the toxic limit of organic solvent types of wood preservatives against Basidiomycetes. A test program was drawn up and after discuss...
T Hof


Accelerated weathering test for the evaluation of wood preservative efficacy
2003 - IRG/WP 03-20262
Wood samples treated with ammonium copper quat (ACQ-1900 and ACQ-2200), Chromated copper arsenate (CCA), Tanalith E 3491 and Wolmanit CX-8 have been studied in accelerated weathering experiments. The weathering experiment was performed by cycles of 2 hours UV-light irradiation followed by water spray for 18 minutes. The changes on the surface of the weathered samples were characterized by FTIR Sp...
A Temiz, M Eikenes, Ü C Yildiz, F G Evans, B Jacobsen


Environmentally benign wood preservatives based on organic biocide antioxidant combinations: A brief review of laboratory and field exposure results and discussion of a proposed mechanism
2004 - IRG/WP 04-30335
The combination of various organic biocides with commercial antioxidants generally increased the biocides’ efficacy 2-3 fold against wood-destroying fungi in short-term laboratory decay tests, and some positive results have been obtained after 2-4 years of outdoor exposure. The two antioxidants principally examined, propyl gallate and butylated hydroxytoluene, are low cost and, since both are f...
T Schultz, D D Nicholas, W Henry, C Pittman, D Wipf, B Goodell


Wood structure in relation to excessive absorption - a literature survey
1971 - IRG/WP 300
This literature study, composed in connection with 'the structure of wood in relation to the excessive absorption', started from the idea that the subject only could be dealt with successfully if the structure was taken into account in relation to a normal absorption pattern in so far as this knowledge can enlighten the understanding of the abnormal situation. The normal penetrat...
S M Jutte


Performance of copper-chrome formulations in ground contact in five test sites in New Zealand
1996 - IRG/WP 96-30113
Copper-chrome-arsenate (CCA), copper-chrome-boron (CCB), copper-chrome-fluoride (CCF) and copper-chrome-phosphate (CCP) have been tested at four retentions each in ground contact (25 x 50 x 500 mm³ radiata pine sapwood stakes) for 16 years in five test sites in New Zealand. Results to date show that test site characteristics have a marked effect on relative performance. In a warm and wet site (an...
M E Hedley, R N Wakeling, J Foster, B E Patterson


Quality and safety scheme for wood in food contact
1995 - IRG/WP 95-50040-11
When there is no tolerance concerning the content in food of potential contaminants the scheme is limited to a ban of any contaminant with objectives of undetectable amounts at the limits of detection of the chemical analysis. When some tolerances exist, there is a need to check the compliance of a production to such requirements, putting in place the necessary prevention of any accidental situati...
G Deroubaix


The potential application of rapid gas-chromatographic assay of microbial respiration to the monitoring of wood decay in field trial situations
1983 - IRG/WP 2196
Gas chromatographic detection of microbial activity (C02 production) within stakes in a field trial situation would appear to provide a sensitive, non-destructive and relatively rapid method for the quantitative assessment of preservative treatments. Most consistent results were obtained when stakes were removed from the soil, washed, saturated with water and incubated in sealed PVC tubes at 25°C...
M A Line


Wood Preservation in Belgium
1981 - IRG/WP 3170
The report reviews wood preservation activities in Belgium and notes the number of authorized treatment depots has doubled during the past five years. It lists the timbers that are allowed to be used for joinery and constructional building purposes and the preservatives and treatments with which these timbers may be protected. In Belgium not only have the wood preservative product and its treatmen...
M Stevens, R Cockcroft


Preservation of wood composites with zinc borate
1995 - IRG/WP 95-30074
Inorganic borates such as boric acid, borax, disodium octaborate tetrahydrate, and zinc borate can be incorporated into wood composites such as waferboard to impart decay and insect resistance to the final product. Zinc borate is especially well suited for this application due to its efficacy and leach resistance. The paper summarizes the work performed to date in this area. The effects on strengt...
P E Laks, M J Manning


Previous Page | Next Page