IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 3629 documents. Displaying 25 entries per page.


Effect of thickened boron in preventing conidial germination of sapwood-inhabiting fungi
1994 - IRG/WP 94-30059
We evaluated the efficacy of thickened boron preservative "Diffusolä" in preventing conidia germination of sapwood-inhabiting fungi using plate bioassay, Southern Yellow Pine and sweetgum block tests, and green pine log sections. The test fungi were sapstain fungi Ceratocystis coerulescens, Ceratocystis minor, and Aureobasidum pullulans and mold fungi, Aspergillus niger, Penicillium spp, and Tric...
S C Croan


Leaching of arsenic, copper and chrome from preservative-treated timber in playground equipment
1984 - IRG/WP 3149
Samples were taken from CCA-treated timber in sand play boxes and other play ground equipment. Sand was also sampled. Sand and wood samples were analysed for copper, chrome and arsenic by AAS. About 20-25% of the arsenic had leached from the timber after 2-4 year's exposure in the playgrounds. Very little of the copper and chrome had been leached. Sand collected in the close vicinity of t...
B Henningsson, B Carlsson


Evaluation of tropical wood by-products as a potential source for termite control products
2001 - IRG/WP 01-10408
Termites damaging in houses represent an ever growing threat in Europe, where the phenomenon has accelerated during the last ten years, as well as in the tropics, where infestations are permanent. To fight against this plague, the current methods used, through injection of organochloric or organophosphorized products into the timber structures and walls, are belonging to the past due to the toxici...
A Zaremski, S Robert, J-L Clement, D Fouquet


Soft-rot in Tabebuia sp. wood used in water cooling tower: identification and degradation capacity of the fungi
1998 - IRG/WP 98-10253
Tabebuia sp. (ipe), a native Brazilian wood, is considered of high natural resistance to decaying fungi, and has been used in harsh environments, as cooling towers. Fifty-one fungi, belonging to mitosporic fungi group (Fungi Imperfecti), were isolated from deteriorated Tabebuia sp. wood samples, collected from the mist eliminator and packing of a cooling tower in operation for about 23 years. The ...
S Brazolin, M Tomazello, I H Schoenlein-Crusius


Remedial wood preservative efficacy of BORA-CARE against the Formosan subterranean termite and eastern subterranean termite (Isoptera: Rhinotermitidae)
1991 - IRG/WP 1504
When a spruce board (3.8 cm x 8.8 cm x 2.4 m) was surface-sprayed with BORA-CARETM solution (containing 23% disodium octaborate tetrahydrate) and stored in an air-conditioned room (24 ± 2°C and 60 ± 5% RH) for eight months, ca. 40% of the wood (measured by the cross section surface proportion) contained borates at the rate of >2,500 ppm BAE (boric acid equivalent). In a choice bioassay, term...
N-Y Su, R H Scheffrahn


A report on the development of "Technical Recommendations Document for the Canadian wood preservation and protection facilities"
1987 - IRG/WP 3447
The wood preservation and wood protection industry uses chemicals which are similar. However, because the methods of applications of preservatives are different in wood preservation (pressure treatment) and wood protection (surface treatment) plants, their problems need to be resolved separately. As a part of a federal strategy to protect the environment and human health from potentially toxic com...
G Das, V N P Mathur


Screening of modified linseed oils on their applicability in wood protection
2004 - IRG/WP 04-30346
In this study modified linseed oils, rape oil and three waxes were screened on their efficacy as wood protecting agents. By testing all products when impregnated with high retentions in Scots Pine sapwood on water repellence qualities, additionally an accelerated weathering test, drying quality, accelerated brown rot and blue stain test, an indication is formed of the capability of these products ...
A Treu, J Lückers, H Militz


Design of a laboratory method for evaluating the effectiveness of soft rot preservatives
1988 - IRG/WP 2312
This purpose of this work was to design a method which makes it possible to evaluate the effectiveness of products which present protect wood against soft rot, using new products·of a different nature, on wood of·Pinus sylvestris L. and Fagus sylvatica L., and which, suitably applied, avoid big economic losses deriving from lack of knowledge of the active principles suitable to present protect w...
M T De Troya, A M Navarrete


Bibliographie sur les produits organiques en solvant pour la préservation du bois
1972 - IRG/WP 313
Le présent travail exécuté dans le cadre do la Section III du Groupe International de la Préservation du bois a pour but de rassembler, en vue d'éventuelles études plus approfondies sur le sujet ou sur l'un de ses aspects, les principales et relativement récentes références sur les produits de protection des bois en solvant, souvent appelés, et parfois improprement, pro...
H Alliot


The efficacy of polymer/preservative treatments in soil-bed exposure
1992 - IRG/WP 92-3729
Southern pine was treated with CCA, CCB, sodium borax/boric acid, or disodiumoctaborate, alone or in combination with an acrylic polymer system containing a water repellent. Treated samples were subjected to an unsterile soil burial test. The addition of polymer reduced the weight loss in borontreated samples at the lower retentions but not at the higher retention. Results with borates indicate th...
R J Murphy, H M Barnes, S M Gray


Preliminary evaluation of the answers to the 2nd IRG/WP-questionnaire on the state of pollution control in the field of wood preservation
1982 - IRG/WP 3209
This preliminary evaluation of the answers to the 2nd IRG/WP-Questionnaire only gives a general survey on those questionnaires which the author received until April 30th, 1982. Details, such as correlations between importance of wood preservation and pollution control, as well as a comparison of the answers with those to the first questionnaire (Doc. IRG/WP/369), could not be considered due to lac...
H Willeitner


Soft rot fungi found in copper/chrome/arsenic treated hardwood power transmission poles in Queensland
1978 - IRG/WP 185
In Queensland the effective service life of copper/chrome/arsenic (CCA) treated hardwood telegraph and power transmission poles is being dramatically shortened due to attack by soft rot decay fungi. The Australian Wood Preservation and Pole Industries are funding research into this serious soft rot problem involving C.S.I.R.O. and the University of Queensland. The C.S.I.R.O. is actively engaged wi...
L E Leightley


The evaluation of a survey of dry rot damages in Japan
1983 - IRG/WP 1179
The damage of wooden houses from Serpula lacrymans has increased in Japan, particularly in the northern area, Hokkaido Prefecture (See Figure 1). The weather conditions in Asahikawa have been recorded. The data obtained from the survey carried out over the five years from 1975 to 1980 were previously reported to the 5th International Biodeterioration Symposium which was held in Aberdeen, Scotland ...
S Doi


Assessing the bioresistance conferred to solid wood by chemical modification
1997 - IRG/WP 97-40099
The chemical modification of wood using straight chain alkyl anhydrides can considerably enhance its durability. This paper presents an assessment of the effectiveness of these modifiers in improving the biological resistance of a susceptible softwood when exposed to four different basidiomycete fungi, soft rots and the larvae of the house longhorn beetle (Hylotrupes bajulus). It was clear that so...
E D Suttie, C A S Hill, D Jones, R J Orsler


Soft rot decay in CCA treated eucalypts in Queensland - A comment
1986 - IRG/WP 1301
A survey has been completed concerned with the distribution and severity of groundline soft rot decay in the CCA treated sapwood of eucalypt poles in Queensland. The survey encountered some 1000 poles of which 55% were slightly, 28% moderately and 17% severely decayed. Soft rot decay was more severe in urban than rural locations. Embedment of poles in concrete resulted in severe soft rot. No signi...
L E Leightley


Environmental consequences of various materials in utility poles - A life cycle analysis
1992 - IRG/WP 92-3726
A model for environmental life cycle analysis, LCA, has been created to compare environmental impact from transmission poles, made alternatively of concrete, steel, aluminium and pine wood treated with CCA type B or creosote. The main pollution sources and energy use are included in the LCA. One pole size, 12 meters long, is presented in the study, a so called "45 kV" pole. Poles of different mate...
M Erlandsson, K Ödeen, M-L Edlund


Decay resistance of Siberian larch wood against brown rot fungus. - Part 3. The variation between plus trees and their grafted clones
2000 - IRG/WP 00-10350
The aim of the study was to estimate the variation in the decay resistance of Siberian larch (Larix sibirica Ledeb.) wood using mature plus trees and their grafted clones. Samples were collected with an increment core borer from 11 original plus trees and their 25-year-old grafted seed orchard clones. A typical brown rot fungus, Coniophora puteana (Schum. ex Fr.) Karst. (BAM Ebw. 15), was used as ...
H Viitanen, L Paajanen, M Venäläinen, A Harju, P Velling


Inhibitory effects of leachates from Scots pine wood on germination of some wood rotting fungi
1986 - IRG/WP 1282
Leachates from sapwood of Pinus sylvestris inhibited or reduced the germination of basidiospores of the wood decay fungi tested. The fungi were selected among those preferentially colonizing hardwood or softwood, representatives for brown rot and white rot fungi, early basidiomycete colonizers and late basidiomycete colonizers in above-ground parts of pine as well as fungi found in high frequencie...
J Bjurman


Weathering of copper-amine treated wood
2000 - IRG/WP 00-40155
Copper ethanolamine (Cu-EA) treated southern pine (SP) were artificially weathered with a QUV Weathering Tester. The weathering regime was composed of a continuous UV-light irradiation for 2 hours followed by a water spray for 18 minutes for a total time of 1200 hours. The changes on the surface of the weathered samples were characterized by Fourier transform infrared spectroscopy (FTIR) analysis,...
J Zhang, D P Kamdem


New principles for the protection of wood: Impregnation with waterborne resins
1995 - IRG/WP 95-40047
The environmental impact of classical wood preservatives as well as the use of tropical wood species with high natural durability is regarded increasingly critically in the public. Therefore other partially new principles for the protection of wood, like chemical modification, or treatment with resins were examined especially in USA, Japan and in Europe with promising results predominantly in the ...
A O Rapp, R-D Peek


The effect of a chelator mediated fenton system on activation of TMP fibres and decolorization of synthesized dyes
2004 - IRG/WP 04-50223
The purpose of this work is to improve our current knowledge of the non-enzymatic mechanisms involved in the brown rot degradation of wood, but also to study the potential applications of a chelator-mediated Fenton system in activation of wood fibers and decolorization of synthesized dyes. In this work, Electron Spin Resonance (ESR) spin-trapping techniques were used to study the generation of hyd...
Yuhui Qian, B Goodell, J Jellison


Natural durability of larch heartwood against decay
1997 - IRG/WP 97-10201
Larch heartwood has been promoted in Sweden and in other European countries as an alternative to preservative treated timber. It has even beeen stated that larch heartwood is more durable than preservative treated timber. This paper presents a compilation of facts from scientific reports on the durability of larch heartwood. Some recent data from this department are also reported. All data suggest...
T Nilsson


Mercury porosimetric evaluation of the impregnability of wood
1985 - IRG/WP 2234
Mercury porosimetric measurements for specimens of a given length can not be used to evaluate the treatability of wood. The reason is that the permeability for low permeable woods deviates from Darcy's law with the specimen length. This paper presents a method of evaluation which respects this phenomenon in indicating not only pore size but also a factor describing the pore size as a func...
J P Hösli


Possibility and problems of characterizing treated wood after service with regard to disposal
1993 - IRG/WP 93-50006
For the disposal of wood waste under ecological conditions, information about its hazardous potential and the logistic aspects for its handling is needed. The main criterion to evaluate the hazardous potential besides the determination of the type and quantity of active ingredients in the wood will be the degree of mixture with different treated or untreated timber. Assortments can be homogeneous ...
A Voss, H Willeitner


Solid state NMR study on pine wood degraded by brown rot fungus Gloeophyllum trabeum
1994 - IRG/WP 94-10067
Blocks of Pinus koraiensis wood were degraded by Gloeophyllum trabeum and examined by solid-state 13C NMR spectroscopy. Chemical compositions were estimated from relative signal aras. There was no evidence for preferential degradation of the noncrystalline cellulose which accounted for about 4% by weight of the wood. Loss of partly ordered cellulose on crystal surfaces exceeded the loss of crystal...
Yoon Soo Kim, R Newman


Previous Page | Next Page