IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 3629 documents. Displaying 25 entries per page.


Silicon tetrachloride: A potential wood preservative
1980 - IRG/WP 3133
In its present form, this paper is a preliminary draft of a paper that will eventually be submitted for publication in the Forest Products Journal. We are continuing the work on the effects of silicon tetrachloride on wood and expect to have additional data for the meeting in May 1980. Specifically we are measuring the penetration rate and depth of SiCl4, and we are chemically analyzing the treate...
C W Owens, W T Shortle, A L Shigo


Remediation of a site contaminated with creosote and CCA - a case study
1998 - IRG/WP 98-50101-12
Over sixty years of wood preservation activity conducted by ImpregNor at Ilseng, Norway, has caused serious contamination of the soil. High concentrations of creosote have been found at two separate sites, one in connection to the creosote wood preservation plant, and one further downstream were residues from the creosote preservation have been deposited. High levels of chromium, copper and arseni...
T Rødsand, K Hellum, H Lillemaehlum


Serial techniques for producing fire-retardant wood products
1997 - IRG/WP 97-30127
A series of techniques including fire-retarders denoted by WFR-1, WFR-2. WFR and their applications in producing fire-retardant wood (WFR wood), fire-retardant plywood (WFR plywood), fire-retardant particleboard (WFR particleboard) and fire-retardant MDF (WFR MDF) were investigated The fire retarders were low toxic, decay resistant and less leachable. The treated wood and WFR panels were of excell...
Zhu Jia Qi, Liu Yan Ji, Gao Chao Ying


Characteristics and quantity of impregnated wood waste in Germany
1995 - IRG/WP 95-50041
The disposal of wood waste in Germany is one of the main problems not only for the wood preservation industry but also for all concerned with wood waste. Data on characteristics and quantity of wood waste are still needed. Based on criterions given in a previous paper (IRG/WP 93-50006), several assortments have been characterized with regard to their hazardous potential and their logistical aspect...
A Voss, H Willeitner


Estimation of mycelial biomass by determination of the ergosterol content of wood decayed by Coniophora puteana and Fomes fomentarius
1989 - IRG/WP 1415
The mycelial biomass of fungi decomposing wood materials may be estimated by the use of an ergosterol assay technique.ln decay tests, essentially according to EN 113, estimates made by HPLC analyses on wood decayed by Coniophora puteana and Fomes fomentarius show the increase in biomass in the wood blocks. The ergosterol contents were correlated with dry weight loss determinations. Degradation of ...
K Nilsson, J Bjurman


Do CCA treated support stakes cause increased arsenic level in crops?
2003 - IRG/WP 03-50204
Trial of using CCA-C treated eucalypts stakes for supporting banana plants in Guangdong Province, China, began in 1998 and later it was expanded as a demonstration program of a joint International Tropical Timber Organization–Chinese Government timber preservation project in 2000. The greatest concern was whether the crop would be contaminated by the preservatives, arsenic in particular. Data fr...
Li Zhaobang, Su Haitao, Liang Linqing


Preservative treatment of rubber wood (Hevea brasiliensis) to increase its service life
2005 - IRG/WP 05-40320
Rubber wood (Hevea brasiliensis) possess excellent properties for interior designing, wood working and furniture making. But it is very much susceptible to sap stain and mould fungi which decreases the service life. For profitable uses , it is necessary to increase the service life of rubber wood. To protect the rubber wood from wood degrading agents, the sawn timber were treated with Borax – b...
K Akhter


Influence of surface coating on the leachability of boric acid and bifluorides from spruce wood
1995 - IRG/WP 95-50050
In the Netherlands, window joinery made from non-durable timber species (spruce) are widely protected with preservative rods. These rods contain non-fixing wood preservatives (e.g. bifluorides or boric acid). This reseach was performed to show the possible influence of a coating system to hinder the leaching of the active ingredients. The results of the leaching tests show, that bifluorides and ev...
W J Homan, H Militz


Targeted inhibition of wood decay fungi: degradation of cotton cellulose
1999 - IRG/WP 99-10321
Brown-rot decay is responsible for 80% of the damage and replacement of wood in service. For nearly thirty years, researchers have postulated a one-electron oxidase system combining Fe+2 oxalic acid, and H2O2 in the production of hydroxy radicals which ultimately oxidize cellulose in situ. Recently, researchers have been investigating antioxicants, in combination with biocides (Schultz, et al.,199...
F Green III, T A Kuster


Microemulsion formulations for wood protection chemicals
1993 - IRG/WP 93-30030
A microemulsion is a thermodynamically stable oil-water dispersion system. As a formulation it provides many unique features such as water compatibility for water-insoluble chemicals, formulation stability, good bioavailability and environmental acceptance. This paper discusses the major criteria for the formulations of water-insoluble wood biocides and the comparison in properties between convent...
Bing Yu, L E Leightley


Microwave modification of wood properties - Improvements in wood permeability
2000 - IRG/WP 00-40181
A new method of microwave (MW) wood modification is described. Microwave irradiation of timber provides an improvement in wood permeability mainly in the radial and longitudinal directions. This is achieved by physically modifying ray cells and forming a large number of cavities in the radial - longitudinal planes. More extensive MW irradiation of different species transforms the wood into a new m...
G Torgovnikov, P Vinden


Which substrate to use in a laboratory test with soft rot micro-fungi: vermiculite or unsterile soil?
1991 - IRG/WP 2372
A draft European Standard is being proposed by CEN TC 38 in which a vermiculite-burial and a soil-burial test to be carried out in succession are required. Various experiments with both procedures were set up with CCA, CC and propiconazole-formulations. The results show that vermiculite and unsterile soil yield comparable threshold values against soft rot. This poses the question of whether a two-...
A R Valcke


Site characteristics impacting historic waterlogged wood: A review
2000 - IRG/WP 00-10344
Survival of waterlogged wood from hundreds and in rare cases millions of years presents scientists with a unique opportunity to examine wood specimens which, due to select properties of the wood itself and/or the depostional environment, have not been completely degraded. Although degradation patterns of various types of microbial wood decay have been studied in detail, the site parameters of the ...
B A Jordan, E L Schmidt


Determination of the amine to copper ratio remaining in wood after leaching
2002 - IRG/WP 02-30285
The effectiveness of the protection and the environmental impact of the treated wood are two of the most important aspects that need to be understood for all preservatives. Both are particularly influenced by the loss of biocidal components from treated wood. For amine copper preservatives, copper fixation determines the leaching resistance of the copper and amine compounds formed in wood. Previou...
N Lucas, J N R Ruddick


Wood preservative potential of fractions of wood pyrolysis tar made from Japanese larch
1996 - IRG/WP 96-30102
Wood pyrolysis tar, which was discharged as a waste by-product in the production of charcoal from Japanese larch (Larix leptolepis), was separated into several fractions by solvent extraction using tetrahydrofuran, benzene and aqueous alkali. The fractions obtained were physico-chemically characterized and examined for wood preservative potential. This separation method compared favorably with fra...
T Suzuki, S Doi, M Yamakawa, K Yamamoto, T Watanabe, M Funaki


The treatability of five Indonesian wood species with BFCA preservative
1987 - IRG/WP 3428
This paper deals with a preliminary study on the treatability of five Indonesian wood species, i.e. Altingia excelsa (AE), Rhodoleria teysmanii (CA), Litsea odorivera (LO), Schima wallichii (SW) and Cratoxylon arborescens (CA). Wood samples measuring 4 x 4 x 100 cm³ were dipped into BFCA preservative solution for about 30 seconds. Preservative penetration and the surface area of treated zone were...
Nana Supriana, T K Waluyo


Utilization of coconut timber from north Sulawesi, Indonesia. Part 2: Treatability
1994 - IRG/WP 94-40025
Under tropical conditions coconut wood is quickly degraded by mold and blue stain fungi. Low density wood in ground contact is commonly decomposed by wood destroying fungi within a period of only a few months, higher density wood from the outer stem regions within 24 to 30 months (MOSTEIRO, CASIN, SERIBAN 1976; McQUIRE 1975). Moreover, according to McQUIRE (1975) green wood of lower density is hig...
R-D Peek


The economics of saving standing wood poles. Labour saving system for pole groundline retreatment
1980 - IRG/WP 3160
This paper consists of 3 contributions First: There are still people who consider wood poles a disposable commodity much the same as paper cups and toilet paper. The idea of conservation is still new in this field, but soon conservation will be a necessity. Only two percent of the forest recources of North America are being replaced. What does it mean? We will run out of poles a lot sooner than ...
W V Inkis


Decay and termite resistance of wood treated with boron-containing quaternary ammonia compound, didecyl dimethyl ammonium tetrafluoroborate (DBF) incorporated with acryl-silicon type resin
2004 - IRG/WP 04-30334
This study evaluates the decay and termite resistance of surface-treated wood with didecyl dimethyl ammonium tetrafluoroborate (DBF) incorporated with acryl-silicon type resin emulsion. DBF is a quaternary ammonia compound and contains boric tetrafluoride (BF4-) as a counter ion in its chemical structure. In the study, DBF was incorporated with an acryl-silicon type resin to increase water-resista...
S N Kartal, W J Hwang, K Shinoda, Y Imamura


IPBC - A new fungicide for wood protection
1984 - IRG/WP 3295
3-iodo-2-propynyl butyl carbamate (IPBC) is presented as a potential low toxic alternative to pentachlorophenol and the sodium chlorophenoxides. Data on its effect against basidiomycetes is shown. Tests according to both the European standard method, EN-113, and American, ASTM D-413, have shown its potential. The chemical gives protection against both the wood destroying fungi, blue stain, mould and algae. It is possible to have it formulated in both water-based and organic solvent-based products. Treatment of wood out of ground contact (vac-vac products, pretreatment products, primers, stains, etc.) and sapstain control are some of the most potential end use areas within wood protection. Besides wood protection, the IPBC is used as a fungicide in paint, adhesives, caulks and sealants, cement, leather, paper, cutting oil, ink and in different roofing materials.
J Hansen


Electricity pole treatments - Wedding Bells State Forest. Inspection September 1983
1985 - IRG/WP 3334
A survey to study the extent of soft rot in hardwood poles in N.S.W. was commenced in 1975. The results of the survey, published in 1982, indicated that a number of factors contributed towards soft rot attack on poles in service. A detailed rest on pole treatments and maintenance procedures was established in 1976, at a site in Wedding Bells State Forest near Coffs Harbour. The site selected was k...
R S Johnstone, R H Eldridge


Trust in the durability of preserved wood during and after the reclamation of the Zuiderzee
1987 - IRG/WP 4134
A firm belief in the durability of preserved wood must have existed during the reclamation of the Zuiderzee, because thousands of m³ have been utilized. The wood is exposed to attacks of marine borers and other organisms in the marine environment. Was this trust right or wrong? A recent examination was made of creosote impregnated pine posts after 65 years service in a dam, near the Barrier Dam a...
H Visscher


Potential for using dip/supercritical fluid treatments for wood impregnation
2004 - IRG/WP 04-40276
While supercritical fluid impregnation offers tremendous potential for impregnating wood species that resist conventional liquid preservative treatments, the resulting treatments are often not uniform among samples in a charge or between charges. One factor that influences treatment is the dynamic change in pressure that occurs during introduction of the biocide laden supercritical fluid into the ...
Sung-Mo Kang, J J Morrell


Deterioration of wood viewed from iron nail
1991 - IRG/WP 2368
Deterioration of nail was graded by a five - rank numerical - rating. The rating of nail moisture content and decay of wood were inspected in a mortal-wall of 34-year-old house. The wood was mostly in decay, when the rating of the nail was above about 4, and the moisture content was above about 20%. Nailed wood specimens kept in several humidity room of 20°C for 4 years showed that the rating of ...
H Imamura


Dimensional stability and decay resistance of wood upon modification with some new type chemical reactants
1994 - IRG/WP 94-40028
Solid wood of home grown species can be upgraded by chemical modification with environmentally acceptable chemicals. The best kwown example of modification reaction is acetylation with acetic anhydride. A continued search for reactive chemicals other than acetic anhydride is ongoing, aiming at the improvement of technical properties of wood. This contribution deals with the results of a screening ...
P Goethals, M Stevens